ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

Super Duplex Stainless Steel

Super Duplex Stainless Steel

Super Duplex Stainless Steel - Ultimate Corrosion Resistance

Super Duplex Stainless Steel is an advanced high-performance alloy featuring exceptional corrosion resistance, superior mechanical strength, and outstanding durability in the most aggressive environments. This premium grade combines the benefits of austenitic and ferritic structures, delivering unmatched performance in extreme corrosive conditions where standard stainless steels fail.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art solution annealing and controlled cooling processes to achieve optimal duplex microstructure with balanced austenite-ferrite phases. Our advanced metallurgical processing ensures superior pitting resistance, enhanced chloride stress corrosion cracking resistance, and exceptional mechanical properties critical for extreme environment applications.

Key Applications

  • Seawater desalination plants and reverse osmosis systems
  • Petrochemical processing equipment and heat exchangers
  • Nuclear power plant components and reactor vessels
  • Deep-sea drilling equipment and subsea manifolds
  • Chemical processing in highly corrosive environments
  • Offshore oil and gas production platforms

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including critical pitting temperature testing, crevice corrosion potential analysis, stress corrosion threshold evaluation, and comprehensive chloride ion resistance testing. Our Super Duplex steel meets ASTM A790, NACE MR0175, and major international standards, ensuring reliability in the most demanding corrosive applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Super Duplex Stainless Steel features a balanced duplex microstructure consisting of approximately 50% austenite and 50% ferrite phases. This unique dual-phase structure combines the excellent corrosion resistance of austenitic grades with the high strength and stress corrosion cracking resistance of ferritic grades. The high chromium, molybdenum, and nitrogen content provides exceptional pitting and crevice corrosion resistance, with PREN values exceeding 40.

Heat Treatment Process

MetalZenith employs solution annealing at 1020-1100°C followed by rapid water quenching to achieve optimal duplex microstructure. This controlled thermal processing prevents harmful intermetallic phase formation while ensuring balanced austenite-ferrite ratio. Post-weld heat treatment at 1050°C may be applied for heavy section welded components to restore optimal corrosion resistance.

Advanced Manufacturing Process

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to ensure chemical homogeneity and minimize inclusions. Our controlled rolling and forging processes maintain optimal grain structure while preventing excessive ferrite formation. Advanced quality control includes ferrite content measurement, intergranular corrosion testing, and comprehensive mechanical property verification.

Specialized Corrosion Testing

MetalZenith conducts comprehensive corrosion evaluation including Critical Pitting Temperature testing in 1M NaCl solution, Crevice Corrosion Potential measurement, Stress Corrosion Cracking threshold determination in chloride environments, and Chloride Ion Resistance testing up to 25% concentration. These specialized tests ensure superior performance in aggressive marine and chemical processing environments.

Application-Specific Engineering

For seawater desalination applications, MetalZenith optimizes material composition for maximum chloride resistance and thermal stability. In petrochemical environments, special attention is given to hydrogen sulfide resistance and high-temperature performance. Nuclear industry applications require enhanced radiation resistance and strict quality documentation. Deep-sea equipment demands superior mechanical properties at low temperatures combined with exceptional seawater corrosion resistance.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.030
Chromium (Cr)24.0 - 26.0
Nickel (Ni)6.0 - 8.0
Molybdenum (Mo)3.0 - 4.0
Tungsten (W)0.5 - 1.0
Nitrogen (N)0.24 - 0.32
Manganese (Mn)≤ 1.20
Silicon (Si)≤ 0.80

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 550
Tensile Strength (MPa)750 - 950
Elongation (%)≥ 25
Hardness (HRC)≤ 32
Critical Pitting Temperature (°C)≥ 80
PREN Value≥ 40
Impact Energy at -40°C (J)≥ 60

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.8
Melting Point (°C)1350 - 1400
Thermal Conductivity (W/m·K)17
Thermal Expansion (×10??/K)13.0
Elastic Modulus (GPa)200
Magnetic PermeabilityFerromagnetic

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Pipes, Tubes, Forgings, Fittings
Thickness Range0.5 - 150mm
Width Range1000 - 3000mm
Length Range2000 - 12000mm
Standards ComplianceASTM A790, A928, NACE MR0175, EN 10088
Heat Treatment ConditionSolution Annealed and Quenched
Surface Finish2B, BA, No.4, Pickled, Polished

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Super Duplex Stainless Steel

Manufacturing Advantage 1

Advanced Solution Annealing Process

MetalZenith employs precision solution annealing at 1020-1100°C with controlled cooling rates to achieve optimal duplex microstructure. Our advanced thermal processing ensures balanced austenite-ferrite phases (45-55% each), maximizing corrosion resistance and mechanical strength for extreme environment applications.

Comprehensive Corrosion Testing Protocol

MetalZenith conducts extensive specialized testing including Critical Pitting Temperature (CPT) testing up to 80°C, Crevice Corrosion Potential analysis, Stress Corrosion Cracking threshold evaluation, and Chloride Ion Resistance testing up to 25% NaCl solutions, ensuring superior performance in aggressive marine and chemical environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Engineering Solutions

MetalZenith provides comprehensive custom fabrication services including precision machining, specialized welding with matching filler metals, and tailored heat treatment protocols. Our technical team offers application-specific material selection and processing optimization for critical corrosive environment applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications