Get A Quote
Alloy | ASTM | Characteristics |
---|---|---|
ASTM A588 | A606/A588a Weathering |
Architectural facades and building cladding Sculptures and outdoor art installations Bridges and large-scale infrastructure projects |
CHEMICAL COMPOSITION
- The chemical composition of this category includes Carbon (C) ranging from 0.1 to 0.22%, Chromium (Cr) from 0.4 to 0.65%, Manganese (Mn) from 0.9 to 1.25%, Copper (Cu) from 0.25 to 0.4%, Iron (Fe) from 97 to 98.5%, Phosphorus (P) up to a maximum of 0.04%, Silicon (Si) from 0.15 to 0.3%, Sulfur (S) up to a maximum of 0.05%, and Vanadium (V) from 0.02 to 0.1%.
MECHANICAL INFORMATION
- This material features a chemical composition primarily composed of 97-98.5% Fe, balanced by minor elements including 0.1-0.22% Carbon (C), 0.4-0.65% Chromium (Cr), 0.9-1.25% Manganese (Mn), 0.25-0.4% Copper (Cu), 0.15-0.3% Silicon (Si), with maximum levels of 0.04% Phosphorus (P) and 0.05% Sulfur (S). Vanadium (V) is present in trace amounts of 0.02-0.1%. The mechanical properties indicate a density of 0.28 lb/in³ (7.75 g/cc), an ultimate tensile strength of 70,000 psi (483 MPa), and a yield tensile strength of 50,000 psi (345 MPa). This material is produced by a hot rolling method and is available in various sizes, including thicknesses of 1/4", 3/8", and 1/2", with respective widths and lengths of 48" or 60" and 120", weighing from 10.210 to 20.420 lbs/ft. Please contact our Customer Service Department for material test reports and further information.
AVAILABLE SIZES
- Available sizes for this category include a 1/4" thickness with options for a width of 48.00" or 60.00" and a length of 120.00", each weighing 10.210 lbs/ft. Additionally, a 3/8" thickness is available with a width of 48.00" and a length of 120.00", weighing 15.315 lbs/ft. Finally, a 1/2" thickness is available with a width of 48.00" and a length of 120.00", weighing 20.420 lbs/ft.