Skip to product information
1 of 1

EN S960QL

EN S960QL

Premium Ultra High Strength Steel from MetalZenith

EN S960QL is an ultra-high strength structural steel designed for demanding applications requiring exceptional strength-to-weight ratios. This quenched and tempered steel offers minimum yield strength of 960 MPa, making it ideal for critical structural components in construction, automotive, and heavy machinery industries.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we utilize state-of-the-art controlled rolling and precision heat treatment processes to produce EN S960QL with superior mechanical properties and dimensional accuracy. Our advanced vacuum degassing technology ensures exceptional cleanliness and consistent quality throughout every batch.

Key Applications & Industries

  • Heavy construction equipment and crane structures
  • Automotive chassis and safety components
  • Mining equipment and earth-moving machinery
  • Offshore platforms and marine structures
  • High-performance architectural applications

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and conducts comprehensive testing including tensile, impact, and hardness testing for every production lot. Our quality control laboratory is equipped with advanced spectrometers and mechanical testing equipment to ensure full compliance with EN 10025-6 standards.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN S960QL is a fine-grained structural steel produced through controlled rolling followed by quenching and tempering heat treatment. The steel features a tempered martensitic microstructure with fine carbide precipitates, providing exceptional strength while maintaining good toughness and weldability. The low carbon equivalent (CEV ≤ 0.65%) ensures excellent weldability without preheating in most applications.

Heat Treatment Process

MetalZenith employs a precisely controlled quenching and tempering process. The steel is austenitized at 900-950°C, followed by water quenching to achieve a martensitic structure. Subsequent tempering at 580-650°C develops the final mechanical properties while relieving internal stresses. Our computer-controlled furnaces ensure uniform heating and cooling rates throughout the material cross-section.

Manufacturing Process

Production begins with electric arc furnace melting followed by ladle refining and vacuum degassing to achieve ultra-low sulfur and phosphorus contents. Continuous casting produces high-quality billets which undergo controlled rolling in our state-of-the-art rolling mills. The thermomechanical controlled processing (TMCP) refines the grain structure and optimizes mechanical properties.

Quality Standards & Certifications

All EN S960QL products are manufactured in accordance with EN 10025-6 standard and undergo comprehensive testing including chemical analysis, tensile testing, impact testing, and hardness verification. MetalZenith maintains ISO 9001:2015, ISO 14001:2015, and OHSAS 18001 certifications. Each delivery includes complete mill test certificates with full traceability documentation and compliance with CE marking requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.20
Manganese (Mn)≤ 1.70
Silicon (Si)≤ 0.80
Phosphorus (P)≤ 0.020
Sulfur (S)≤ 0.010
Chromium (Cr)≤ 1.50
Nickel (Ni)≤ 2.00
Molybdenum (Mo)≤ 0.70
Vanadium (V)≤ 0.12
Niobium (Nb)≤ 0.06
Titanium (Ti)≤ 0.05
Boron (B)≤ 0.005
Aluminum (Al)≥ 0.015
Copper (Cu)≤ 0.50

⚙️ Mechanical Properties

PropertyValueTest Standard
Yield Strength (ReH)≥ 960 MPaEN ISO 6892-1
Tensile Strength (Rm)980-1150 MPaEN ISO 6892-1
Elongation (A5)≥ 10%EN ISO 6892-1
Impact Energy (KV) at -40°C≥ 30 JEN ISO 148-1
Brinell Hardness (HBW)300-380EN ISO 6506-1
Young's Modulus210 GPaEN ISO 6892-1
Poisson's Ratio0.30ASTM E132
Fatigue Limit (2×106 cycles)480 MPaEN 6072
Reduction of Area (Z)≥ 35%EN ISO 6892-1

🔬 Physical Properties

PropertyValueTemperature Range
Density7.85 g/cm³20°C
Melting Point1510°C-
Thermal Conductivity54 W/m·K20°C
Specific Heat Capacity500 J/kg·K20°C
Thermal Expansion Coefficient12×10-6/K20-100°C
Electrical Resistivity0.16 µΩ·m20°C
Magnetic PermeabilityFerromagnetic20°C
Curie Temperature770°C-
Thermal Diffusivity13.7 mm²/s20°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsPlates, Sheets, Bars, Profiles, TubesEN 10025-6
Plate Thickness3-100 mmEN 10029
Sheet Thickness0.5-3 mmEN 10131
Bar Diameter10-300 mmEN 10060
Width Range600-3200 mmEN 10025-6
Length Range2000-18000 mmCustomer Specified
Surface FinishHot Rolled, Pickled, Shot BlastedEN 10163
Dimensional ToleranceClass A, B, CEN 10029
Edge ConditionMill Edge, Cut Edge, Slit EdgeEN 10025-6
Heat TreatmentQuenched and Tempered (Q+T)EN 10025-6

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN S960QL

Manufacturing Advantage 1

Advanced Quenching & Tempering Technology

MetalZenith employs precision-controlled quenching and tempering processes with automated temperature monitoring systems, ensuring consistent mechanical properties and optimal grain structure throughout the entire steel section thickness.

Comprehensive Quality Control Laboratory

Our state-of-the-art testing facility features advanced optical emission spectrometers, universal testing machines, and Charpy impact testers, providing complete chemical and mechanical property verification for every production batch.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply Chain

MetalZenith offers extensive customization including precision cutting, machining, and surface treatments, backed by our global distribution network ensuring reliable delivery to customers worldwide with full traceability documentation.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo