ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

XM-19 Stainless Steel

XM-19 Stainless Steel

XM-19 Super-Austenitic Stainless Steel

XM-19 is a super-austenitic stainless steel specifically engineered for extreme corrosion resistance in highly aggressive environments. This nitrogen-strengthened grade offers exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking, making it ideal for critical applications in chemical processing, marine environments, and high-temperature service conditions.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum induction melting and electroslag remelting processes to produce XM-19 with superior chemical homogeneity and cleanliness. Our advanced solution annealing and controlled cooling techniques ensure optimal austenitic microstructure and maximum corrosion resistance, critical for demanding industrial applications.

Key Applications

  • Chemical processing equipment and reactors
  • Food and pharmaceutical processing systems
  • Medical implants and surgical instruments
  • Offshore oil and gas production platforms
  • Architectural facades and decorative elements

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including comprehensive corrosion testing, pitting potential analysis, intergranular corrosion testing per ASTM A262, and stress corrosion cracking evaluation. Our XM-19 meets ASTM A240, ASME SA-240, and FDA requirements for food contact applications, ensuring reliability in critical service environments.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

XM-19 exhibits a fully austenitic microstructure stabilized by high nickel content and nitrogen addition. The controlled nitrogen content provides solid solution strengthening while enhancing pitting and crevice corrosion resistance. The absence of ferrite phase ensures excellent toughness and prevents sigma phase formation during elevated temperature exposure.

Heat Treatment Process

MetalZenith employs solution annealing at 1100-1150°C followed by rapid water quenching to achieve optimal corrosion resistance and mechanical properties. Our controlled atmosphere furnaces prevent surface oxidation and maintain precise temperature uniformity throughout the material cross-section.

Advanced Manufacturing Process

Our production process begins with vacuum induction melting using high-purity raw materials, followed by electroslag remelting for enhanced cleanliness. Hot working is performed within carefully controlled temperature ranges to prevent cracking, followed by solution annealing and descaling treatments to achieve superior surface quality.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including pitting potential measurement exceeding 1000mV vs SCE, intergranular corrosion testing per ASTM A262 Practice E, stress corrosion cracking evaluation in boiling MgCl2 solution, and passivation film analysis using X-ray photoelectron spectroscopy to verify optimal surface chemistry.

Application-Specific Considerations

For chemical processing applications, XM-19 provides exceptional resistance to chloride-containing environments and organic acids. In food industry applications, the material meets FDA requirements with superior cleanability and bacterial resistance. Medical device applications benefit from biocompatibility and MRI compatibility. Marine applications leverage the high PREN value for seawater resistance, while architectural applications utilize the material's aesthetic appeal and long-term durability.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.03
Chromium (Cr)20.0 - 22.0
Nickel (Ni)23.0 - 25.0
Molybdenum (Mo)6.0 - 7.0
Nitrogen (N)0.15 - 0.25
Manganese (Mn)≤ 2.0
Silicon (Si)≤ 1.0
Copper (Cu)0.5 - 1.0

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 350
Tensile Strength (MPa)690 - 900
Elongation (%)≥ 35
Hardness (HRB)≤ 95
Pitting Resistance (PREN)≥ 42
Impact Energy at RT (J)≥ 100

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.1
Melting Point (°C)1350 - 1400
Thermal Conductivity (W/m·K)14.2
Thermal Expansion (×10??/K)16.5
Electrical Resistivity (μΩ·cm)95
Elastic Modulus (GPa)200

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Tubes, Forgings, Wire
Thickness Range0.5 - 80mm
Width Range1000 - 2500mm
Length Range2000 - 12000mm
Standards ComplianceASTM A240, ASME SA-240, EN 10088
Surface Finish2B, BA, No.4, No.8, Custom
Heat Treatment ConditionSolution Annealed and Pickled

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing XM-19 Stainless Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to achieve exceptional chemical homogeneity and ultra-low inclusion content. Our controlled atmosphere processing ensures optimal nitrogen content and prevents carbide precipitation, maximizing corrosion resistance and mechanical properties.

Comprehensive Corrosion Testing Protocol

MetalZenith conducts extensive corrosion testing including pitting potential measurement (>1000mV vs SCE), intergranular corrosion testing per ASTM A262 Practice E, stress corrosion cracking evaluation in chloride environments, and passivation film thickness analysis using XPS technology to ensure superior corrosion performance.

Manufacturing Advantage 2
Manufacturing Advantage 3

Specialized Processing & Technical Support

MetalZenith offers comprehensive custom processing including precision machining, specialized welding procedures, and surface finishing treatments. Our metallurgical experts provide technical consultation for material selection, fabrication guidelines, and application-specific heat treatment recommendations.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo