Skip to product information
1 of 1

Low Carbon Steel (Low Temperature Grade)

Low Carbon Steel (Low Temperature Grade)

Low Carbon Steel - Low Temperature Grade

Low Carbon Steel Low Temperature Grade is a specialized structural steel engineered for exceptional performance in cryogenic and extreme cold environments. This advanced steel grade features enhanced low-temperature toughness, superior impact resistance at sub-zero temperatures, and excellent ductility retention, making it ideal for critical applications in LNG facilities, aerospace systems, and polar operations.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art controlled cooling and specialized heat treatment processes to produce low-temperature grade steel with optimized microstructure and exceptional cryogenic performance. Our advanced thermomechanical processing ensures superior grain refinement and enhanced impact toughness down to -196°C, critical for cryogenic applications.

Key Applications

  • LNG storage tanks and cryogenic vessels
  • Low-temperature pipeline systems and transfer lines
  • Polar and arctic equipment structures
  • Aerospace and rocket fuel systems
  • Superconducting equipment housings and supports

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control throughout production, including specialized cryogenic impact testing at -196°C, DBTT temperature determination, crack propagation rate testing, and complete low-temperature fatigue analysis. Our low-temperature grade steel meets ASTM A333, ASME Section VIII, and other critical cryogenic application standards.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics for Cryogenic Service

Low Carbon Steel Low Temperature Grade features a fine-grained ferritic-pearlitic microstructure optimized for cryogenic applications. The controlled addition of nickel enhances low-temperature toughness, while aluminum deoxidation ensures fine grain structure. The steel maintains excellent ductility and impact resistance at temperatures down to -196°C through careful control of carbon content and grain refinement.

Specialized Heat Treatment Process

MetalZenith employs controlled normalization at 900-920°C followed by controlled cooling to achieve optimal microstructure for cryogenic service. Fine grain practice is utilized to ensure ASTM grain size 6 or finer, critical for low-temperature impact properties. Post-heat treatment stress relief at 580-620°C may be applied for thick sections to optimize residual stress distribution.

Advanced Manufacturing Process

Our manufacturing process incorporates controlled rolling with finish rolling temperatures above 850°C to ensure proper austenite conditioning. MetalZenith utilizes advanced ladle metallurgy for precise chemistry control and inclusion modification, followed by continuous casting with electromagnetic stirring for homogeneous microstructure. All processes are optimized to achieve superior low-temperature performance.

Comprehensive Cryogenic Testing Protocol

MetalZenith conducts extensive low-temperature testing including Charpy V-notch impact testing at -196°C, ductile-to-brittle transition temperature (DBTT) determination, crack tip opening displacement (CTOD) testing, and low-temperature fatigue crack growth rate analysis. Drop weight tear testing (DWTT) and fracture appearance transition temperature (FATT) evaluations ensure reliable performance in cryogenic service conditions.

Application-Specific Technical Considerations

For LNG storage applications, the steel provides exceptional thermal shock resistance and maintains structural integrity during rapid temperature cycling. In low-temperature pipeline systems, superior fracture toughness prevents brittle failure under operational stresses. For polar equipment, enhanced impact resistance ensures reliability in extreme arctic conditions. Aerospace applications benefit from the steel's lightweight strength and cryogenic fuel compatibility, while superconducting equipment applications utilize the material's stable magnetic properties and thermal conductivity at cryogenic temperatures.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.30
Manganese (Mn)0.40 - 1.06
Silicon (Si)0.10 - 0.35
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.025
Nickel (Ni)0.40 - 1.00
Aluminum (Al)≥ 0.020
Copper (Cu)≤ 0.40

⚙️ Mechanical Properties

PropertyValue
Low Temperature Yield Strength at -196°C (MPa)≥ 240
Tensile Strength (MPa)415 - 550
Low Temperature Impact Energy at -196°C (J)≥ 27
DBTT Temperature (°C)≤ -100
Fatigue Strength at -196°C (MPa)≥ 180
Fracture Toughness KIC (MPa√m)≥ 100
Elongation (%)≥ 22

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.87
Melting Point (°C)1510 - 1540
Low Temperature Thermal Conductivity at -196°C (W/m·K)52.8
Thermal Expansion Coefficient (×10??/K)11.8
Low Temperature Elastic Modulus at -196°C (GPa)220
Specific Heat Capacity (J/kg·K)460

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Pipes, Tubes, Forgings, Bars
Thickness Range3 - 150mm
Width Range1000 - 3500mm
Length Range6000 - 15000mm
Standards ComplianceASTM A333, ASME SA-333, EN 10028-4
Heat Treatment ConditionNormalized, Fine Grain Practice
Service Temperature Range-196°C to +400°C

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Low Carbon Steel (Low Temperature Grade)

Manufacturing Advantage 1

Advanced Cryogenic Processing Technology

MetalZenith employs specialized controlled cooling and normalization processes with precise temperature monitoring to achieve optimal fine-grain microstructure. Our advanced cryogenic processing ensures exceptional impact toughness and ductility retention at temperatures down to -196°C, critical for LNG and aerospace applications.

Comprehensive Low-Temperature Testing

Our rigorous quality control includes specialized cryogenic testing protocols: Charpy V-notch impact testing at -196°C, ductile-to-brittle transition temperature (DBTT) determination, crack propagation rate analysis, and low-temperature fatigue performance evaluation. These tests ensure reliable performance in extreme cold environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Cryogenic Solutions

MetalZenith provides tailored solutions for cryogenic applications with custom heat treatment schedules, specialized forming processes, and comprehensive technical support. Our engineering team works closely with clients to optimize material properties for specific low-temperature service conditions.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo