20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
Hot Rolled Steel Sheet is manufactured through hot rolling process at temperatures above the recrystallization temperature, typically around 1000°C. This carbon steel sheet offers excellent formability, weldability, and cost-effectiveness for a wide range of structural and general engineering applications.
Key Features:
- Excellent formability and ductility
- Good weldability with standard welding processes
- Cost-effective solution for structural applications
- Wide range of thickness and size availability
- Suitable for further processing and fabrication
Manufacturing Process: Hot rolled through continuous rolling mills at high temperature, followed by controlled cooling to achieve desired mechanical properties and microstructure.
Applications: Construction and building structures, automotive components, shipbuilding, machinery manufacturing, general fabrication, storage tanks, pressure vessels, and industrial equipment manufacturing.
🧪 Chemical Composition
| Element | Min % | Max % | Typical % | ASTM A36 Requirement |
|---|---|---|---|---|
| Carbon (C) | - | 0.26 | 0.18 | ≤ 0.26 |
| Manganese (Mn) | 0.80 | 1.20 | 0.95 | 0.80-1.20 |
| Silicon (Si) | 0.15 | 0.40 | 0.25 | 0.15-0.40 |
| Phosphorus (P) | - | 0.040 | 0.025 | ≤ 0.040 |
| Sulfur (S) | - | 0.050 | 0.030 | ≤ 0.050 |
| Copper (Cu) | - | 0.20 | 0.12 | ≤ 0.20 |
| Nickel (Ni) | - | 0.20 | 0.10 | ≤ 0.20 |
| Chromium (Cr) | - | 0.20 | 0.08 | ≤ 0.20 |
| Iron (Fe) | Balance | Balance | 98.2 | Balance |
⚙️ Mechanical Properties
| Property | ASTM Requirement | Typical Value | Test Method | Temperature |
|---|---|---|---|---|
| Tensile Strength | 400-550 MPa | 480 MPa | ASTM A370 | Room Temp |
| Yield Strength | 250 MPa min | 280 MPa | ASTM A370 | Room Temp |
| Elongation | 20% min | 26% | ASTM A370 | Room Temp |
| Hardness (Brinell) | - | 140 HB | ASTM E10 | Room Temp |
| Hardness (Rockwell B) | - | 78 HRB | ASTM E18 | Room Temp |
| Modulus of Elasticity | - | 200 GPa | ASTM E111 | Room Temp |
| Impact Energy (Charpy V) | - | 80+ J | ASTM E23 | Room Temp |
🔬 Physical Properties
| Property | Value | Unit | Temperature | Test Standard |
|---|---|---|---|---|
| Density | 7.85 | g/cm3 | 20°C | ASTM B311 |
| Melting Point | 1510-1540 | °C | - | DSC Analysis |
| Thermal Conductivity | 50.2 | W/m·K | 100°C | ASTM E1461 |
| Specific Heat | 460 | J/kg·K | 0-100°C | ASTM C351 |
| Linear Expansion | 12.0 | μm/m·K | 0-100°C | ASTM E228 |
| Electrical Resistivity | 170 | n|°¤m | 20°C | ASTM B193 |
| Magnetic Permeability | High | μ/μ₀ | Room Temp | ASTM A342 |
| Curie Temperature | 770 | °C | - | Ferromagnetic |
📏 Product Specifications
| Specification | Available Range | Standard Size | Custom Available | Tolerance |
|---|---|---|---|---|
| Thickness | 1.5mm - 100mm | Various | Yes | ±0.1mm |
| Width | 600mm - 2500mm | 1250mm, 1500mm | Yes | ±5mm |
| Length | 2m - 12m | 6m, 12m | Yes | +50mm/-0mm |
| Surface Finish | Hot Rolled, Pickled | Hot Rolled | Yes | Ra ≤ 6.3μm |
| Edge Condition | Mill Edge, Cut Edge | Mill Edge | Both | ASTM standard |
| Flatness | Standard, Precision | Standard | Yes | ≤ 10mm/m |
| Standards Compliance | ASTM A36, A572, A588 | A36 | Multiple | Full compliance |
| Coil Weight | 5-30 tons | 15-25 tons | Yes | ±5% |
| Test Certificate | Mill TC, EN 10204 3.1 | Mill TC | Yes | Standard |
| Packaging | Coils, Cut Sheets, Bundles | Coils | Custom | Export standard |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing Hot rolled steel sheet
High Temperature Processing
Manufacturing at temperatures exceeding 1,700°F enables optimal material flow and malleability, resulting in consistent thickness throughout the sheet and superior structural integrity compared to cold-rolled alternatives.
Efficient Rolling Process
Continuous rolling operation allows for high-volume production with minimal production steps, reducing manufacturing time and costs while maintaining precise dimensional control during the forming process.
Simplified Surface Finishing
The hot rolling process naturally creates a workable mill scale surface finish that requires minimal post-processing, making it ideal for applications where exact surface smoothness is not critical.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications