ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

Maraging 250 Steel

Maraging 250 Steel

Maraging 250 Ultra-High Strength Structural Steel

Maraging 250 is an ultra-high strength structural steel renowned for its exceptional combination of strength, toughness, and dimensional stability. This precipitation-hardened martensitic steel delivers outstanding mechanical properties while maintaining excellent weldability and machinability, making it ideal for critical structural applications requiring superior performance.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum induction melting and controlled aging processes to produce Maraging 250 steel with exceptional purity and uniform microstructure. Our precision heat treatment protocols ensure optimal precipitation of intermetallic compounds, delivering consistent ultra-high strength properties throughout the material cross-section.

Key Applications

  • High-performance building structures and skyscrapers
  • Critical bridge components and cable-stayed structures
  • Heavy machinery frames and precision equipment
  • Automotive chassis and high-strength vehicle components
  • General engineering applications requiring ultra-high strength

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete metallurgical analysis. Our Maraging 250 steel meets ASTM A538 and AMS specifications, ensuring reliability in demanding structural applications with full traceability and certification documentation.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Maraging 250 features a unique martensitic microstructure strengthened by precipitation of intermetallic compounds including Ni?Mo, Ni?Ti, and Fe?Mo. The low carbon content ensures excellent weldability while the controlled addition of nickel, cobalt, molybdenum, and titanium provides exceptional strength through age hardening. The fine martensitic matrix offers superior toughness compared to conventional high-strength steels.

Heat Treatment Process

MetalZenith employs a two-stage heat treatment process: solution annealing at 820°C followed by aging at 480°C for 3 hours. This controlled thermal processing ensures optimal precipitation of strengthening phases while maintaining dimensional stability and minimizing residual stresses critical for structural applications.

Advanced Manufacturing Process

Our production utilizes vacuum induction melting (VIM) followed by vacuum arc remelting (VAR) to achieve exceptional cleanliness and homogeneity. Controlled forging and rolling operations ensure optimal grain structure and mechanical property distribution, while our proprietary aging protocols deliver consistent ultra-high strength performance.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including welding performance evaluation using standard structural welding procedures, forming limit analysis for complex geometries, high-cycle fatigue testing up to 10? cycles, and accelerated atmospheric corrosion testing per ASTM standards to ensure long-term structural integrity.

Structural Engineering Considerations

For building structures, Maraging 250 offers exceptional strength-to-weight ratios enabling lighter designs. In bridge engineering, its fatigue resistance and dimensional stability ensure long service life. For machinery manufacturing, the combination of strength and machinability allows complex component fabrication. In vehicle manufacturing, the material provides crash performance and weight reduction benefits. General engineering applications benefit from the predictable mechanical properties and excellent joining characteristics.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.03
Nickel (Ni)17.0 - 19.0
Cobalt (Co)8.0 - 9.0
Molybdenum (Mo)4.6 - 5.2
Titanium (Ti)0.6 - 0.8
Aluminum (Al)0.05 - 0.15
Silicon (Si)≤ 0.10
Iron (Fe)Balance

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 1720
Tensile Strength (MPa)1790 - 1930
Elongation (%)≥ 8
Impact Energy at RT (J)≥ 20
Hardness (HRC)50 - 55
Fatigue Strength (MPa)≥ 690

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.00
Melting Point (°C)1413 - 1440
Thermal Conductivity (W/m·K)20.1
Thermal Expansion (×10??/K)10.1
Elastic Modulus (GPa)186
Poisson's Ratio0.31

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Bars, Forgings, Billets, Custom Shapes
Thickness Range3 - 200mm
Width Range100 - 2000mm
Length Range500 - 6000mm
Standards ComplianceASTM A538, AMS 6514, DIN 1.2709
Heat Treatment ConditionSolution Annealed + Aged
Surface FinishHot Rolled, Cold Finished, Machined

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Maraging 250 Steel

Manufacturing Advantage 1

Precision Vacuum Melting & Aging Process

MetalZenith utilizes advanced vacuum induction melting followed by controlled aging at 480°C to achieve optimal precipitation hardening. Our precise temperature control and atmosphere management ensure uniform microstructure and exceptional mechanical properties throughout the material thickness.

Comprehensive Structural Performance Testing

Our quality assurance includes specialized testing for structural applications: advanced welding performance evaluation, forming limit analysis, high-cycle fatigue testing, and accelerated atmospheric corrosion resistance testing to ensure superior performance in demanding structural environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Structural Solutions & Engineering Support

MetalZenith provides comprehensive custom processing services including precision machining, heat treatment optimization, and dimensional inspection. Our technical team offers engineering support for structural design optimization and material selection to maximize performance in specific applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo