Premium JIS SUS304L Stainless Steel from MetalZenith

MetalZenith proudly manufactures JIS SUS304L, a low-carbon austenitic stainless steel equivalent to AISI 304L, engineered for superior corrosion resistance and weldability. Our advanced production facilities utilize state-of-the-art melting and refining technologies to ensure consistent chemical composition and exceptional material properties.

MetalZenith Manufacturing Excellence

Our integrated steel production complex features advanced AOD (Argon Oxygen Decarburization) refining systems and precision rolling mills, enabling us to produce JIS SUS304L with ultra-low carbon content (≤ 0.030%) and superior surface quality. Our continuous casting technology ensures homogeneous microstructure and eliminates segregation issues common in conventional production methods.

Key Applications & Industries

  • Chemical processing equipment and storage tanks
  • Food and beverage processing machinery
  • Pharmaceutical and biotechnology equipment
  • Architectural and decorative applications
  • Marine and coastal construction projects

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and adheres to JIS G4303 standards. Our comprehensive quality control includes spectroscopic analysis, mechanical testing, and corrosion resistance evaluation. Each batch undergoes rigorous inspection using advanced NDT methods including ultrasonic testing and eddy current inspection to ensure defect-free delivery.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

JIS SUS304L is an austenitic stainless steel with a face-centered cubic crystal structure that provides excellent ductility and formability. The low carbon content (≤ 0.030%) minimizes carbide precipitation during welding and high-temperature exposure, ensuring superior intergranular corrosion resistance. The balanced chromium-nickel composition creates a stable austenitic matrix that remains non-magnetic in the annealed condition.

Heat Treatment Process

MetalZenith employs controlled solution annealing at 1010-1120°C followed by rapid cooling to achieve optimal microstructure. Our continuous annealing lines feature precise temperature control (±5°C) and protective atmosphere processing to prevent oxidation and ensure consistent mechanical properties. Post-annealing pickling and passivation treatments enhance surface corrosion resistance.

Manufacturing Process Excellence

Our integrated production process begins with electric arc furnace melting followed by AOD refining to achieve precise chemical composition. Continuous casting produces high-quality billets that undergo hot rolling, cold rolling, and precision finishing. Advanced process control systems monitor temperature, reduction ratios, and surface quality throughout production to ensure consistent material properties.

Quality Standards & Testing

All JIS SUS304L products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical property evaluation per JIS Z2241, and corrosion resistance testing according to ASTM A262. Our quality management system ensures full traceability from raw materials to finished products, with complete mill test certificates provided for every shipment.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.030
Silicon (Si)≤ 1.00
Manganese (Mn)≤ 2.00
Phosphorus (P)≤ 0.045
Sulfur (S)≤ 0.030
Chromium (Cr)18.00 - 20.00
Nickel (Ni)8.00 - 12.00
Nitrogen (N)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Tensile Strength≥ 520 MPa
Yield Strength (0.2% Offset)≥ 205 MPa
Elongation (50mm gauge)≥ 40%
Hardness (Brinell)≤ 200 HB
Hardness (Rockwell B)≤ 90 HRB
Impact Energy (Charpy V-notch, 20°C)≥ 120 J
Young's Modulus200 GPa
Fatigue Limit (107 cycles)240 MPa

🔬 Physical Properties

PropertyValue
Density (20°C)8.00 g/cm³
Melting Point1400-1450°C
Thermal Conductivity (20°C)16.2 W/m·K
Thermal Expansion Coefficient (20-100°C)17.3×10-6/K
Specific Heat Capacity (20°C)500 J/kg·K
Electrical Resistivity (20°C)0.72 µΩ·m
Magnetic Permeability1.02 (Non-magnetic)
Thermal Diffusivity (20°C)4.05×10-6 m²/s

📏 Product Specifications

SpecificationAvailable Options
Product FormsSheets, Plates, Coils, Bars, Rods, Tubes, Pipes
Sheet Thickness0.3mm - 6.0mm
Plate Thickness6.0mm - 100mm
Bar Diameter6mm - 300mm
Tube Outer Diameter6mm - 219mm
Standards ComplianceJIS G4303, ASTM A240, EN 10088-2
Surface Finishes2B, BA, No.4, HL (Hairline), Mirror
Dimensional Tolerance±0.02mm to ±0.5mm (depending on form)
Edge ConditionMill Edge, Slit Edge, Trimmed Edge

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing JIS SUS304L

Manufacturing Advantage 1

Advanced AOD Refining Technology

MetalZenith employs cutting-edge Argon Oxygen Decarburization (AOD) technology to achieve ultra-low carbon content (≤ 0.030%) while maintaining optimal chromium and nickel levels. Our proprietary refining process ensures superior chemical homogeneity and eliminates carbide precipitation, resulting in enhanced corrosion resistance and weldability compared to conventional production methods.

Comprehensive Quality Control System

Our integrated quality management system features real-time spectroscopic monitoring, automated dimensional inspection, and advanced surface quality assessment. Every coil and batch undergoes rigorous testing including intergranular corrosion testing (ASTM A262), ensuring consistent material properties and compliance with JIS G4303 standards throughout the entire production process.

Manufacturing Advantage 2
Manufacturing Advantage 3

Flexible Customization & Global Supply

MetalZenith offers extensive customization capabilities including precision cold rolling, specialized surface finishes (2B, BA, No.4), and custom dimensional tolerances. Our global distribution network ensures reliable delivery worldwide, while our technical support team provides comprehensive material selection guidance and application engineering services to optimize performance for specific customer requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo