JIS SUS440C is a high-carbon martensitic stainless steel renowned for its exceptional hardness, wear resistance, and corrosion resistance. This premium bearing steel, equivalent to AISI 440C, combines superior mechanical properties with excellent dimensional stability, making it the preferred choice for precision applications requiring long-term reliability.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art vacuum induction melting and electroslag remelting technologies to produce ultra-clean JIS SUS440C steel with exceptional purity and homogeneity. Our advanced processing capabilities include precision heat treatment in controlled atmospheres, ensuring optimal microstructure and consistent mechanical properties throughout each batch.

Key Applications & Industries

  • High-precision ball and roller bearings for aerospace and automotive applications
  • Surgical instruments and medical devices requiring biocompatibility
  • Cutting tools, knives, and wear-resistant components
  • Valve components and pump parts in corrosive environments

Quality Assurance & Certification

MetalZenith maintains ISO 9001:2015 and AS9100D certifications, ensuring every batch of JIS SUS440C meets stringent international standards. Our comprehensive testing protocols include chemical analysis, mechanical testing, microstructural examination, and non-destructive testing to guarantee consistent quality and traceability.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

JIS SUS440C is a high-carbon martensitic stainless steel with a complex microstructure consisting of tempered martensite matrix with dispersed chromium carbides. The high carbon content (0.95-1.20%) enables exceptional hardness after heat treatment, while the chromium content (16-18%) provides adequate corrosion resistance. The steel exhibits excellent hardenability and can achieve uniform hardness throughout substantial cross-sections.

Heat Treatment Process

MetalZenith's optimized heat treatment process begins with annealing at 850-900°C followed by slow cooling to achieve maximum machinability. Hardening involves austenitizing at 1010-1065°C in controlled atmosphere, followed by oil or air quenching. Tempering is performed at 150-200°C for maximum hardness or 200-300°C for improved toughness, depending on application requirements.

Manufacturing Process Excellence

Our manufacturing process employs electric arc furnace melting followed by ladle refining and vacuum degassing to minimize harmful elements. Secondary refining through electroslag remelting ensures exceptional cleanliness and homogeneity. Hot working is performed within the temperature range of 1150-850°C, followed by controlled cooling to optimize microstructure.

Quality Standards & Testing

Every batch undergoes comprehensive testing including optical emission spectroscopy for chemical analysis, tensile and hardness testing, microstructural examination, and ultrasonic testing for internal soundness. MetalZenith maintains full traceability from raw materials through final inspection, ensuring compliance with international aerospace and medical device standards including AS9100D and ISO 13485.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.20
Silicon (Si)≤ 1.00
Manganese (Mn)≤ 1.00
Phosphorus (P)≤ 0.040
Sulfur (S)≤ 0.030
Chromium (Cr)16.00 - 18.00
Molybdenum (Mo)≤ 0.75
Nickel (Ni)≤ 0.60
Copper (Cu)≤ 0.50
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Hardened & Tempered)≥ 1900 MPa
Yield Strength (0.2% Offset)≥ 1650 MPa
Elongation (50mm gauge length)≥ 2%
Reduction of Area≥ 15%
Hardness (Hardened & Tempered)58-62 HRC
Hardness (Annealed)≤ 269 HB
Impact Energy (Charpy V-notch, 20°C)15-25 J
Fatigue Limit (107 cycles)800-900 MPa
Young's Modulus200 GPa
Poisson's Ratio0.27-0.30

🔬 Physical Properties

PropertyValue
Density7.70 g/cm³
Melting Point1480-1530°C
Thermal Conductivity (20°C)24.2 W/m·K
Thermal Expansion Coefficient (20-100°C)10.4×10-6/K
Thermal Expansion Coefficient (20-300°C)11.2×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.60 µΩ·m
Magnetic Permeability (Hardened)Ferromagnetic
Curie TemperatureApproximately 450°C
Thermal Diffusivity6.8×10-6 m²/s

📏 Product Specifications

SpecificationAvailable Options
Product FormsRound bars, square bars, flat bars, plates, sheets, strips, tubes, forgings
Round Bar Diameter6mm - 300mm
Plate Thickness3mm - 100mm
Sheet Thickness0.5mm - 6mm
Strip Thickness0.1mm - 3mm
Tube Outer Diameter10mm - 200mm
LengthUp to 6000mm (custom lengths available)
Surface FinishHot rolled, cold drawn, ground, polished, pickled
Heat Treatment ConditionAnnealed, hardened & tempered, solution treated
Dimensional Tolerance±0.1mm to ±0.5mm (depending on form and size)
Standards ComplianceJIS G4303, ASTM A276, EN 10088-3, GB/T 1220

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing JIS SUS440C

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith employs cutting-edge vacuum induction melting (VIM) and electroslag remelting (ESR) processes to achieve ultra-low inclusion content and superior cleanliness in JIS SUS440C production. This advanced technology ensures exceptional fatigue life and reliability in critical bearing applications.

Precision Heat Treatment Control

Our state-of-the-art heat treatment facilities feature computer-controlled furnaces with precise atmosphere control, enabling optimal austenitizing, quenching, and tempering cycles. This ensures consistent hardness distribution and dimensional stability throughout the entire cross-section of JIS SUS440C components.

Manufacturing Advantage 2
Manufacturing Advantage 3

Comprehensive Customization Capabilities

MetalZenith offers extensive customization options for JIS SUS440C, including specialized chemical compositions, custom heat treatment specifications, and precision machining services. Our global supply chain and flexible production capabilities ensure timely delivery of tailored solutions to meet specific application requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo