Product Overview
Metallurgical Characteristics
UNS N06059 is a precipitation-hardening nickel-based super alloy with exceptional corrosion resistance derived from its high chromium and molybdenum content. The alloy's microstructure consists of a face-centered cubic austenitic matrix strengthened by gamma-prime (Ni3Al) precipitates formed during age hardening. This unique metallurgical structure provides outstanding resistance to localized corrosion, including pitting and crevice corrosion in chloride environments.
Heat Treatment Process
MetalZenith's optimized heat treatment process begins with solution annealing at 1175°C (2150°F) followed by rapid cooling to dissolve precipitates and achieve a homogeneous microstructure. Age hardening is performed at 718°C (1325°F) for 8 hours, followed by furnace cooling to 621°C (1150°F) and holding for 8 hours before air cooling. This dual-aging process maximizes strength while maintaining excellent corrosion resistance.
Manufacturing Process Excellence
Our manufacturing process utilizes vacuum induction melting (VIM) followed by vacuum arc remelting (VAR) to ensure chemical homogeneity and minimize segregation. Hot working operations are performed between 1200-900°C with careful temperature control to optimize grain structure. Cold working capabilities include precision rolling, drawing, and forming operations with intermediate annealing cycles as required.
Quality Standards & Testing
All UNS N06059 products manufactured by MetalZenith comply with ASTM B575, B619, B622, and B626 specifications. Comprehensive testing includes chemical analysis by optical emission spectroscopy, mechanical property verification, intergranular corrosion testing per ASTM G28, and critical pitting temperature evaluation. Non-destructive testing includes ultrasonic inspection, eddy current testing, and liquid penetrant inspection as specified.
🧪 Chemical Composition
| Element | Weight % |
|---|---|
| Nickel (Ni) | 58.0 - 63.0 |
| Chromium (Cr) | 22.0 - 24.0 |
| Molybdenum (Mo) | 15.0 - 16.5 |
| Aluminum (Al) | 1.10 - 1.50 |
| Titanium (Ti) | 0.05 - 0.25 |
| Iron (Fe) | ≤ 1.50 |
| Carbon (C) | ≤ 0.010 |
| Manganese (Mn) | ≤ 0.50 |
| Silicon (Si) | ≤ 0.50 |
| Phosphorus (P) | ≤ 0.015 |
| Sulfur (S) | ≤ 0.010 |
| Copper (Cu) | ≤ 0.50 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Ultimate) | ≥ 1035 MPa (150 ksi) |
| Yield Strength (0.2% Offset) | ≥ 725 MPa (105 ksi) |
| Elongation in 50mm | ≥ 30% |
| Reduction of Area | ≥ 50% |
| Hardness (Brinell) | 302 - 363 HB |
| Hardness (Rockwell C) | 32 - 38 HRC |
| Impact Energy (Charpy V-notch) | ≥ 95 J (70 ft-lb) |
| Fatigue Strength (10^7 cycles) | 450 MPa |
| Modulus of Elasticity | 207 GPa (30 × 10³ ksi) |
| Shear Modulus | 79 GPa (11.5 × 10³ ksi) |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 8.36 g/cm³ (0.302 lb/in³) |
| Melting Point | 1350-1400°C (2460-2550°F) |
| Thermal Conductivity (100°C) | 10.4 W/m·K (6.0 BTU/hr·ft·°F) |
| Thermal Conductivity (500°C) | 17.3 W/m·K (10.0 BTU/hr·ft·°F) |
| Thermal Expansion (20-100°C) | 12.8×10-6/K (7.1×10-6/°F) |
| Thermal Expansion (20-500°C) | 14.2×10-6/K (7.9×10-6/°F) |
| Specific Heat Capacity | 435 J/kg·K (0.104 BTU/lb·°F) |
| Electrical Resistivity | 1.24 µΩ·m |
| Magnetic Permeability | 1.001 (Non-magnetic) |
| Curie Temperature | Not applicable |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Round Bar, Flat Bar, Plate, Sheet, Strip, Wire, Tube, Pipe, Forging Stock |
| Round Bar Diameter | 6mm - 300mm (0.25" - 12") |
| Plate Thickness | 3mm - 100mm (0.125" - 4") |
| Sheet Thickness | 0.5mm - 6mm (0.020" - 0.25") |
| Tube Outer Diameter | 6mm - 200mm (0.25" - 8") |
| Standards Compliance | ASTM B575, ASTM B619, ASTM B622, ASTM B626, UNS N06059 |
| Surface Finish | Hot Rolled, Cold Rolled, Pickled, Polished, Machined |
| Dimensional Tolerance | ASTM Standard, Custom Precision Available |
| Length Options | Standard: 3m, 6m, 12m | Custom lengths available |
| Heat Treatment Condition | Solution Annealed, Aged, Custom Heat Treatment |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing UNS N06059
Advanced Vacuum Melting Technology
MetalZenith utilizes cutting-edge vacuum induction melting (VIM) and vacuum arc remelting (VAR) processes to produce UNS N06059 with exceptional chemical homogeneity and minimal inclusion content, ensuring superior mechanical properties and corrosion resistance performance.
Comprehensive Quality Control Systems
Our state-of-the-art testing laboratory features advanced spectroscopic analysis, mechanical testing equipment, and corrosion testing facilities. Every batch undergoes rigorous inspection including chemical verification, tensile testing, hardness measurement, and specialized corrosion resistance evaluation.
Custom Processing & Global Supply
MetalZenith offers complete customization capabilities including precision machining, specialized heat treatments, and custom dimensions. Our global distribution network ensures reliable delivery worldwide with comprehensive technical support and engineering consultation services.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications