20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
QT 100 features a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The optimized alloy composition with chromium, molybdenum, and nickel additions provides enhanced hardenability and improved mechanical properties. The fine-grained microstructure ensures excellent strength-toughness balance critical for structural applications.
Heat Treatment Process
MetalZenith employs austenitizing at 880-920°C followed by water or oil quenching to achieve martensitic transformation. Subsequent tempering at 580-650°C optimizes the strength-toughness relationship while maintaining excellent weldability. Our controlled atmosphere furnaces ensure uniform heating and precise temperature control throughout the process.
Manufacturing Process Excellence
Our advanced manufacturing process includes electric arc furnace melting with secondary refining, continuous casting, and controlled rolling. MetalZenith's integrated production line ensures consistent chemical composition and mechanical properties while minimizing inclusions and segregation for superior structural performance.
Specialized Quality Testing
QT 100 undergoes comprehensive testing including weldability assessment per AWS D1.1, formability evaluation through bend testing, fatigue strength analysis using rotating beam testing, and atmospheric corrosion resistance evaluation. Our quality control program ensures compliance with structural engineering requirements and long-term durability.
Structural Application Engineering
For building construction, QT 100 provides exceptional load-bearing capacity with reduced weight. In bridge engineering, its high fatigue resistance ensures long service life under cyclic loading. For machinery manufacturing, the steel offers superior wear resistance and dimensional stability. Vehicle applications benefit from enhanced crash performance and structural integrity, while general engineering applications leverage its versatile processing characteristics and reliable performance.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.15 - 0.22 |
| Manganese (Mn) | 1.20 - 1.60 |
| Silicon (Si) | 0.20 - 0.60 |
| Phosphorus (P) | ≤ 0.020 |
| Sulfur (S) | ≤ 0.015 |
| Chromium (Cr) | 0.30 - 0.80 |
| Molybdenum (Mo) | 0.15 - 0.30 |
| Nickel (Ni) | 0.30 - 0.70 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Yield Strength (MPa) | ≥ 900 |
| Tensile Strength (MPa) | 1000 - 1200 |
| Elongation (%) | ≥ 12 |
| Impact Energy at -20°C (J) | ≥ 35 |
| Hardness (HB) | 300 - 380 |
| Fatigue Strength (MPa) | ≥ 450 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density (g/cm3) | 7.85 |
| Melting Point (°C) | 1480 - 1520 |
| Thermal Conductivity (W/m·K) | 42.5 |
| Thermal Expansion (×10??/K) | 11.8 |
| Elastic Modulus (GPa) | 210 |
| Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Bars, Beams, Channels, Angles |
| Thickness Range | 8 - 150mm |
| Width Range | 1200 - 3500mm |
| Length Range | 6000 - 15000mm |
| Standards Compliance | ASTM A514, EN 10025-6, JIS G3106 |
| Heat Treatment Condition | Quenched and Tempered (QT) |
| Surface Finish | Hot Rolled, Shot Blasted, Pickled |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing QT 100 Steel
Advanced Quenching and Tempering Process
MetalZenith utilizes precision-controlled quenching and tempering with real-time temperature monitoring and optimized cooling curves to achieve uniform microstructure. Our advanced heat treatment process ensures consistent mechanical properties and enhanced toughness throughout the material thickness, critical for structural applications.
Comprehensive Structural Performance Testing
Our QT 100 steel undergoes extensive testing including weldability assessment, formability evaluation, fatigue strength analysis, and atmospheric corrosion resistance testing. MetalZenith's quality assurance program ensures optimal performance in demanding structural environments with complete traceability and certification.
Custom Processing and Engineering Support
MetalZenith provides comprehensive custom processing services including precision cutting, forming, and machining to exact specifications. Our technical team offers engineering support for structural design optimization, welding procedures, and application-specific heat treatment modifications to meet unique project requirements.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications