EN S690QL is a thermomechanically rolled, quenched and tempered high strength structural steel offering exceptional mechanical properties with excellent weldability. This advanced steel grade provides minimum yield strength of 690 MPa while maintaining superior toughness and formability characteristics essential for demanding structural applications.

MetalZenith Manufacturing Excellence

MetalZenith leverages state-of-the-art thermomechanical controlled processing (TMCP) technology combined with precision quenching and tempering facilities to produce EN S690QL steel with consistent microstructure and superior mechanical properties. Our advanced rolling mills and heat treatment systems ensure optimal grain refinement and uniform property distribution throughout the material thickness.

Key Applications & Industries

  • Heavy construction machinery and mobile cranes
  • Mining equipment and earthmoving machinery
  • Offshore platforms and marine structures
  • Bridge construction and structural steelwork
  • Pressure vessels and storage tanks
  • Wind energy tower components

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control systems including advanced spectroscopic analysis, mechanical testing laboratories, and non-destructive testing capabilities. All EN S690QL products are manufactured under ISO 9001:2015 certification with full traceability and compliance to EN 10025-6 standards, ensuring consistent quality and performance for critical applications.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN S690QL is a low-alloy, high-strength structural steel produced through advanced thermomechanical controlled processing (TMCP) followed by quenching and tempering heat treatment. The steel exhibits a fine-grained tempered martensitic microstructure with excellent combination of strength, toughness, and weldability. The controlled chemical composition with optimized carbon equivalent ensures superior mechanical properties while maintaining good formability and machinability characteristics.

Heat Treatment Process

MetalZenith employs precision-controlled quenching from austenitizing temperature of 900-950°C followed by tempering at 580-650°C to achieve the required mechanical properties. The quenching process utilizes advanced cooling systems to ensure uniform transformation throughout the material cross-section, while the tempering treatment optimizes the balance between strength and toughness. This heat treatment cycle produces a stable microstructure with excellent dimensional stability and stress relief.

Manufacturing Process Excellence

Our state-of-the-art production facility incorporates continuous casting technology, high-precision rolling mills with computerized process control, and advanced heat treatment systems. The thermomechanical controlled processing ensures optimal grain refinement and precipitation hardening, while real-time monitoring systems guarantee consistent quality throughout production. Post-processing operations include precision cutting, surface treatment, and comprehensive quality testing to meet exact customer specifications.

Quality Standards & Certifications

All EN S690QL steel products manufactured by MetalZenith comply with EN 10025-6 European standards and are produced under ISO 9001:2015 quality management system. Our comprehensive testing protocols include chemical analysis using optical emission spectroscopy, mechanical property verification through tensile and impact testing, ultrasonic inspection for internal soundness, and dimensional verification. Each delivery includes complete mill test certificates with full traceability documentation, ensuring compliance with international quality standards and customer specifications.

🧪 Chemical Composition

ElementComposition (%)Specification
Carbon (C)≤ 0.20EN 10025-6
Manganese (Mn)≤ 1.70EN 10025-6
Silicon (Si)≤ 0.80EN 10025-6
Phosphorus (P)≤ 0.025EN 10025-6
Sulfur (S)≤ 0.015EN 10025-6
Chromium (Cr)≤ 1.50EN 10025-6
Nickel (Ni)≤ 2.00EN 10025-6
Molybdenum (Mo)≤ 0.70EN 10025-6
Vanadium (V)≤ 0.12EN 10025-6
Niobium (Nb)≤ 0.06EN 10025-6
Titanium (Ti)≤ 0.05EN 10025-6
Boron (B)≤ 0.005EN 10025-6

⚙️ Mechanical Properties

PropertyValueTest Standard
Yield Strength (Rp0.2)≥ 690 MPaEN ISO 6892-1
Tensile Strength (Rm)770-940 MPaEN ISO 6892-1
Elongation (A5)≥ 14%EN ISO 6892-1
Impact Energy (KV) at -40°C≥ 30 JEN ISO 148-1
Impact Energy (KV) at -60°C≥ 27 JEN ISO 148-1
Brinell Hardness (HBW)230-300EN ISO 6506-1
Young's Modulus210 GPaEN ISO 6892-1
Poisson's Ratio0.30ASTM E132
Fatigue Limit (2×106 cycles)320 MPaEN 6072
Fracture Toughness (KIC)150 MPa·m1/2ASTM E399

🔬 Physical Properties

PropertyValueTemperature Range
Density7.85 g/cm³20°C
Melting Point1510°C-
Thermal Conductivity54 W/m·K20°C
Thermal Expansion Coefficient12×10-6/K20-100°C
Specific Heat Capacity500 J/kg·K20°C
Electrical Resistivity0.16 µΩ·m20°C
Magnetic PermeabilityFerromagnetic20°C
Thermal Diffusivity13.8 mm²/s20°C
Curie Temperature770°C-
Emissivity0.85600°C

📏 Product Specifications

SpecificationAvailable OptionsStandards
Product FormsPlates, Sheets, Bars, Profiles, TubesEN 10025-6
Plate Thickness3-100 mmEN 10025-6
Sheet Thickness0.5-3.0 mmEN 10025-6
Width Range1000-4000 mmEN 10025-6
Length Range2000-18000 mmEN 10025-6
Surface FinishHot Rolled, Pickled, Shot BlastedEN 10163
Dimensional ToleranceClass A, B, CEN 10051
Flatness Tolerance≤ 5 mm/mEN 10029
Edge ConditionMill Edge, Trimmed EdgeEN 10025-6
Delivery ConditionQuenched and Tempered (+QT)EN 10025-6

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN S690QL

Manufacturing Advantage 1

Advanced TMCP Technology

MetalZenith utilizes cutting-edge Thermomechanical Controlled Processing (TMCP) technology with precision-controlled rolling temperatures and deformation schedules, ensuring optimal microstructure refinement and superior mechanical properties in EN S690QL steel production.

Comprehensive Quality Control

Our integrated quality management system features real-time chemical composition monitoring, automated mechanical testing, and advanced non-destructive testing capabilities, guaranteeing consistent EN S690QL steel properties and full compliance with international standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing Solutions

MetalZenith offers extensive customization capabilities including precision cutting, forming, heat treatment modifications, and surface finishing services, enabling tailored EN S690QL steel solutions for specific application requirements with global logistics support.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo