Maraging Steel

Maraging Steel

Maraging Steel - Ultra-High Strength Structural Steel

Maraging Steel is an ultra-high strength structural steel renowned for its exceptional combination of strength, toughness, and dimensional stability. This precipitation-hardened steel achieves remarkable mechanical properties through age-hardening of a low-carbon, high-nickel martensitic matrix, making it ideal for demanding structural applications requiring superior performance.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum induction melting and controlled atmosphere processing to produce Maraging Steel with exceptional purity and homogeneity. Our precision age-hardening processes with computer-controlled temperature profiles ensure optimal precipitation of intermetallic compounds, delivering consistent ultra-high strength properties throughout the material cross-section.

Key Applications

  • High-performance structural components in aerospace and defense
  • Critical load-bearing elements in bridge construction
  • Precision machinery frames and high-stress mechanical components
  • Advanced automotive chassis and safety-critical vehicle structures
  • Specialized engineering applications requiring ultra-high strength

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and detailed metallographic analysis. Our Maraging Steel meets ASTM A538 and AMS specifications, ensuring reliability in critical structural applications where failure is not an option.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Maraging Steel features a unique low-carbon, high-nickel martensitic matrix that transforms during solution treatment at 815-845°C. The microstructure consists of lath martensite with fine, coherent precipitates of Ni3Mo, Ni3Ti, and Fe2Mo intermetallic compounds formed during age-hardening. This precipitation strengthening mechanism provides exceptional strength while maintaining good toughness and dimensional stability.

Heat Treatment Process

MetalZenith employs a two-stage heat treatment process: solution annealing at 820°C followed by controlled cooling, then precision age-hardening at 480°C for 3 hours. Our vacuum furnaces with protective atmosphere prevent decarburization and ensure uniform heating throughout the cross-section, critical for achieving consistent ultra-high strength properties.

Manufacturing Process Excellence

Our manufacturing process begins with vacuum induction melting to ensure exceptional cleanliness and homogeneity. Controlled forging and rolling operations maintain optimal grain structure, followed by precision machining capabilities for complex geometries. Advanced quality control includes ultrasonic testing, magnetic particle inspection, and comprehensive mechanical property verification.

Specialized Quality Testing

MetalZenith conducts extensive testing specific to structural applications: TIG and electron beam weldability assessment with post-weld heat treatment optimization, forming limit analysis for complex structural shapes, high-cycle fatigue testing under variable amplitude loading, and atmospheric corrosion resistance evaluation in industrial environments. These tests ensure reliable performance in critical structural applications.

Structural Application Engineering

For building structures, our Maraging Steel provides exceptional strength-to-weight ratios enabling innovative architectural designs. In bridge engineering, the material's fatigue resistance and dimensional stability ensure long-term structural integrity under dynamic loading. For machinery manufacturing, the combination of high strength and machinability allows precision components with tight tolerances. In vehicle manufacturing, the material enables lightweight yet ultra-strong safety structures, while general engineering applications benefit from the material's versatility and reliability in high-stress environments.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.03
Nickel (Ni)17.0 - 19.0
Cobalt (Co)8.0 - 12.0
Molybdenum (Mo)4.6 - 5.2
Titanium (Ti)0.6 - 0.8
Aluminum (Al)0.05 - 0.15
Silicon (Si)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 1720
Tensile Strength (MPa)1860 - 2070
Elongation (%)≥ 8
Impact Energy at RT (J)≥ 20
Hardness (HRC)50 - 55
Fatigue Strength (MPa)≥ 690

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.00
Melting Point (°C)1413 - 1440
Thermal Conductivity (W/m·K)17.4
Thermal Expansion (×10??/K)10.1
Elastic Modulus (GPa)186
Poisson's Ratio0.31

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Bars, Forgings, Precision Machined Components
Thickness Range3 - 200mm
Width Range100 - 2000mm
Length Range500 - 6000mm
Standards ComplianceASTM A538, AMS 6514, AMS 6521
Heat Treatment ConditionSolution Annealed + Age Hardened
Surface FinishHot Rolled, Cold Finished, Precision Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Maraging Steel

Manufacturing Advantage 1

Precision Age-Hardening Technology

MetalZenith utilizes advanced vacuum induction melting followed by precisely controlled age-hardening processes at 480-500°C. Our computer-controlled furnaces with ±3°C temperature accuracy ensure optimal precipitation of Ni3Mo, Ni3Ti, and Fe2Mo intermetallic compounds, achieving consistent ultra-high strength properties.

Comprehensive Structural Testing

Our specialized testing protocols include advanced weldability assessment using controlled thermal severity tests, forming limit analysis for complex geometries, high-cycle fatigue testing up to 10^7 cycles, and accelerated atmospheric corrosion testing. These ensure optimal performance in demanding structural applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Engineering Solutions

MetalZenith provides tailored age-hardening treatments, precision machining services, and comprehensive technical support for structural applications. Our metallurgical engineers work closely with clients to optimize material properties for specific load requirements and environmental conditions.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo