20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
Spring Steel exhibits a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The high carbon content combined with chromium and vanadium additions provides exceptional elastic properties and fatigue resistance. The fine-grained structure ensures uniform mechanical properties and superior performance under cyclic loading conditions typical in structural applications.
Heat Treatment Process
MetalZenith employs precision-controlled austenitizing at 830-860°C followed by oil quenching and tempering at 400-500°C. This specialized heat treatment cycle optimizes the balance between hardness and toughness while maintaining excellent elastic recovery properties essential for structural performance.
Manufacturing Process
Our advanced manufacturing process includes electric arc furnace melting, continuous casting, and controlled rolling with precise temperature control. Secondary refining ensures low inclusion content and optimal cleanliness, critical for fatigue performance in structural applications. Quality control includes ultrasonic testing and comprehensive mechanical property verification.
Specialized Quality Testing
MetalZenith conducts comprehensive testing including welding performance evaluation using standard procedures, forming capability assessment through bend testing, fatigue strength testing under cyclic loading, and atmospheric corrosion resistance testing in simulated environmental conditions. These tests ensure optimal performance in structural applications.
Structural Application Considerations
For building structures and bridge engineering, Spring Steel provides excellent load-bearing capacity and dynamic response characteristics. In machinery manufacturing and vehicle construction, its superior fatigue resistance ensures long service life under operational stresses. General engineering applications benefit from its combination of strength, elasticity, and formability, making it ideal for complex structural geometries and demanding service conditions.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.50 - 0.70 |
| Manganese (Mn) | 0.60 - 1.00 |
| Silicon (Si) | 0.15 - 0.35 |
| Phosphorus (P) | ≤ 0.030 |
| Sulfur (S) | ≤ 0.030 |
| Chromium (Cr) | 0.70 - 1.20 |
| Vanadium (V) | 0.10 - 0.25 |
| Nickel (Ni) | ≤ 0.30 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Yield Strength (MPa) | 1200 - 1400 |
| Tensile Strength (MPa) | 1400 - 1600 |
| Elongation (%) | 8 - 12 |
| Impact Energy at 20°C (J) | ≥ 15 |
| Hardness (HRC) | 42 - 50 |
| Fatigue Strength (MPa) | 600 - 800 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density (g/cm3) | 7.85 |
| Melting Point (°C) | 1460 - 1520 |
| Thermal Conductivity (W/m·K) | 42.6 |
| Thermal Expansion (×10??/K) | 11.5 |
| Elastic Modulus (GPa) | 210 |
| Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Bars, Strips, Wire, Forgings |
| Thickness Range | 0.5 - 80mm |
| Width Range | 10 - 2000mm |
| Length Range | 1000 - 12000mm |
| Standards Compliance | ASTM A684, SAE 5160, EN 10089, JIS G4801 |
| Heat Treatment Condition | Quenched and Tempered |
| Surface Finish | Hot Rolled, Cold Rolled, Polished |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing Spring Steel
Advanced Heat Treatment Processing
MetalZenith utilizes precision-controlled quenching and tempering processes with real-time temperature monitoring to achieve optimal hardness and elasticity balance. Our specialized heat treatment ensures consistent mechanical properties and enhanced fatigue resistance throughout the material cross-section.
Comprehensive Structural Testing
Our Spring Steel undergoes extensive testing including welding performance evaluation, forming capability assessment, fatigue strength testing, and atmospheric corrosion resistance analysis. This comprehensive testing ensures superior performance in structural applications requiring long-term durability.
Custom Fabrication Services
MetalZenith provides complete custom processing services including precision cutting, forming, heat treatment, and surface finishing. Our technical team offers expert consultation for structural design optimization and material selection to meet specific engineering requirements.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications