JIS SM490

JIS SM490 High-Strength Structural Steel

JIS SM490 is a high-strength structural steel grade specified under Japanese Industrial Standard (JIS G 3106) for welded structures. This carbon-manganese steel offers excellent weldability, formability, and superior mechanical properties, making it ideal for heavy construction and engineering applications requiring enhanced strength-to-weight ratios.

MetalZenith's Advanced Manufacturing Excellence

As a leading steel manufacturer, MetalZenith employs state-of-the-art controlled rolling and thermomechanical processing techniques to produce JIS SM490 steel with exceptional consistency and performance. Our advanced electric arc furnaces and continuous casting systems ensure precise chemical composition control, while our modern rolling mills deliver superior surface quality and dimensional accuracy.

Key Applications & Industries

  • Heavy construction and infrastructure projects
  • Bridge construction and structural frameworks
  • Offshore platforms and marine structures
  • Industrial equipment and machinery frames
  • Pressure vessels and storage tanks
  • Mining and earthmoving equipment

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and adheres to strict JIS G 3106 standards. Our comprehensive quality control includes chemical analysis, mechanical testing, ultrasonic inspection, and dimensional verification. Each batch undergoes rigorous testing to ensure compliance with specified requirements and customer expectations.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

JIS SM490 is a low-alloy, high-strength structural steel with a predominantly ferritic-pearlitic microstructure. The controlled carbon content (≤ 0.18%) ensures excellent weldability while maintaining adequate strength levels. The addition of manganese enhances hardenability and strength, while silicon acts as a deoxidizer and contributes to solid solution strengthening.

Manufacturing Process

MetalZenith produces JIS SM490 through advanced steelmaking processes including electric arc furnace melting, ladle refining, and continuous casting. The steel undergoes controlled rolling at temperatures between 900-1100°C, followed by accelerated cooling to achieve optimal grain refinement and mechanical properties. Thermomechanical controlled processing (TMCP) ensures consistent microstructure and enhanced toughness.

Heat Treatment Options

While JIS SM490 is typically supplied in the as-rolled condition, various heat treatment options are available including normalizing (900-950°C), stress relieving (580-650°C), and controlled cooling treatments. These processes can be tailored to specific application requirements for enhanced mechanical properties or stress relief.

Welding Characteristics

The low carbon equivalent (Ceq ≤ 0.44%) of JIS SM490 provides excellent weldability with minimal preheating requirements. The steel is compatible with various welding processes including SMAW, GMAW, FCAW, and SAW. Proper welding procedures ensure full strength joints without significant heat-affected zone degradation.

Quality Standards & Testing

MetalZenith's JIS SM490 production adheres to strict quality standards including JIS G 3106 specifications. Comprehensive testing includes chemical analysis by optical emission spectroscopy, mechanical testing per JIS Z 2241, Charpy impact testing at specified temperatures, and ultrasonic inspection for internal soundness. Mill test certificates (3.1 per EN 10204) are provided with each shipment.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.18
Manganese (Mn)≤ 1.60
Silicon (Si)≤ 0.55
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.035
Chromium (Cr)≤ 0.30
Nickel (Ni)≤ 0.30
Copper (Cu)≤ 0.30
Vanadium (V)≤ 0.10
Niobium (Nb)≤ 0.05
Titanium (Ti)≤ 0.05
Aluminum (Al)≥ 0.015

⚙️ Mechanical Properties

PropertyValue
Yield Strength (min)325 MPa
Tensile Strength490-610 MPa
Elongation (min)17%
Brinell Hardness147-207 HB
Charpy V-Notch Impact Energy (0°C)≥ 27 J
Young's Modulus200-210 GPa
Shear Modulus80 GPa
Poisson's Ratio0.27-0.30
Fatigue Limit (10^7 cycles)245 MPa
Reduction of Area (min)50%

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510-1540°C
Thermal Conductivity (20°C)54 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.16 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C
Thermal Diffusivity13.8 mm²/s
Emissivity (oxidized surface)0.79

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Beams, Channels, Angles
Plate Thickness Range6-200 mm
Sheet Thickness Range1.5-6 mm
Width Range1000-4000 mm
Length Range2000-18000 mm
Standards ComplianceJIS G 3106, JIS G 3136
Surface FinishHot Rolled, Normalized, Shot Blasted
Dimensional Tolerance±0.5mm (thickness), ±5mm (width/length)
Edge ConditionMill Edge, Slit Edge, Flame Cut
Delivery ConditionAs Rolled, Normalized, Stress Relieved

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing JIS SM490

Manufacturing Advantage 1

Advanced Thermomechanical Processing

MetalZenith utilizes cutting-edge controlled rolling and accelerated cooling technologies to achieve optimal grain refinement and enhanced mechanical properties in JIS SM490 steel, ensuring superior strength and toughness characteristics.

Comprehensive Quality Control System

Our integrated quality management system includes real-time chemical analysis, automated mechanical testing, ultrasonic inspection, and statistical process control to guarantee consistent material properties and dimensional accuracy.

Manufacturing Advantage 2
Manufacturing Advantage 3

Flexible Customization & Global Supply

MetalZenith offers extensive customization options including specific dimensions, surface treatments, and packaging solutions, supported by our global distribution network and just-in-time delivery capabilities.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo