310 Stainless Steel is classified as an austenitic stainless steel, known for its high chromium and nickel content, which provides excellent oxidation resistance and high-temperature strength. The primary alloying elements in 310 stainless steel include approximately 24% chromium and 19% nickel, which contribute to its superior corrosion resistance and mechanical properties.

Comprehensive Overview

310 stainless steel is particularly valued for its ability to withstand extreme temperatures and corrosive environments, making it suitable for applications in various industries, including aerospace, chemical processing, and power generation. Its high chromium content enhances its resistance to oxidation and scaling at elevated temperatures, while the nickel content improves its ductility and toughness.

Advantages and Limitations

Advantages Limitations
Excellent high-temperature strength Higher cost compared to lower alloy grades
Superior oxidation resistance Limited weldability compared to some other stainless steels
Good resistance to sulfuric and phosphoric acids Susceptible to stress corrosion cracking in certain environments
High ductility and toughness Requires careful handling during fabrication to avoid work hardening

310 stainless steel holds a significant position in the market due to its unique properties, making it a preferred choice for high-temperature applications. Historically, it has been used in applications such as furnace components, heat exchangers, and gas turbine parts, showcasing its versatility and reliability.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S31000 USA Closest equivalent to AISI 310
AISI/SAE 310 USA Commonly used designation
ASTM A240 USA Standard specification for stainless steel plates
EN 1.4845 Europe Similar properties, minor compositional differences
JIS SUS310 Japan Equivalent grade with similar characteristics
GB 00Cr25Ni20 China Closest equivalent with slight variations

The differences between these equivalent grades can affect selection based on specific application requirements, such as temperature limits and corrosion resistance. For example, while 1.4845 offers similar properties, it may have slightly different mechanical characteristics that could influence performance in specific environments.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Cr (Chromium) 24.0 - 26.0
Ni (Nickel) 19.0 - 22.0
C (Carbon) ≤ 0.08
Mn (Manganese) ≤ 2.0
Si (Silicon) ≤ 1.0
P (Phosphorus) ≤ 0.045
S (Sulfur) ≤ 0.03

Chromium is crucial for enhancing corrosion resistance and oxidation resistance, while nickel contributes to the steel's toughness and ductility. The low carbon content minimizes the risk of carbide precipitation, which can lead to intergranular corrosion.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Annealed 515 - 750 MPa 75 - 109 ksi ASTM E8
Yield Strength (0.2% offset) Annealed 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed 40 - 50% 40 - 50% ASTM E8
Hardness (Rockwell B) Annealed 70 - 90 70 - 90 ASTM E18
Impact Strength (Charpy) -20°C 30 J 22 ft-lbf ASTM E23

The combination of high tensile and yield strength, along with good elongation, makes 310 stainless steel suitable for applications requiring structural integrity under mechanical loading. Its impact strength at low temperatures ensures reliability in cryogenic applications.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density Room Temperature 7.9 g/cm³ 0.285 lb/in³
Melting Point - 1400 - 1450 °C 2552 - 2642 °F
Thermal Conductivity Room Temperature 16.2 W/m·K 112 BTU·in/ft²·h·°F
Specific Heat Capacity Room Temperature 500 J/kg·K 0.12 BTU/lb·°F
Electrical Resistivity Room Temperature 0.72 µΩ·m 0.0000013 Ω·in

The density of 310 stainless steel contributes to its strength, while its thermal conductivity and specific heat capacity make it suitable for high-temperature applications where heat transfer is critical.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3-10 20-60 / 68-140 Fair Risk of pitting
Sulfuric Acid 10-30 20-60 / 68-140 Good Resistant at moderate temps
Phosphoric Acid 10-50 20-60 / 68-140 Excellent Very good resistance
Atmospheric Conditions - - Excellent Resistant to oxidation

310 stainless steel exhibits excellent resistance to a variety of corrosive environments, particularly in acidic conditions. Its performance against chlorides is moderate, and care should be taken to avoid pitting corrosion. Compared to grades like 304 and 316, 310 offers superior high-temperature oxidation resistance but may not perform as well in chloride-rich environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 1150 °C 2100 °F Suitable for high-temperature applications
Max Intermittent Service Temp 1050 °C 1922 °F Can withstand short-term exposure at higher temps
Scaling Temperature 900 °C 1652 °F Begins to oxidize significantly above this temperature

At elevated temperatures, 310 stainless steel maintains its strength and oxidation resistance, making it ideal for furnace applications and heat exchangers. However, prolonged exposure to temperatures above 1150 °C can lead to scaling and degradation of material properties.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER310 Argon Good for thin sections
MIG ER310 Argon + CO2 mix Suitable for thicker sections
SMAW E310 - Requires preheat for thick sections

310 stainless steel can be welded using various methods, but care must be taken to avoid cracking. Preheating and post-weld heat treatment are recommended to relieve stresses and improve weld integrity.

Machinability

Machining Parameter 310 Stainless Steel AISI 1212 Notes/Tips
Relative Machinability Index 30% 100% Requires slower speeds
Typical Cutting Speed 20-30 m/min 60-80 m/min Use carbide tools for best results

Machinability of 310 stainless steel is lower compared to free-machining steels like AISI 1212. Optimal conditions include using sharp tools and appropriate cutting fluids to minimize work hardening.

Formability

310 stainless steel exhibits good formability, allowing for cold and hot working processes. However, due to its high strength, it may require larger bend radii to avoid cracking during forming operations.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Solution Annealing 1000 - 1100 °C / 1832 - 2012 °F 1 hour Air or water Dissolve carbides, improve ductility
Stress Relief 600 - 800 °C / 1112 - 1472 °F 1 hour Air Reduce residual stresses

Heat treatment processes such as solution annealing enhance the ductility and toughness of 310 stainless steel by dissolving carbides and refining the microstructure.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Aerospace Exhaust systems High-temperature strength, oxidation resistance Required for extreme conditions
Chemical Processing Heat exchangers Corrosion resistance, thermal stability Effective in acidic environments
Power Generation Boiler tubes High strength, thermal conductivity Essential for heat transfer
Oil and Gas Flare stacks High-temperature performance Safety in extreme conditions

Other applications include:

  • Furnace components
  • Kiln linings
  • Industrial ovens
  • Heat treatment fixtures

The selection of 310 stainless steel in these applications is primarily due to its ability to withstand high temperatures and corrosive environments, ensuring longevity and reliability.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 310 Stainless Steel AISI 316 AISI 304 Brief Pro/Con or Trade-off Note
Key Mechanical Property High strength Moderate strength Lower strength 310 is better for high temps
Key Corrosion Aspect Excellent in acids Good in chlorides Fair in acids 310 excels in high-temperature acids
Weldability Moderate Good Excellent 310 requires more care in welding
Machinability Low Moderate High 310 is harder to machine
Formability Moderate Good Excellent 310 requires larger bend radii
Approx. Relative Cost High Moderate Low Cost reflects performance benefits
Typical Availability Moderate High Very High 304 is the most common stainless steel

When selecting 310 stainless steel, considerations include its cost-effectiveness, availability, and specific performance requirements in high-temperature and corrosive environments. While it may be more expensive than other grades, its unique properties often justify the investment in critical applications.

In summary, 310 stainless steel is a versatile and robust material, ideal for high-temperature and corrosive applications. Its unique properties make it a preferred choice in various industries, ensuring safety and reliability in demanding environments.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S31000, ASTM A240, EN 1.4845, JIS SUS310, GB 00Cr25Ni20). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

6 comments

Excelente artículo sobre las propiedades térmicas del acero 310, me ha sido muy útil para comparar la resistencia a la oxidación en hornos industriales. Estoy evaluando su uso para un proyecto de infraestructura térmica que planeamos implementar en España, pero como estamos coordinando la parte operativa, me surgió una duda legal: ¿saben si para la adquisición de materiales a gran escala como proveedores locales es obligatorio contar ya con el registro fiscal, o se puede tramitar en paralelo? Lo pregunto porque estamos revisando procesos como el de https://e-residence.com/it/nie-spain-online/madrid/ para agilizar la documentación en Madrid y no queremos que la burocracia retrase la compra del acero. ¡Gracias de antemano!

Sarah

Leave a comment