Technical Specifications
Product Overview
Metallurgical Characteristics
XAR300 features a fine-grained martensitic microstructure achieved through controlled quenching and tempering processes. The optimized chemical composition with controlled carbon content and strategic alloying elements ensures excellent hardenability while maintaining good weldability and machinability characteristics.
Heat Treatment Process
MetalZenith employs a sophisticated heat treatment cycle involving austenitization at 900-950°C, followed by controlled water quenching to achieve uniform martensitic transformation. Subsequent tempering at 200-250°C optimizes the hardness-toughness balance, resulting in consistent 300 HBW hardness throughout the material thickness.
Manufacturing Process
Our advanced production facility utilizes electric arc furnace steelmaking with secondary refining processes including ladle furnace treatment and vacuum degassing. Continuous casting followed by controlled rolling ensures optimal grain structure and mechanical properties. Final heat treatment in computer-controlled furnaces guarantees consistent quality and performance.
Quality Standards & Testing
All XAR300 products comply with international standards including EN 10204-3.1 certification. Comprehensive testing includes chemical analysis by optical emission spectroscopy, mechanical property verification through tensile and impact testing, hardness mapping across the plate surface, and ultrasonic inspection for internal soundness verification.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | ≤ 0.25 |
| Silicon (Si) | ≤ 0.70 |
| Manganese (Mn) | ≤ 1.60 |
| Phosphorus (P) | ≤ 0.025 |
| Sulfur (S) | ≤ 0.010 |
| Chromium (Cr) | 0.30 - 1.50 |
| Nickel (Ni) | ≤ 1.50 |
| Molybdenum (Mo) | ≤ 0.60 |
| Boron (B) | ≤ 0.005 |
| Aluminum (Al) | ≥ 0.015 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Brinell Hardness (HBW) | 280 - 320 |
| Tensile Strength (Rm) | 900 - 1180 MPa |
| Yield Strength (Rp0.2) | ≥ 700 MPa |
| Elongation (A5) | ≥ 10% |
| Impact Energy (KV) at -20°C | ≥ 27 J |
| Impact Energy (KV) at -40°C | ≥ 20 J |
| Fatigue Limit (10^7 cycles) | 450 MPa |
| Young's Modulus | 210 GPa |
| Poisson's Ratio | 0.30 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1450 - 1520°C |
| Thermal Conductivity (20°C) | 42 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 12.5×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.20 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
| Thermal Diffusivity | 11.6 mm²/s |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Cut-to-size pieces |
| Thickness Range | 6 - 80 mm |
| Width Range | 1000 - 3200 mm |
| Length Range | 2000 - 12000 mm |
| Standards | EN 10204-3.1, ASTM A514, JIS G3128 |
| Surface Finish | Hot rolled, Shot blasted, Pickled |
| Thickness Tolerance | ± 0.3 mm (6-20mm), ± 0.5 mm (>20mm) |
| Width Tolerance | ± 5 mm |
| Length Tolerance | ± 10 mm |
| Flatness | ≤ 5 mm/m |
| Edge Condition | Mill edge, Sheared edge, Flame cut |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing XAR300
Advanced Heat Treatment Technology
MetalZenith employs precision-controlled quenching and tempering processes with automated temperature monitoring systems, ensuring consistent 300 HBW hardness and optimal microstructure throughout the material thickness for superior wear resistance performance.
Comprehensive Quality Control Systems
Our state-of-the-art testing laboratory features advanced spectrometers, universal testing machines, and ultrasonic inspection equipment. Every XAR300 plate undergoes complete chemical analysis, mechanical testing, and non-destructive evaluation to guarantee specification compliance.
Custom Processing & Global Supply
MetalZenith offers complete customization services including precision cutting, machining, and surface treatment. Our global distribution network and strategic inventory locations ensure rapid delivery of XAR300 products worldwide with full traceability documentation.