Nitronic 50 Stainless Steel

Nitronic 50 Stainless Steel

Nitronic 50 Super Austenitic Stainless Steel

Nitronic 50 is a nitrogen-strengthened super austenitic stainless steel offering exceptional strength, superior corrosion resistance, and outstanding galling resistance. This premium grade combines the corrosion resistance of 316L with nearly twice the yield strength, making it ideal for demanding applications in chemical processing, marine environments, and high-stress mechanical components.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs advanced vacuum melting and controlled nitrogen addition processes to produce Nitronic 50 with superior mechanical properties and microstructural stability. Our precision solution annealing and controlled cooling techniques ensure optimal austenitic structure formation and nitrogen retention, critical for achieving maximum strength and corrosion resistance.

Key Applications

  • Chemical processing equipment and reactor vessels
  • Food processing machinery and pharmaceutical equipment
  • Medical implants and surgical instruments
  • Marine hardware and offshore platform components
  • Architectural facades and decorative structural elements

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including pitting potential testing, intergranular corrosion evaluation, stress corrosion cracking assessment, and passivation film thickness measurement. Our Nitronic 50 meets ASTM A240, ASME SA-240, and FDA compliance requirements, ensuring reliability in critical chemical, food, and medical applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Nitronic 50 features a fully austenitic microstructure strengthened by controlled nitrogen addition. The nitrogen atoms occupy interstitial positions in the austenite lattice, providing solid solution strengthening while maintaining excellent ductility and toughness. The balanced chromium-nickel-manganese composition ensures stable austenite formation and prevents harmful phase precipitation during service.

Heat Treatment Process

MetalZenith employs solution annealing at 1900-2100°F (1040-1150°C) followed by rapid water quenching to retain nitrogen in solution and achieve optimal mechanical properties. Our controlled cooling process prevents carbide precipitation and maintains the homogeneous austenitic structure essential for corrosion resistance.

Advanced Manufacturing Process

MetalZenith utilizes vacuum induction melting with controlled nitrogen atmosphere to achieve precise chemical composition and minimize inclusions. Our hot rolling and cold finishing processes are optimized to maintain uniform properties while achieving excellent surface quality suitable for critical applications.

Specialized Quality Testing

Comprehensive testing protocols include pitting potential measurement exceeding 1000mV vs SCE, ASTM A262 Practice A, E intergranular corrosion testing, stress corrosion cracking evaluation per ASTM G36, and passivation film analysis using X-ray photoelectron spectroscopy to ensure superior corrosion performance in chloride environments.

Application-Specific Considerations

For chemical processing equipment, Nitronic 50 provides excellent resistance to pitting and crevice corrosion in chloride-containing media. In food industry applications, its FDA compliance and easy cleanability make it ideal for processing equipment. Medical device applications benefit from its biocompatibility and high strength-to-weight ratio. Marine applications leverage its superior resistance to seawater corrosion, while architectural applications utilize its attractive appearance and low maintenance requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.06
Chromium (Cr)21.0 - 23.0
Nickel (Ni)11.5 - 13.5
Manganese (Mn)4.0 - 6.0
Silicon (Si)≤ 1.0
Nitrogen (N)0.20 - 0.40
Molybdenum (Mo)1.5 - 3.0
Phosphorus (P)≤ 0.04
Sulfur (S)≤ 0.03

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 380
Tensile Strength (MPa)760 - 1035
Elongation (%)≥ 35
Hardness (HRB)95 - 102
Pitting Resistance (PREN)≥ 34
Impact Energy at RT (J)≥ 150

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.9
Melting Point (°C)1400 - 1420
Thermal Conductivity (W/m·K)14.2
Thermal Expansion (×10??/K)16.0
Electrical Resistivity (μΩ·cm)85
Elastic Modulus (GPa)200

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Rods, Pipes, Forgings
Thickness Range0.5 - 150mm
Width Range1000 - 2500mm
Length Range2000 - 12000mm
Standards ComplianceASTM A240, ASME SA-240, UNS S20910
Heat Treatment ConditionSolution Annealed and Pickled
Surface Finish2B, BA, No.4, No.8, Custom

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Nitronic 50 Stainless Steel

Manufacturing Advantage 1

Advanced Nitrogen-Enhanced Processing

MetalZenith utilizes controlled vacuum melting with precise nitrogen addition and solution annealing at 1900-2100°F to achieve optimal austenitic microstructure. Our advanced processing ensures uniform nitrogen distribution and maximum strength development while maintaining excellent corrosion resistance properties.

Comprehensive Corrosion Testing Protocol

MetalZenith conducts extensive specialized testing including pitting potential measurement (>1000mV vs SCE), ASTM A262 intergranular corrosion testing, stress corrosion cracking evaluation in chloride environments, and passivation film thickness analysis using XPS technology to ensure superior corrosion performance.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Fabrication & Technical Support

MetalZenith provides comprehensive custom processing services including precision machining, forming, welding consultation, and heat treatment optimization. Our metallurgical engineers offer technical support for application-specific requirements in chemical, food, medical, and marine industries.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo