ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

NM300

NM300

Premium NM300 Wear Resistant Steel by MetalZenith

MetalZenith's NM300 is a high-performance wear resistant steel plate engineered for exceptional durability in demanding industrial applications. As a leading steel manufacturer, MetalZenith produces this premium grade steel using advanced metallurgical processes and state-of-the-art equipment to ensure consistent quality and superior performance characteristics.

Advanced Manufacturing Capabilities

Our specialized production facilities utilize controlled rolling and quenching technologies to achieve optimal hardness levels of 280-320 HBW. MetalZenith's precision heat treatment processes ensure uniform microstructure and mechanical properties throughout the material thickness, delivering reliable performance in abrasive environments.

Key Applications

  • Mining equipment and wear plates
  • Construction machinery components
  • Material handling systems
  • Agricultural equipment
  • Recycling and waste management machinery

Quality Assurance Excellence

MetalZenith maintains rigorous quality control standards with comprehensive testing protocols including chemical analysis, mechanical property verification, and dimensional inspection. Our ISO 9001:2015 certified facilities ensure every NM300 plate meets international standards and customer specifications, backed by full material traceability and certification documentation.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

NM300 is a quenched and tempered wear resistant steel with a martensitic microstructure optimized for abrasion resistance. The controlled chemical composition and precise heat treatment process result in a fine-grained structure with excellent toughness-to-hardness ratio.

Heat Treatment Process

MetalZenith's advanced heat treatment involves austenitizing at 900-950°C followed by controlled water quenching to achieve the desired hardness. Tempering at 200-250°C ensures optimal balance between hardness and toughness while maintaining dimensional stability.

Manufacturing Process

Production begins with electric arc furnace melting using premium raw materials, followed by ladle refining and continuous casting. The steel undergoes controlled rolling in our state-of-the-art hot rolling mill, ensuring uniform thickness and surface quality. Final heat treatment is performed in computer-controlled furnaces with precise temperature monitoring.

Quality Standards

All NM300 products are manufactured in accordance with ISO 9001:2015 quality management systems. Comprehensive testing includes chemical analysis via optical emission spectroscopy, mechanical property verification through tensile and impact testing, hardness mapping, and ultrasonic inspection for internal soundness. Each shipment includes material test certificates and full traceability documentation.

Welding and Fabrication

NM300 can be welded using conventional methods with appropriate preheating (150-200°C) and post-weld heat treatment when required. MetalZenith provides comprehensive welding guidelines and technical support to ensure optimal joint properties and performance in service.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.25
Manganese (Mn)1.60
Silicon (Si)≤ 0.70
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.010
Chromium (Cr)0.25
Nickel (Ni)0.25
Molybdenum (Mo)0.25
Boron (B)0.004
Aluminum (Al)≥ 0.015

⚙️ Mechanical Properties

PropertyValue
Hardness (HBW)280-320
Tensile Strength (Rm)950-1250 MPa
Yield Strength (Rp0.2)≥ 700 MPa
Elongation (A5)≥ 10%
Impact Energy (KV) at -20°C≥ 30 J
Impact Energy (KV) at -40°C≥ 25 J
Young's Modulus210 GPa
Fatigue Limit450 MPa
Reduction of Area≥ 35%

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1510°C
Thermal Conductivity (20°C)42 W/m·K
Thermal Expansion Coefficient (20-100°C)12×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity0.18 µΩ·m
Magnetic PermeabilityFerromagnetic
Poisson's Ratio0.27-0.30
Thermal Diffusivity11.6 mm²/s

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Coils, Cut-to-size pieces
Thickness Range4-80 mm
Width Range1000-3200 mm
Length Range2000-12000 mm
StandardsEN 10204-3.1, ASTM A514, JIS G3114
Surface FinishHot rolled, Shot blasted, Pickled
Thickness Tolerance±0.3 mm (4-20mm), ±0.5 mm (>20mm)
Width Tolerance±5 mm
Length Tolerance±10 mm
Flatness≤5 mm/m

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing NM300

Manufacturing Advantage 1

Advanced Quenching Technology

MetalZenith employs state-of-the-art controlled quenching systems with precise temperature monitoring to achieve uniform hardness distribution and optimal microstructure in NM300 steel plates, ensuring consistent wear resistance properties.

Comprehensive Quality Testing

Our integrated quality control laboratory conducts extensive mechanical testing, chemical analysis, and non-destructive testing on every batch of NM300 steel, guaranteeing compliance with international standards and customer specifications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing Solutions

MetalZenith offers complete customization services including precision cutting, machining, forming, and surface treatment for NM300 steel plates, delivering ready-to-use components tailored to specific application requirements.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo