20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Metallurgical Characteristics
HY-100 exhibits a tempered martensitic microstructure achieved through controlled quenching and tempering processes. The low-alloy composition with nickel, chromium, and molybdenum additions provides exceptional hardenability and toughness. The fine-grained structure ensures uniform strength distribution and excellent impact resistance, making it ideal for high-stress structural applications requiring superior mechanical properties.
Heat Treatment Process
MetalZenith employs precision austenitizing at 870-900°C followed by controlled water quenching to achieve full martensitic transformation. Subsequent tempering at 580-620°C optimizes the strength-toughness balance while maintaining excellent structural integrity. Our advanced heat treatment facilities ensure uniform temperature distribution and controlled cooling rates for consistent mechanical properties.
Manufacturing Process Excellence
Our manufacturing process begins with electric arc furnace melting followed by ladle refining and vacuum degassing to achieve superior cleanliness. Continuous casting and controlled rolling optimize the microstructure before heat treatment. Advanced process control systems monitor temperature, time, and cooling rates throughout production to ensure consistent quality and performance.
Specialized Quality Testing
MetalZenith conducts comprehensive testing specific to structural applications including: welding performance evaluation using standard procedures, forming capability assessment through bend testing, fatigue strength determination under cyclic loading conditions, and atmospheric corrosion resistance testing in simulated environmental conditions. These specialized tests ensure optimal performance in demanding structural environments.
Structural Application Engineering
For building construction, HY-100's high strength-to-weight ratio enables lighter structural designs while maintaining safety factors. In bridge engineering, excellent fatigue resistance ensures long-term durability under dynamic loading. For machinery manufacturing, superior toughness prevents brittle failure in high-stress components. Vehicle manufacturing benefits from weight reduction without compromising structural integrity. General engineering applications leverage the combination of high strength, good weldability, and reliable performance across temperature ranges.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | 0.12 - 0.18 |
| Manganese (Mn) | 0.95 - 1.30 |
| Silicon (Si) | 0.20 - 0.35 |
| Phosphorus (P) | ≤ 0.015 |
| Sulfur (S) | ≤ 0.015 |
| Chromium (Cr) | 0.40 - 0.65 |
| Nickel (Ni) | 2.00 - 3.50 |
| Molybdenum (Mo) | 0.15 - 0.25 |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Yield Strength (MPa) | ≥ 690 |
| Tensile Strength (MPa) | 760 - 895 |
| Elongation (%) | ≥ 16 |
| Impact Energy at -40°C (J) | ≥ 20 |
| Hardness (HB) | 235 - 285 |
| Fatigue Strength (MPa) | 345 - 380 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density (g/cm3) | 7.85 |
| Melting Point (°C) | 1480 - 1520 |
| Thermal Conductivity (W/m·K) | 44.5 |
| Thermal Expansion (×10??/K) | 12.3 |
| Elastic Modulus (GPa) | 200 |
| Poisson's Ratio | 0.27 - 0.30 |
📏 Product Specifications
| Specification | Details |
|---|---|
| Available Forms | Plates, Sheets, Bars, Structural Shapes, Forgings |
| Thickness Range | 6 - 150mm |
| Width Range | 1200 - 4500mm |
| Length Range | 6000 - 20000mm |
| Standards Compliance | ASTM A514, ASTM A517, MIL-S-16216 |
| Heat Treatment Condition | Quenched and Tempered |
| Surface Finish | Hot Rolled, Pickled, Shot Blasted |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing HY-100 Steel
Precision Quench & Temper Processing
MetalZenith utilizes advanced quenching and tempering technology with precise temperature control and uniform cooling rates to achieve optimal microstructural refinement. Our controlled heat treatment process ensures consistent high-strength properties and superior toughness throughout the material thickness, critical for structural applications.
Comprehensive Structural Testing
Our quality assurance program includes specialized testing for structural applications: advanced welding performance evaluation, forming capability assessment, fatigue strength testing under cyclic loading, and atmospheric corrosion resistance testing. These comprehensive evaluations ensure optimal performance in demanding structural environments.
Custom Structural Solutions
MetalZenith provides tailored processing services including precision cutting, forming, and heat treatment modifications to meet specific structural requirements. Our technical team offers comprehensive engineering support for complex projects, ensuring optimal material selection and processing for each unique application.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications