Skip to product information
1 of 1

JIS SUJ2

JIS SUJ2

Premium JIS SUJ2 Bearing Steel from MetalZenith

MetalZenith proudly manufactures JIS SUJ2, a high-carbon chromium bearing steel equivalent to AISI 52100 and EN 100Cr6. This premium bearing steel is engineered for exceptional hardness, wear resistance, and fatigue strength, making it the ideal choice for high-performance bearing applications across diverse industries.

Advanced Manufacturing Excellence

Our state-of-the-art production facilities utilize advanced electric arc furnace technology combined with vacuum degassing and ladle refining processes to ensure superior steel cleanliness and homogeneity. MetalZenith's precision-controlled manufacturing environment guarantees consistent chemical composition and mechanical properties in every batch of JIS SUJ2 steel.

Key Applications

  • Ball and roller bearings for automotive applications
  • Industrial machinery bearings and precision components
  • Aerospace bearing systems requiring high reliability
  • Railway and transportation bearing assemblies
  • High-speed spindle bearings for machine tools

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control protocols including ultrasonic testing, magnetic particle inspection, and complete chemical analysis. Our advanced metallurgical laboratory ensures every shipment meets or exceeds JIS G 4805 specifications and customer requirements.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

JIS SUJ2 is a high-carbon, low-alloy steel specifically designed for bearing applications. The steel's microstructure consists of fine pearlite in the annealed condition, which transforms to martensite with retained austenite upon hardening. The chromium content provides enhanced hardenability and wear resistance, while maintaining excellent dimensional stability during heat treatment.

Heat Treatment Process

MetalZenith's controlled heat treatment process involves austenitizing at 820-860°C, followed by oil quenching to achieve full hardness. Tempering is performed at 150-200°C to achieve the desired hardness range of 60-65 HRC. Our advanced furnace technology ensures uniform heating and precise temperature control throughout the process, resulting in consistent mechanical properties and minimal distortion.

Manufacturing Process Excellence

Our production process begins with electric arc furnace melting, followed by ladle refining and vacuum degassing to achieve ultra-low inclusion content. The steel is cast into ingots or continuously cast billets, then hot rolled to the required dimensions. Cold drawing and precision grinding operations are available to achieve tight dimensional tolerances and superior surface finish.

Quality Standards & Testing

MetalZenith maintains strict adherence to JIS G 4805 standards and implements comprehensive quality control protocols. Every batch undergoes complete chemical analysis, mechanical testing, ultrasonic inspection, and magnetic particle testing. Our ISO 9001:2015 certified quality management system ensures consistent product quality and full traceability from raw materials to finished products. Additional testing services include fatigue testing, cleanliness evaluation, and microstructural analysis to meet specific customer requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.10
Silicon (Si)0.15 - 0.35
Manganese (Mn)≤ 0.50
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025
Chromium (Cr)1.30 - 1.60
Nickel (Ni)≤ 0.25
Copper (Cu)≤ 0.25
Aluminum (Al)≤ 0.050
Oxygen (O)≤ 0.0015

⚙️ Mechanical Properties

PropertyValueCondition
Tensile Strength2100 - 2400 MPaHardened & Tempered
Yield Strength1800 - 2100 MPaHardened & Tempered
Elongation8 - 12%Hardened & Tempered
Hardness (HRC)60 - 65Hardened & Tempered
Hardness (HB)≤ 269Annealed
Impact Energy (Charpy V)15 - 25 JRoom Temperature
Fatigue Limit900 - 1100 MPa107 cycles
Young's Modulus210 GPaRoom Temperature
Poisson's Ratio0.27 - 0.30Room Temperature

🔬 Physical Properties

PropertyValueTemperature
Density7.81 g/cm³20°C
Melting Point1480 - 1520°C-
Thermal Conductivity42.6 W/m·K20°C
Thermal Expansion Coefficient12.3×10-6/K20-100°C
Specific Heat Capacity460 J/kg·K20°C
Electrical Resistivity0.25 µΩ·m20°C
Magnetic PermeabilityFerromagneticRoom Temperature
Curie Temperature740°C-
Thermal Diffusivity11.8 mm²/s20°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsRound Bars, Square Bars, Flat Bars, Wire Rod, Forged RingsJIS G 4805
Round Bar Diameter6mm - 300mmJIS G 4805
Square Bar Size10mm - 150mmJIS G 4805
Flat Bar Thickness5mm - 100mmJIS G 4805
Wire Rod Diameter5.5mm - 42mmJIS G 3507
Length3000mm - 12000mm (Custom lengths available)Customer Specification
Surface FinishHot Rolled, Cold Drawn, Peeled, GroundJIS G 4805
Dimensional Toleranceh9, h10, h11 (ISO 286)ISO 286-2
Heat Treatment ConditionAnnealed, Normalized, SpheroidizedJIS G 4805
Equivalent StandardsAISI 52100, EN 100Cr6, DIN 1.3505International

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing JIS SUJ2

Manufacturing Advantage 1

Advanced Vacuum Degassing Technology

MetalZenith employs cutting-edge vacuum degassing and ladle refining processes to achieve ultra-low inclusion content and superior steel cleanliness. Our controlled atmosphere melting ensures exceptional bearing fatigue life and reliability in critical applications.

Comprehensive Quality Control System

Our ISO 9001:2015 certified facility features advanced testing capabilities including ultrasonic inspection, magnetic particle testing, and complete chemical analysis. Every batch undergoes rigorous mechanical testing to guarantee consistent performance and compliance with JIS G 4805 standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain & Custom Solutions

MetalZenith offers flexible supply solutions with global distribution capabilities and custom processing services. We provide tailored heat treatment, precision machining, and specialized surface treatments to meet specific customer requirements and delivery schedules.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo