20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
MS 1200 features a tempered martensitic microstructure optimized for ultra-high strength applications. The carefully balanced alloy composition promotes fine carbide precipitation during tempering, resulting in exceptional strength while maintaining adequate toughness. The low carbon content combined with strategic alloying minimizes weld cracking susceptibility while preserving hardenability.
Heat Treatment Process
MetalZenith's proprietary heat treatment involves austenitizing at 900-950°C followed by rapid quenching to achieve full martensitic transformation. Subsequent tempering at 580-620°C optimizes the strength-toughness balance. Our computer-controlled furnaces ensure uniform heating and precise temperature control throughout the process, with continuous monitoring of cooling rates and transformation kinetics.
Manufacturing Process Excellence
Production begins with vacuum induction melting of premium raw materials, followed by electroslag remelting for enhanced cleanliness. Hot rolling is performed using controlled thermomechanical processing to refine grain structure. MetalZenith's advanced rolling mills maintain precise temperature control and deformation schedules to optimize mechanical properties and dimensional accuracy.
Quality Standards & Testing
Every production lot undergoes comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical property verification per ASTM standards, and ultrasonic testing for internal soundness. Charpy impact testing at various temperatures ensures adequate toughness, while fatigue testing validates long-term performance. MetalZenith maintains full traceability documentation and provides certified test reports with each shipment, ensuring compliance with aerospace AS9100D and automotive TS16949 quality management systems.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.10-0.15 |
| Manganese (Mn) | 1.40-1.80 |
| Silicon (Si) | 0.15-0.35 |
| Phosphorus (P) | ≤ 0.015 |
| Sulfur (S) | ≤ 0.005 |
| Chromium (Cr) | 0.30-0.60 |
| Nickel (Ni) | 1.80-2.20 |
| Molybdenum (Mo) | 0.15-0.30 |
| Boron (B) | 0.002-0.005 |
| Titanium (Ti) | 0.020-0.050 |
| Aluminum (Al) | 0.015-0.050 |
| Nitrogen (N) | ≤ 0.008 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength (Rm) | 1200-1400 MPa |
| Yield Strength (Rp0.2) | ≥ 1050 MPa |
| Elongation (A5) | ≥ 12% |
| Reduction of Area (Z) | ≥ 45% |
| Hardness (HRC) | 38-42 |
| Impact Energy (KV at -40°C) | ≥ 27 J |
| Fatigue Limit (107 cycles) | 420 MPa |
| Young's Modulus (E) | 210 GPa |
| Poisson's Ratio (ν) | 0.30 |
| Fracture Toughness (KIC) | 85 MPa·m1/2 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.85 g/cm³ |
| Melting Point | 1480-1520°C |
| Thermal Conductivity (20°C) | 42 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 11.5×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.18 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 760°C |
| Thermal Diffusivity | 11.6 mm²/s |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Plates, Sheets, Bars, Forgings, Tubes |
| Plate Thickness | 3-150 mm |
| Sheet Thickness | 0.5-6.0 mm |
| Bar Diameter | 10-300 mm |
| Maximum Dimensions | 3000×1500 mm (plates) |
| Surface Finish | Hot Rolled, Cold Rolled, Pickled, Ground |
| Dimensional Tolerance | ±0.1 mm (thickness), ±2 mm (width/length) |
| Standards Compliance | ASTM A514, EN 10025-6, JIS G3106 |
| Heat Treatment Condition | Quenched and Tempered (Q&T) |
| Edge Condition | Mill Edge, Slit Edge, Sheared Edge |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing MS 1200
Advanced Vacuum Metallurgy Technology
MetalZenith employs cutting-edge vacuum induction melting (VIM) and electroslag remelting (ESR) processes to achieve exceptional cleanliness and homogeneity in MS 1200 production. Our controlled atmosphere processing eliminates inclusions and ensures consistent mechanical properties throughout the material cross-section.
Precision Heat Treatment & Quality Control
Our state-of-the-art heat treatment facilities feature computer-controlled quenching and tempering systems with real-time monitoring. Every batch undergoes comprehensive testing including tensile, impact, and fatigue testing, with statistical process control ensuring consistent quality and performance.
Custom Engineering & Global Supply Chain
MetalZenith offers complete customization capabilities including bespoke chemical compositions, specialized heat treatments, and precision machining services. Our global distribution network and strategic inventory management ensure reliable supply with lead times optimized for customer production schedules.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications