H21 Tool Steel

H21 Premium Hot Work Tool Steel

H21 is a premium tungsten-chromium hot work tool steel specifically engineered for high-temperature applications requiring exceptional thermal shock resistance and dimensional stability. This advanced tool steel grade delivers superior performance in demanding environments where conventional tool steels fail, making it ideal for hot forming operations and high-stress tooling applications.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum melting and controlled forging processes to produce H21 tool steel with exceptional cleanliness and microstructural uniformity. Our advanced heat treatment protocols ensure optimal carbide distribution and enhanced thermal fatigue resistance, critical for hot work tooling applications requiring extended service life.

Key Applications

  • Hot forging dies and extrusion tooling
  • Die casting dies for aluminum and magnesium
  • Hot shearing blades and punches
  • Precision injection molding tools
  • Automotive stamping dies and forming tools

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control throughout production, including ultrasonic testing, thermal fatigue testing, and complete microstructural analysis. Our H21 tool steel meets ASTM A681 and international tool steel standards, ensuring reliability in critical tooling applications with rigorous dimensional tolerance requirements.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

H21 tool steel exhibits a complex microstructure consisting of tempered martensite matrix with uniformly distributed tungsten and chromium carbides. The high tungsten content provides exceptional hot hardness and thermal shock resistance, while chromium carbides enhance wear resistance and dimensional stability at elevated temperatures. The fine carbide distribution achieved through MetalZenith's controlled processing ensures optimal tool performance.

Heat Treatment Process

MetalZenith employs controlled austenitizing at 1150-1180°C followed by oil or air quenching and multiple tempering cycles at 550-650°C. This precise heat treatment protocol optimizes the balance between hardness, toughness, and thermal fatigue resistance. Stress relieving at 650-700°C is recommended for complex tool geometries to minimize distortion.

Advanced Manufacturing Process

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to achieve superior cleanliness and homogeneity. Controlled forging operations with precise temperature monitoring ensure optimal grain flow and carbide distribution. Our advanced quality control includes ultrasonic testing and microstructural analysis to guarantee tool steel integrity.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including Rockwell hardness distribution mapping, residual austenite content analysis using X-ray diffraction, carbide distribution evaluation through metallographic analysis, and thermal fatigue strength testing. These specialized tests ensure consistent performance in demanding hot work applications and extended tool life.

Application-Specific Technical Considerations

For cutting tools, H21 provides excellent hot hardness retention and thermal shock resistance. In die and mold manufacturing, the superior dimensional stability and thermal fatigue resistance ensure extended service life. For precision machinery components, the uniform microstructure and controlled thermal expansion provide reliable performance. In automotive applications, H21's combination of wear resistance and toughness makes it ideal for hot forming dies and stamping tools operating at elevated temperatures.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.28 - 0.35
Chromium (Cr)3.00 - 3.75
Tungsten (W)9.00 - 9.75
Vanadium (V)0.40 - 0.60
Silicon (Si)0.15 - 0.40
Manganese (Mn)0.15 - 0.40
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)48 - 52
Compressive Strength (MPa)2800 - 3200
Impact Toughness (J)15 - 25
Wear Resistance Index8.5 - 9.2
Hardenability (mm)75 - 100
Thermal Fatigue ResistanceExcellent

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.15
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)24.5
Thermal Expansion (×10??/K)11.8
Elastic Modulus (GPa)215
Specific Heat (J/kg·K)460

📏 Product Specifications

SpecificationDetails
Available FormsBars, Blocks, Plates, Forgings, Custom Shapes
Diameter Range10 - 500mm
Thickness Range5 - 300mm
Length Range100 - 6000mm
Standards ComplianceASTM A681, DIN 1.2581, JIS SKD61
Heat Treatment ConditionAnnealed, Hardened & Tempered
Surface FinishHot Rolled, Machined, Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing H21 Tool Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes advanced vacuum induction melting followed by electroslag remelting (ESR) to achieve exceptional cleanliness and homogeneity in H21 tool steel. Our controlled forging and heat treatment processes ensure optimal carbide distribution and grain structure for maximum thermal fatigue resistance and tool life.

Comprehensive Tool Steel Testing

MetalZenith conducts specialized testing protocols including Rockwell hardness mapping across tool sections, residual austenite content analysis, carbide distribution evaluation, and thermal fatigue strength testing. Our quality assurance ensures consistent performance in demanding hot work applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment Services

MetalZenith offers specialized heat treatment services tailored to specific tooling applications, including custom tempering cycles, stress relieving, and surface hardening treatments. Our metallurgical expertise ensures optimal tool performance with comprehensive technical support throughout the tool manufacturing process.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo