ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

AISI 304L

AISI 304L

Premium AISI 304L Stainless Steel from MetalZenith

AISI 304L is a low-carbon variant of the widely used 304 austenitic stainless steel, offering exceptional corrosion resistance and superior weldability. With carbon content limited to ≤ 0.030%, this grade minimizes carbide precipitation during welding, making it ideal for applications requiring extensive fabrication.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art AOD (Argon Oxygen Decarburization) refining technology to precisely control carbon content and achieve optimal chemical composition. Our advanced vacuum degassing systems ensure superior cleanliness and mechanical properties, while our controlled atmosphere heat treatment facilities guarantee consistent microstructure and performance characteristics.

Versatile Applications Across Industries

  • Food processing equipment and pharmaceutical applications
  • Chemical processing vessels and piping systems
  • Architectural components and decorative applications
  • Marine hardware and coastal construction
  • Heat exchangers and pressure vessels

Quality Assurance and Certification

MetalZenith maintains ISO 9001:2015 certification and adheres to international standards including ASTM A240, EN 10088, and JIS G4305. Our comprehensive testing laboratory performs chemical analysis, mechanical testing, and non-destructive examination to ensure every product meets stringent quality requirements. We provide complete material traceability and certification documentation with each shipment.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AISI 304L exhibits a fully austenitic microstructure at room temperature due to its balanced chromium-nickel composition. The low carbon content (≤ 0.030%) significantly reduces the formation of chromium carbides during welding and high-temperature exposure, maintaining corrosion resistance in heat-affected zones. The austenitic structure provides excellent ductility and toughness across a wide temperature range.

Heat Treatment and Processing

MetalZenith employs solution annealing at 1040-1120°C followed by rapid cooling to achieve optimal properties. This treatment dissolves any carbides and provides a homogeneous austenitic structure. Cold working increases strength but reduces ductility, while the material cannot be hardened by heat treatment. Our controlled atmosphere furnaces prevent surface oxidation and ensure consistent results.

Manufacturing Process Excellence

Our production process begins with electric arc furnace melting followed by AOD refining for precise composition control. Continuous casting produces high-quality billets, which undergo hot rolling, solution annealing, and pickling. Cold rolling and precision finishing operations achieve final dimensions and surface quality. Advanced process control systems monitor temperature, atmosphere, and cooling rates throughout production.

Quality Standards and Testing

MetalZenith maintains compliance with international standards including ASTM A240, EN 10088-2, and JIS G4305. Our quality management system encompasses incoming material inspection, in-process monitoring, and final product testing. Chemical composition verification using optical emission spectroscopy, mechanical property testing, intergranular corrosion testing (ASTM A262), and dimensional inspection ensure consistent quality. Non-destructive testing including ultrasonic and dye penetrant inspection is available for critical applications.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.030
Manganese (Mn)≤ 2.00
Silicon (Si)≤ 0.75
Phosphorus (P)≤ 0.045
Sulfur (S)≤ 0.030
Chromium (Cr)18.00 - 20.00
Nickel (Ni)8.00 - 12.00
Nitrogen (N)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Tensile Strength≥ 515 MPa
Yield Strength (0.2% Offset)≥ 205 MPa
Elongation in 50mm≥ 40%
Reduction of Area≥ 50%
Hardness (Brinell)≤ 200 HB
Hardness (Rockwell B)≤ 90 HRB
Impact Energy (Charpy V-notch at 20°C)≥ 120 J
Fatigue Limit (107 cycles)240 MPa
Modulus of Elasticity200 GPa

🔬 Physical Properties

PropertyValue
Density8.00 g/cm³
Melting Point1400-1450°C
Thermal Conductivity (at 100°C)16.2 W/m·K
Thermal Expansion Coefficient (20-100°C)17.2×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (at 20°C)0.72 µΩ·m
Magnetic Permeability1.02 (Paramagnetic)
Curie TemperatureNon-magnetic

📏 Product Specifications

SpecificationAvailable Options
Product FormsSheets, Plates, Bars, Rods, Tubes, Pipes, Coils, Strips
Sheet Thickness0.3mm - 6.0mm
Plate Thickness6mm - 100mm
Bar Diameter6mm - 300mm
Tube Outer Diameter6mm - 610mm
StandardsASTM A240, A276, A312, EN 10088-2, JIS G4305, GB/T 3280
Surface Finishes2B, BA, No.4, HL (Hairline), Mirror, Pickled
Tolerance±0.1mm (thickness), ±3mm (width), ±6mm (length)
Edge ConditionMill Edge, Slit Edge, Trimmed Edge

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AISI 304L

Manufacturing Advantage 1

Advanced AOD Refining Technology

MetalZenith utilizes cutting-edge Argon Oxygen Decarburization (AOD) technology combined with vacuum degassing systems to achieve precise carbon control below 0.030%, ensuring optimal weldability and preventing carbide precipitation during fabrication processes.

Comprehensive Quality Control System

Our state-of-the-art testing laboratory features advanced spectroscopic analysis, mechanical testing equipment, and non-destructive testing capabilities. Every batch undergoes rigorous chemical composition verification, mechanical property testing, and microstructure examination to guarantee consistent quality.

Manufacturing Advantage 2
Manufacturing Advantage 3

Global Supply Chain Excellence

MetalZenith offers extensive customization capabilities including precision cutting, surface finishing, and heat treatment services. Our global distribution network ensures reliable delivery worldwide, supported by comprehensive technical documentation and engineering support for specialized applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo