20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
DILLIDUR 400V features a fine-grained martensitic microstructure achieved through controlled quenching and tempering processes. The optimized chemical composition with controlled carbon content and strategic alloying elements ensures excellent hardenability while maintaining good weldability and formability. The microstructure provides superior wear resistance through high surface hardness combined with a tough core.
Heat Treatment Process
MetalZenith employs advanced heat treatment technology including controlled austenitizing at 900-950°C, followed by accelerated cooling to achieve the desired martensitic transformation. Subsequent tempering at 150-250°C optimizes the balance between hardness and toughness. Our computer-controlled furnaces ensure uniform temperature distribution and consistent mechanical properties throughout the plate thickness.
Manufacturing Process
The production process begins with electric arc furnace melting followed by ladle refining and continuous casting. Hot rolling is performed using advanced rolling mills with precise temperature control. The quenching and tempering line features rapid cooling systems and automated tempering furnaces to achieve optimal microstructure and mechanical properties. Final inspection includes ultrasonic testing and surface quality verification.
Quality Standards & Certifications
DILLIDUR 400V is manufactured in accordance with international standards including EN 10204-3.1, ASTM A514, and JIS G3128. MetalZenith maintains ISO 9001:2015, ISO 14001:2015, and OHSAS 18001 certifications. Each plate undergoes comprehensive testing including chemical analysis, mechanical property verification, dimensional inspection, and non-destructive testing to ensure compliance with specified requirements and customer expectations.
🧪 Chemical Composition
| Element | Content (%) |
|---|---|
| Carbon (C) | ≤ 0.32 |
| Manganese (Mn) | 1.00 - 1.60 |
| Silicon (Si) | 0.10 - 0.70 |
| Phosphorus (P) | ≤ 0.025 |
| Sulfur (S) | ≤ 0.010 |
| Chromium (Cr) | 0.25 - 1.50 |
| Nickel (Ni) | ≤ 1.50 |
| Molybdenum (Mo) | ≤ 0.60 |
| Boron (B) | 0.0005 - 0.0060 |
| Titanium (Ti) | ≤ 0.15 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Hardness (HBW) | 370 - 430 |
| Tensile Strength (Rm) | 1200 - 1550 MPa |
| Yield Strength (Rp0.2) | ≥ 1000 MPa |
| Elongation (A5) | ≥ 10% |
| Impact Energy (KV) at -40°C | ≥ 30 J |
| Impact Energy (KV) at -20°C | ≥ 45 J |
| Young's Modulus | 210 GPa |
| Fatigue Limit | 450 MPa |
| Poisson's Ratio | 0.27 - 0.30 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1450 - 1520°C |
| Thermal Conductivity (20°C) | 42 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 12.5×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.20 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Cut-to-size pieces |
| Thickness Range | 4 - 80 mm |
| Width Range | 1000 - 3200 mm |
| Length Range | 2000 - 12000 mm |
| Standards | EN 10204-3.1, ASTM A514, JIS G3128 |
| Surface Finish | Hot rolled, Pickled, Shot blasted |
| Thickness Tolerance | ± 0.3 mm (t ≤ 20mm), ± 0.5 mm (t > 20mm) |
| Width Tolerance | ± 5 mm |
| Length Tolerance | ± 10 mm |
| Flatness | ≤ 5 mm/m |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing DILLIDUR 400V
Advanced Quenching & Tempering Technology
MetalZenith employs cutting-edge controlled cooling systems and precision heat treatment processes to achieve uniform hardness distribution and optimal microstructure throughout the entire plate thickness, ensuring consistent performance and extended service life.
Comprehensive Quality Control System
Our integrated quality management includes real-time chemical composition monitoring, mechanical property verification, ultrasonic testing, and dimensional inspection. Every plate is certified with complete material traceability and test certificates.
Custom Processing & Global Supply
MetalZenith offers complete customization including plasma cutting, machining, forming, and welding services. Our global distribution network ensures reliable supply with technical support and engineering consultation for optimal material selection.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications