20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
EN 1.4301 is an austenitic stainless steel with a face-centered cubic crystal structure that provides excellent ductility and toughness. The chromium content of 17.5-19.5% forms a passive oxide layer that provides superior corrosion resistance, while the nickel content of 8.0-10.5% stabilizes the austenitic structure and enhances formability.
Heat Treatment Process
MetalZenith applies solution annealing at 1050-1100°C followed by rapid cooling to achieve optimal mechanical properties. This process dissolves carbides, relieves internal stresses, and ensures uniform microstructure. The material cannot be hardened by heat treatment but can be work-hardened through cold working.
Manufacturing Process
Our production process begins with electric arc furnace melting using premium raw materials, followed by argon oxygen decarburization (AOD) refining for precise chemistry control. Continuous casting produces high-quality billets that undergo hot rolling, cold rolling, and finishing operations including pickling, annealing, and surface treatment.
Quality Standards & Testing
Every batch undergoes comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical testing per ASTM standards, intergranular corrosion testing (ASTM A262), and microstructural examination. Non-destructive testing includes ultrasonic inspection and surface quality assessment to ensure defect-free products.
Corrosion Resistance
EN 1.4301 exhibits excellent resistance to atmospheric corrosion, mild chemical environments, and food acids. The passive layer self-heals in oxidizing conditions, providing long-term durability. However, it may be susceptible to chloride-induced pitting and crevice corrosion in harsh marine environments.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | ≤ 0.070 |
| Silicon (Si) | ≤ 1.00 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Chromium (Cr) | 17.5 - 19.5 |
| Nickel (Ni) | 8.0 - 10.5 |
| Nitrogen (N) | ≤ 0.10 |
| Iron (Fe) | Balance |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Rm) | 520 - 720 MPa |
| Yield Strength (Rp0.2) | ≥ 210 MPa |
| Elongation (A5) | ≥ 45% |
| Hardness (HRB) | ≤ 92 |
| Hardness (HV) | ≤ 200 |
| Impact Energy (KV) | ≥ 120 J |
| Young's Modulus | 200 GPa |
| Fatigue Limit | 240 MPa |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.90 g/cm³ |
| Melting Point | 1400 - 1450°C |
| Thermal Expansion Coefficient (20-100°C) | 17.2×10-6/K |
| Thermal Conductivity (20°C) | 15 W/m·K |
| Specific Heat Capacity | 500 J/kg·K |
| Electrical Resistivity (20°C) | 0.73 µΩ·m |
| Magnetic Permeability | 1.02 µr |
| Curie Temperature | Non-magnetic |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Sheets, Plates, Bars, Rods, Tubes, Pipes, Coils, Strips |
| Sheet Thickness | 0.3 - 6.0 mm |
| Plate Thickness | 6.0 - 100 mm |
| Bar Diameter | 6 - 300 mm |
| Tube Outer Diameter | 6 - 610 mm |
| Surface Finishes | 2B, BA, No.4, HL, Mirror, Pickled |
| Standards | EN 10088, ASTM A240/A276/A312, JIS G4303/G4304 |
| Dimensional Tolerance | ±0.1 mm (thickness), ±2 mm (width/length) |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing EN 1.4301
Advanced Electric Arc Furnace Technology
MetalZenith utilizes cutting-edge electric arc furnace technology with precise temperature control and advanced refining processes, ensuring optimal chemical composition and superior metallurgical properties in every batch of EN 1.4301 stainless steel.
Comprehensive Quality Control System
Our state-of-the-art testing laboratory conducts rigorous chemical analysis, mechanical testing, and microstructural examination. Every product undergoes ultrasonic testing and surface inspection to guarantee compliance with international standards and customer specifications.
Global Supply Chain & Custom Solutions
MetalZenith offers flexible customization options including specific dimensions, surface finishes, and heat treatment conditions. Our global distribution network ensures reliable delivery worldwide, supported by technical engineering services and application consulting.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
สอบถามด่วน
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications