ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

EN 1.4462

EN 1.4462

Premium EN 1.4462 Duplex Steel Manufacturing

EN 1.4462, also known as SAF 2205 or UNS S32205, is a premium duplex stainless steel that combines exceptional corrosion resistance with superior mechanical strength. This austenitic-ferritic stainless steel contains approximately 22% chromium, 5% nickel, and 3% molybdenum, delivering outstanding performance in demanding industrial applications.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art vacuum induction melting and electroslag remelting technologies to produce EN 1.4462 with exceptional purity and homogeneity. Our advanced thermomechanical processing ensures optimal duplex microstructure with balanced austenite and ferrite phases, maximizing both strength and corrosion resistance.

Key Applications & Industries

  • Oil and gas industry: Offshore platforms, pipelines, and subsea equipment
  • Chemical processing: Heat exchangers, pressure vessels, and reactor components
  • Marine applications: Propeller shafts, pump components, and seawater systems
  • Pulp and paper industry: Digesters, bleach plants, and recovery boilers

Quality Assurance & Certification

MetalZenith maintains ISO 9001:2015, ISO 14001, and OHSAS 18001 certifications. Every batch undergoes comprehensive testing including chemical analysis, mechanical testing, and corrosion resistance evaluation. We provide full material traceability and third-party inspection certificates to ensure complete compliance with international standards.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

EN 1.4462 exhibits a balanced duplex microstructure consisting of approximately 50% austenite and 50% ferrite phases. This unique dual-phase structure provides exceptional strength-to-weight ratio and superior resistance to stress corrosion cracking compared to conventional austenitic stainless steels. The high chromium, molybdenum, and nitrogen content ensures excellent pitting and crevice corrosion resistance in chloride environments.

Heat Treatment Process

Solution annealing is performed at 1020-1100°C followed by rapid cooling in water or air to maintain optimal duplex microstructure. MetalZenith's controlled cooling process prevents harmful intermetallic phase precipitation while ensuring proper ferrite-austenite balance. Post-weld heat treatment at 1050°C may be applied for stress relief in welded components.

Manufacturing Process Excellence

MetalZenith employs advanced vacuum induction melting (VIM) technology to achieve superior chemical homogeneity and cleanliness. Our thermomechanical controlled processing (TMCP) ensures optimal grain refinement and mechanical properties. Hot working is performed between 950-1150°C, while cold working capabilities allow for enhanced strength through controlled deformation.

Quality Standards & Testing

All EN 1.4462 products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical testing per ASTM A370, ferrite content measurement using magnetic methods, and corrosion testing according to ASTM G48. Ultrasonic testing, magnetic particle inspection, and dimensional verification ensure complete quality compliance. Material certificates include full traceability documentation and third-party inspection reports.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.030
Silicon (Si)≤ 1.00
Manganese (Mn)≤ 2.00
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.020
Chromium (Cr)21.0 - 23.0
Nickel (Ni)4.5 - 6.5
Molybdenum (Mo)2.5 - 3.5
Nitrogen (N)0.08 - 0.20
Copper (Cu)≤ 0.50
Tungsten (W)≤ 0.50

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Rm)≥ 640 MPa
Yield Strength 0.2% (Rp0.2)≥ 450 MPa
Elongation (A5)≥ 25%
Hardness (HRC)≤ 31
Hardness (HB)≤ 290
Impact Energy (KV) at -40°C≥ 60 J
Young's Modulus200 GPa
Fatigue Limit (107 cycles)320 MPa
Ferrite Content40-60%
PREN Value≥ 35

🔬 Physical Properties

PropertyValue
Density7.8 g/cm³
Melting Point1350-1400°C
Thermal Conductivity (20°C)14 W/m·K
Thermal Conductivity (100°C)16 W/m·K
Thermal Expansion (20-100°C)13×10-6/K
Thermal Expansion (20-300°C)14×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.85 µΩ·m
Magnetic Permeability1.5-2.0
Poisson's Ratio0.28

📏 Product Specifications

SpecificationAvailable Options
Product FormsRound bars, flat bars, plates, sheets, tubes, pipes, forgings, flanges
Round Bar Diameter6mm - 300mm
Flat Bar Dimensions10×3mm - 200×50mm
Plate Thickness3mm - 100mm
Sheet Thickness0.5mm - 6mm
Tube Outer Diameter6mm - 219mm
StandardsEN 10088, ASTM A240, A479, A790, JIS G4305, GB/T 1220
Surface FinishHot rolled, cold rolled, 2B, BA, No.4, hairline, mirror
Tolerance±0.1mm to ±0.5mm (depending on form and size)
LengthStandard: 6m, Custom: up to 12m

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing EN 1.4462

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith employs cutting-edge vacuum induction melting (VIM) and electroslag remelting (ESR) processes to achieve exceptional chemical homogeneity and purity in EN 1.4462 production. Our controlled atmosphere melting eliminates inclusions and ensures optimal duplex microstructure with balanced austenite-ferrite phases.

Comprehensive Quality Control System

Our integrated quality management system features real-time process monitoring, automated chemical analysis, and advanced metallurgical testing. Every heat of EN 1.4462 undergoes rigorous testing including PREN calculation, ferrite content measurement, and corrosion resistance evaluation to guarantee consistent performance.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain & Customization

MetalZenith maintains strategic inventory locations worldwide and offers extensive customization capabilities for EN 1.4462. From precision machining to specialized heat treatments, we provide tailored solutions with flexible delivery schedules to meet specific project requirements and tight deadlines.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo