Maraging 350 Steel

Maraging 350 Steel

Maraging 350 Ultra-High Strength Structural Steel

Maraging 350 is an ultra-high strength structural steel renowned for exceptional strength-to-weight ratio and superior toughness. This precipitation-hardened martensitic steel delivers outstanding mechanical properties through age-hardening treatment, making it ideal for critical structural applications requiring maximum strength and reliability.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision vacuum induction melting and controlled aging processes to produce Maraging 350 steel with exceptional uniformity and mechanical properties. Our advanced metallurgical control ensures optimal precipitation of intermetallic compounds, delivering consistent ultra-high strength and excellent dimensional stability throughout the material.

Key Applications

  • High-performance structural components in aerospace and defense
  • Critical load-bearing elements in bridge construction
  • Heavy machinery frames and structural supports
  • High-strength vehicle chassis and safety structures
  • Precision tooling and high-stress engineering components

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete metallographic analysis. Our Maraging 350 steel meets ASTM A538 and AMS specifications, ensuring superior performance in demanding structural applications with full traceability and certification.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Maraging 350 exhibits a unique martensitic microstructure strengthened by precipitation of intermetallic compounds including Ni3Mo, Ni3Ti, and Fe2Mo during aging treatment. The low carbon content ensures excellent weldability while maintaining ultra-high strength through age hardening mechanisms. The fine martensitic matrix provides exceptional toughness and dimensional stability.

Heat Treatment Process

MetalZenith employs solution annealing at 815-845°C followed by controlled aging at 480°C for 3 hours. This precise thermal cycle ensures optimal precipitation of strengthening phases while maintaining excellent ductility and impact resistance. Our controlled atmosphere processing prevents oxidation and ensures consistent properties throughout the material cross-section.

Manufacturing Process Excellence

Our advanced vacuum induction melting process ensures exceptional cleanliness and homogeneity. Controlled forging and rolling operations maintain optimal grain structure, while our proprietary aging cycles deliver consistent ultra-high strength properties. Real-time monitoring systems ensure precise temperature control throughout all processing stages.

Specialized Quality Testing

Comprehensive testing includes TIG and MIG welding performance evaluation, bend testing for forming behavior assessment, rotating beam fatigue testing to 10^7 cycles, and salt spray corrosion testing per ASTM B117. Ultrasonic inspection ensures internal soundness while hardness mapping verifies uniform age hardening response.

Structural Application Considerations

For building construction, Maraging 350 provides exceptional strength-to-weight ratios in critical load-bearing applications. Bridge engineering benefits from superior fatigue resistance and dimensional stability. Machinery manufacturing utilizes the excellent machinability and weldability for precision structural components. Vehicle manufacturing leverages the high strength for weight reduction while maintaining safety performance. General engineering applications benefit from the combination of ultra-high strength and good toughness for demanding structural requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.03
Nickel (Ni)17.0 - 19.0
Cobalt (Co)11.5 - 12.5
Molybdenum (Mo)4.6 - 5.2
Titanium (Ti)1.3 - 1.8
Aluminum (Al)0.05 - 0.15
Silicon (Si)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 2400
Tensile Strength (MPa)2450 - 2650
Elongation (%)≥ 8
Impact Energy at RT (J)≥ 20
Hardness (HRC)50 - 55
Fatigue Strength (MPa)≥ 1200

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.10
Melting Point (°C)1413 - 1440
Thermal Conductivity (W/m·K)17.0
Thermal Expansion (×10??/K)10.1
Elastic Modulus (GPa)186
Poisson's Ratio0.31

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Bars, Forgings, Billets, Custom Shapes
Thickness Range3 - 200mm
Width Range100 - 2000mm
Length Range500 - 6000mm
Standards ComplianceASTM A538, AMS 6514, MIL-S-46850
Heat Treatment ConditionSolution Annealed + Aged
Surface FinishHot Rolled, Cold Finished, Machined

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Maraging 350 Steel

Manufacturing Advantage 1

Precision Vacuum Melting & Age Hardening

MetalZenith utilizes advanced vacuum induction melting followed by controlled aging at 480°C to achieve optimal precipitation hardening. Our precise temperature control and atmosphere management ensure consistent ultra-high strength properties and exceptional dimensional stability throughout the material cross-section.

Comprehensive Structural Performance Testing

Our quality assurance includes specialized testing for structural applications: advanced welding performance evaluation, forming behavior analysis under high stress, fatigue strength testing up to 10^7 cycles, and accelerated atmospheric corrosion resistance testing to ensure long-term structural integrity.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Structural Solutions & Engineering Support

MetalZenith provides tailored processing solutions including custom heat treatment cycles, precision machining to tight tolerances, and comprehensive technical support for structural design optimization. Our engineering team assists with material selection and application-specific property enhancement.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo