Skip to product information
1 of 1

AISI 321H

AISI 321H

AISI 321H High Carbon Stabilized Stainless Steel

AISI 321H is a high carbon variant of the titanium-stabilized austenitic stainless steel grade 321, specifically designed for elevated temperature applications requiring superior creep resistance and thermal stability. This grade offers enhanced mechanical properties at high temperatures compared to standard 321 grade.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith leverages state-of-the-art vacuum induction melting (VIM) and electroslag remelting (ESR) technologies to produce AISI 321H with exceptional purity and homogeneity. Our advanced titanium stabilization process ensures optimal carbide precipitation control, maximizing the steel's high-temperature performance characteristics.

Key Applications

  • High-temperature furnace components and heat exchangers
  • Petrochemical processing equipment operating above 550°C
  • Power generation turbine components and steam piping
  • Aerospace engine parts requiring creep resistance
  • Industrial heating elements and thermal processing equipment

Quality Assurance & Certifications

MetalZenith maintains ISO 9001:2015, AS9100D, and NADCAP certifications, ensuring the highest quality standards. Our comprehensive testing protocols include chemical analysis, mechanical testing, non-destructive examination, and microstructural evaluation to guarantee material integrity and performance reliability.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

AISI 321H is an austenitic stainless steel with a face-centered cubic crystal structure stabilized by titanium additions. The higher carbon content (0.04-0.10%) compared to standard 321 grade enhances creep strength and high-temperature mechanical properties. Titanium forms stable carbides (TiC) that prevent chromium carbide precipitation, maintaining corrosion resistance at elevated temperatures.

Heat Treatment Process

Solution annealing is performed at 1040-1120°C followed by rapid cooling to achieve optimal microstructure. A stabilization treatment at 870-900°C for 2-4 hours may be applied to promote titanium carbide formation and enhance high-temperature stability. MetalZenith's controlled atmosphere furnaces ensure precise temperature control and prevent surface oxidation during heat treatment.

Manufacturing Process

MetalZenith employs electric arc furnace (EAF) melting followed by argon oxygen decarburization (AOD) for precise composition control. Vacuum induction melting (VIM) and electroslag remelting (ESR) processes are utilized for critical applications requiring ultra-high purity. Hot working is performed between 1150-950°C, while cold working can achieve significant strength increases through work hardening.

Quality Standards & Testing

All AISI 321H products undergo comprehensive testing including chemical analysis by optical emission spectroscopy, mechanical testing per ASTM standards, ultrasonic testing for internal soundness, and microstructural examination. Creep testing at elevated temperatures validates long-term performance characteristics. MetalZenith maintains full traceability from raw materials through final inspection, ensuring compliance with aerospace, nuclear, and petrochemical industry requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.04 - 0.10
Manganese (Mn)≤ 2.00
Silicon (Si)≤ 0.75
Phosphorus (P)≤ 0.045
Sulfur (S)≤ 0.030
Chromium (Cr)17.0 - 20.0
Nickel (Ni)9.0 - 13.0
Titanium (Ti)4×(C+N) min, 0.70 max
Nitrogen (N)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Tensile Strength (Room Temperature)≥ 515 MPa
Yield Strength (0.2% Offset)≥ 205 MPa
Elongation (50mm gauge)≥ 40%
Reduction of Area≥ 50%
Hardness (Brinell)≤ 217 HB
Impact Energy (Charpy V-notch, Room Temp)≥ 68 J
Young's Modulus200 GPa
Creep Strength (100,000h at 650°C)35 MPa
Fatigue Limit (107 cycles)240 MPa

🔬 Physical Properties

PropertyValue
Density7.90 g/cm³
Melting Point1400-1450°C
Thermal Conductivity (20°C)16.3 W/m·K
Thermal Conductivity (100°C)17.8 W/m·K
Thermal Expansion (20-100°C)17.2×10-6/K
Thermal Expansion (20-500°C)18.4×10-6/K
Specific Heat Capacity500 J/kg·K
Electrical Resistivity (20°C)0.72 µΩ·m
Magnetic Permeability1.02 µr (Non-magnetic)
Curie TemperatureNon-magnetic

📏 Product Specifications

SpecificationAvailable Options
Product FormsBars, Rods, Plates, Sheets, Tubes, Pipes, Forgings, Castings
Bar Diameter Range6mm - 300mm
Plate Thickness Range3mm - 150mm
Sheet Thickness Range0.5mm - 6mm
Tube Outer Diameter6mm - 219mm
Standards ComplianceASTM A240, A479, A312, EN 10088-2, JIS G4304, GB/T 1220
Surface FinishesHot Rolled, Cold Rolled, 2B, BA, No.4, HL, Mirror
Dimensional Tolerance±0.1mm to ±0.5mm (depending on form and size)
Length OptionsStandard lengths or cut to customer specifications

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing AISI 321H

Manufacturing Advantage 1

Advanced Titanium Stabilization Technology

MetalZenith employs proprietary controlled atmosphere melting and precise titanium addition techniques to achieve optimal Ti/C ratios, ensuring superior carbide precipitation control and enhanced high-temperature stability in AISI 321H production.

Comprehensive High-Temperature Testing

Our specialized testing laboratory features advanced creep testing equipment and high-temperature mechanical testing capabilities up to 1000°C, ensuring every batch of AISI 321H meets stringent performance requirements for critical applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment & Processing

MetalZenith offers tailored solution annealing, stabilization treatments, and custom forming services to optimize AISI 321H properties for specific applications, backed by our global supply chain and technical support network.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo