20 Years Experience | 1000+ Brand Partners | Full Customization
We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.
Technical Specifications
Product Overview
304 Stainless Steel Plate is manufactured from premium grade 304 austenitic stainless steel, providing excellent corrosion resistance, formability, and weldability. This versatile plate material is ideal for a wide range of industrial, architectural, and food processing applications.
Key Features:
- Excellent corrosion resistance in most environments
- Superior formability and deep drawing capabilities
- Non-magnetic in annealed condition
- FDA approved for food contact applications
- Easy to clean and maintain hygienic surfaces
- Good weldability with all standard welding methods
Manufacturing Process: Hot rolled and cold rolled using advanced mill technology, followed by annealing and pickling to achieve optimal mechanical properties and surface finish.
Applications: Kitchen equipment, food processing machinery, chemical processing equipment, pharmaceutical equipment, architectural panels, decorative applications, pressure vessels, and general fabrication projects requiring corrosion resistance.
🧪 Chemical Composition
| Element | Min % | Max % | Typical % | ASTM A240 Requirement |
|---|---|---|---|---|
| Carbon (C) | - | 0.080 | 0.045 | ≤ 0.08 |
| Chromium (Cr) | 18.0 | 20.0 | 18.5 | 18.0-20.0 |
| Nickel (Ni) | 8.0 | 12.0 | 9.2 | 8.0-12.0 |
| Manganese (Mn) | - | 2.00 | 1.45 | ≤ 2.00 |
| Silicon (Si) | - | 0.75 | 0.42 | ≤ 0.75 |
| Phosphorus (P) | - | 0.045 | 0.028 | ≤ 0.045 |
| Sulfur (S) | - | 0.030 | 0.015 | ≤ 0.030 |
| Nitrogen (N) | - | 0.10 | 0.06 | ≤ 0.10 |
| Iron (Fe) | Balance | Balance | 70.1 | Balance |
⚙️ Mechanical Properties
| Property | ASTM Requirement | Typical Value | Test Method | Temperature |
|---|---|---|---|---|
| Tensile Strength | 515 MPa min | 580 MPa | ASTM A370 | Room Temp |
| Yield Strength (0.2%) | 205 MPa min | 240 MPa | ASTM A370 | Room Temp |
| Elongation | 40% min | 50% | ASTM A370 | Room Temp |
| Hardness (Brinell) | 201 HB max | 170 HB | ASTM E10 | Room Temp |
| Hardness (Rockwell B) | 92 HRB max | 85 HRB | ASTM E18 | Room Temp |
| Modulus of Elasticity | - | 200 GPa | ASTM E111 | Room Temp |
| Impact Energy (Charpy V) | - | 300+ J | ASTM E23 | Room Temp |
🔬 Physical Properties
| Property | Value | Unit | Temperature | Test Standard |
|---|---|---|---|---|
| Density | 8.00 | g/cm3 | 20°C | ASTM B311 |
| Melting Point | 1400-1450 | °C | - | DSC Analysis |
| Thermal Conductivity | 16.2 | W/m·K | 100°C | ASTM E1461 |
| Specific Heat | 500 | J/kg·K | 0-100°C | ASTM C351 |
| Linear Expansion | 17.2 | μm/m·K | 0-100°C | ASTM E228 |
| Electrical Resistivity | 720 | n|°¤m | 20°C | ASTM B193 |
| Magnetic Permeability | 1.02 | μ/μ₀ | Room Temp | ASTM A342 |
| Curie Temperature | None | - | - | Non-magnetic |
📏 Product Specifications
| Specification | Available Range | Standard Size | Custom Available | Tolerance |
|---|---|---|---|---|
| Thickness | 0.3mm - 100mm | Various | Yes | ±0.1mm (≤3mm), ±3% (>3mm) |
| Width | 100mm - 2500mm | 1000mm, 1219mm, 1500mm | Yes | ±3mm |
| Length | 500mm - 6000mm | 2000mm, 2438mm, 3000mm | Yes | ±5mm |
| Surface Finish | 2B, BA, No.1, No.4, HL, Mirror | 2B | Yes | Ra ≤ 0.4μm (2B) |
| Edge Condition | Mill Edge, Slit Edge | Mill Edge | Both | ASTM standard |
| Flatness | ≤ 3mm/m | ≤ 2mm/m | Improved | ASTM A480 |
| Standards Compliance | ASTM A240, A480, JIS G4304 | A240 | Multiple | Full compliance |
| Condition | Annealed, Cold Rolled | Annealed | Both | ASTM A240 |
| Test Certificate | Mill TC, EN 10204 3.1 | Mill TC | Yes | Standard |
| Packaging | Wooden Crates, Steel Pallets | Wooden Crates | Custom | Export standard |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing 304 Stainless Steel Plate
Precision Rolling Technology
Advanced 4-roll cold rolling process ensures 2B surface finish with thickness tolerance ?¨¤0.1mm for consistent dimensional accuracy
Comprehensive Quality Control
100% chemical composition testing per batch, 99.9% intergranular corrosion test pass rate, strictly compliant with ASTM A240 standards
Superior Corrosion Resistance
316L-grade corrosion performance, salt spray test >1000 hours without rust, ideal for chemical, food, and medical applications