ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

AISI 410

AISI 410

AISI 410 Martensitic Stainless Steel

AISI 410 is a general-purpose martensitic stainless steel offering excellent corrosion resistance, high strength, and good wear resistance. As a leading steel manufacturer, MetalZenith produces premium-grade AISI 410 using advanced vacuum melting technology and precision rolling processes to ensure superior metallurgical properties and dimensional accuracy.

MetalZenith Manufacturing Excellence

Our state-of-the-art production facilities feature electric arc furnaces with argon oxygen decarburization (AOD) refining, enabling precise control of chemical composition and elimination of impurities. MetalZenith's advanced hot rolling and heat treatment capabilities ensure optimal microstructure development and consistent mechanical properties throughout the material.

Key Applications

  • Cutlery and surgical instruments requiring sharp edges and corrosion resistance
  • Valve components and pump shafts in mildly corrosive environments
  • Turbine blades and compressor components in power generation
  • Automotive exhaust systems and decorative trim applications
  • Industrial fasteners and hardware requiring strength and durability

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control protocols including spectroscopic analysis, mechanical testing, and non-destructive examination. Our laboratory facilities perform complete chemical analysis, tensile testing, hardness verification, and corrosion resistance evaluation to ensure compliance with ASTM A276, ASTM A479, and international standards.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AISI 410 is a straight chromium martensitic stainless steel with 11.5-13.5% chromium content, providing excellent corrosion resistance in mild environments. The martensitic microstructure develops through controlled cooling from austenitic temperatures, resulting in high strength and hardness capabilities. MetalZenith's precision melting process ensures optimal carbide distribution and grain refinement for enhanced mechanical properties.

Heat Treatment Process

Annealing: Heat to 815-870°C, hold for uniform temperature, then furnace cool to below 600°C followed by air cooling. Hardening: Austenitize at 925-1010°C, oil or air quench to achieve maximum hardness of 40 HRC. Tempering: Reheat to 150-650°C depending on desired hardness and toughness balance. MetalZenith's controlled atmosphere furnaces ensure consistent heat treatment results with minimal oxidation and decarburization.

Manufacturing Process

MetalZenith employs electric arc furnace melting with argon oxygen decarburization (AOD) refining to achieve precise chemical composition control. The molten steel undergoes vacuum degassing to minimize hydrogen and nitrogen content, followed by continuous casting into billets or slabs. Hot rolling operations utilize computer-controlled rolling mills to achieve dimensional accuracy and optimal microstructure development.

Quality Standards & Testing

All AISI 410 products undergo comprehensive testing including chemical analysis via optical emission spectroscopy, mechanical property verification through tensile and hardness testing, and microstructural examination. Non-destructive testing methods including ultrasonic inspection and magnetic particle testing ensure internal soundness. MetalZenith maintains compliance with ASTM A276, A479, A240, EN 10088, and JIS G4303 standards, with full material traceability and certification documentation provided.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.15
Manganese (Mn)≤ 1.00
Silicon (Si)≤ 1.00
Phosphorus (P)≤ 0.040
Sulfur (S)≤ 0.030
Chromium (Cr)11.5 - 13.5
Nickel (Ni)≤ 0.75
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyAnnealed ConditionHardened & Tempered
Tensile Strength485-620 MPa725-850 MPa
Yield Strength (0.2% offset)275-415 MPa550-690 MPa
Elongation (50mm)≥ 20%≥ 15%
Reduction of Area≥ 50%≥ 45%
Hardness (Brinell)155-217 HB235-285 HB
Hardness (Rockwell C)-22-32 HRC
Impact Energy (Charpy V-notch)54-81 J27-54 J
Fatigue Limit (10&sup7; cycles)240 MPa360 MPa

🔬 Physical Properties

PropertyValue
Density7.75 g/cm³
Melting Point1480-1530°C
Specific Heat (20°C)460 J/kg·K
Thermal Conductivity (100°C)24.9 W/m·K
Thermal Expansion (20-100°C)9.9×10-6/K
Thermal Expansion (20-500°C)11.2×10-6/K
Electrical Resistivity (20°C)0.57 µΩ·m
Magnetic PermeabilityFerromagnetic
Modulus of Elasticity200 GPa
Poisson's Ratio0.27-0.30

📏 Product Specifications

Product FormSize RangeStandards
Round Bars6-300mm diameterASTM A276, A479
Square Bars10-150mmASTM A276
Flat Bars3-100mm thick, up to 300mm wideASTM A276
Sheets0.5-6mm thick, up to 2000mm wideASTM A240
Plates6-100mm thick, up to 3000mm wideASTM A240
Tubes6-219mm OD, 0.5-20mm wallASTM A268
Surface FinishHot rolled, cold drawn, polished2B, BA, No.4, No.8
Tolerance±0.1mm to ±1.0mmEN 10029, ASTM A480

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AISI 410

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes state-of-the-art vacuum induction melting (VIM) and electroslag remelting (ESR) processes to produce ultra-clean AISI 410 steel with minimal inclusions, superior surface quality, and enhanced mechanical properties for critical applications.

Comprehensive Quality Control System

Our integrated quality management system features real-time process monitoring, automated testing equipment, and certified laboratory facilities ensuring 100% traceability and compliance with international standards including ASTM, EN, and JIS specifications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply

MetalZenith offers extensive customization capabilities including precision machining, heat treatment optimization, and special surface finishes. Our global distribution network ensures reliable delivery worldwide with comprehensive technical support and engineering consultation services.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo