Skip to product information
1 of 1

AISI 6150

AISI 6150

AISI 6150 Chrome Vanadium Spring Steel

AISI 6150 is a high-strength, low-alloy chrome vanadium spring steel renowned for its exceptional fatigue resistance, toughness, and hardenability. This versatile steel grade combines excellent mechanical properties with superior performance in demanding applications requiring high stress resistance and durability.

MetalZenith's Manufacturing Excellence

As a leading steel manufacturer, MetalZenith employs state-of-the-art electric arc furnace technology and advanced secondary refining processes to produce premium-grade AISI 6150 steel. Our controlled atmosphere heat treatment facilities ensure optimal microstructure development, while our precision rolling and forging capabilities deliver consistent mechanical properties throughout the material cross-section.

Key Applications

  • Automotive leaf springs and coil springs
  • Heavy-duty suspension components
  • Agricultural machinery springs
  • Railway vehicle suspension systems
  • Industrial machinery components
  • High-stress fasteners and bolts

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control measures including chemical analysis, mechanical testing, and non-destructive examination. Our advanced laboratory facilities perform fatigue testing, impact testing, and metallographic analysis to ensure every batch meets stringent specifications. We provide full material traceability and certification documentation for critical applications.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AISI 6150 is a medium-carbon, low-alloy steel with chromium and vanadium additions that provide enhanced hardenability, strength, and fatigue resistance. The chromium content improves corrosion resistance and hardenability, while vanadium acts as a grain refiner and carbide former, contributing to improved toughness and wear resistance. The steel exhibits excellent through-hardening properties in sections up to 100mm diameter.

Heat Treatment Process

MetalZenith employs controlled atmosphere furnaces for optimal heat treatment of AISI 6150. Austenitizing is performed at 845-870°C, followed by oil quenching to achieve martensitic structure. Tempering at 400-650°C develops the desired combination of strength and toughness. Our computer-controlled systems ensure uniform heating rates and precise temperature control throughout the process, resulting in consistent mechanical properties.

Manufacturing Process

Our AISI 6150 steel production begins with electric arc furnace melting using premium scrap and alloy additions. Secondary refining through ladle furnace and vacuum degassing ensures low inclusion content and optimal cleanliness. Continuous casting produces high-quality billets, which are subsequently hot rolled or forged to final dimensions. Advanced rolling mill technology with computerized process control ensures excellent surface quality and dimensional accuracy.

Quality Standards & Testing

MetalZenith maintains strict quality control throughout production, conducting chemical analysis via optical emission spectrometry, mechanical testing including tensile, impact, and fatigue testing, and metallographic examination. All products comply with ASTM A29, SAE J404, and EN 10083-3 standards. Non-destructive testing including ultrasonic and magnetic particle inspection ensures internal soundness. Complete material certification and test reports accompany every shipment.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.48 - 0.53
Manganese (Mn)0.70 - 1.00
Silicon (Si)0.15 - 0.30
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.040
Chromium (Cr)0.80 - 1.10
Vanadium (V)0.15 - 0.25
Nickel (Ni)≤ 0.25
Copper (Cu)≤ 0.25

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Quenched & Tempered)1380 - 1620 MPa
Yield Strength (0.2% Offset)≥ 1240 MPa
Elongation in 50mm≥ 10%
Reduction of Area≥ 40%
Hardness (Quenched & Tempered)42 - 48 HRC
Impact Energy (Charpy V-notch)≥ 27 J
Fatigue Limit (10&sup7; cycles)620 - 690 MPa
Elastic Modulus210 GPa
Poisson's Ratio0.27 - 0.30

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1480 - 1520°C
Thermal Expansion Coefficient (20-100°C)11.5×10-6/K
Thermal Conductivity (at 20°C)42 W/m·K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity0.25 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature770°C

📏 Product Specifications

SpecificationAvailable Options
Product FormsRound bars, flat bars, plates, sheets, forgings, wire
Round Bar Diameter6mm - 300mm
Flat Bar Dimensions10mm - 150mm thickness, up to 500mm width
Plate Thickness8mm - 100mm
LengthUp to 12 meters (custom lengths available)
StandardsASTM A29, ASTM A322, SAE J404, EN 10083-3
Surface FinishHot rolled, cold drawn, peeled, ground, machined
Dimensional Tolerance±0.1mm to ±0.5mm (depending on size and finish)
Heat Treatment ConditionAnnealed, normalized, quenched & tempered

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AISI 6150

Manufacturing Advantage 1

Advanced Heat Treatment Technology

MetalZenith utilizes computer-controlled atmosphere furnaces with precise temperature profiling and quench rate optimization to achieve superior microstructure uniformity and mechanical properties in AISI 6150 steel, ensuring consistent performance across all product dimensions.

Comprehensive Quality Testing

Our state-of-the-art testing laboratory performs extensive fatigue testing, Charpy impact analysis, and stress-strain evaluation on every production lot, guaranteeing that our AISI 6150 steel meets or exceeds industry standards for spring applications and high-stress components.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply

MetalZenith offers complete customization services including precision cutting, heat treatment to customer specifications, and surface finishing. Our global distribution network ensures reliable delivery of AISI 6150 steel products worldwide with full technical support and engineering consultation.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo