M2 High-Speed Tool Steel

M2 is a premium tungsten-molybdenum high-speed tool steel renowned for its exceptional hardness, wear resistance, and red hardness retention at elevated temperatures. This versatile tool steel is specifically engineered for demanding cutting applications and precision tooling where superior performance and extended tool life are critical.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs state-of-the-art vacuum melting and powder metallurgy processes to produce M2 tool steel with superior carbide distribution and microstructural uniformity. Our advanced heat treatment facilities ensure optimal hardness profiles and dimensional stability, critical for precision cutting tools and high-performance applications.

Key Applications

  • High-speed cutting tools and drill bits
  • Cold forming dies and punching tools
  • Precision bearing components and races
  • Automotive engine components and transmission parts
  • Precision machinery components and gauges

Quality Assurance & Certifications

MetalZenith maintains comprehensive quality control throughout production, including ultrasonic testing, hardness mapping, carbide distribution analysis, and complete metallographic examination. Our M2 tool steel meets ASTM A600, AISI M2, and international tool steel standards, ensuring reliability in critical precision applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

M2 tool steel exhibits a complex microstructure consisting of a tempered martensitic matrix with uniformly distributed primary and secondary carbides. The high tungsten and molybdenum content provides exceptional red hardness and wear resistance, while vanadium carbides contribute to superior cutting edge retention. The fine carbide distribution achieved through MetalZenith's controlled solidification process ensures optimal tool performance.

Heat Treatment Process

MetalZenith employs vacuum hardening at 1210-1230°C followed by controlled cooling and multiple tempering cycles at 540-580°C. Our precise heat treatment protocols ensure optimal hardness distribution while minimizing retained austenite content below 8%. Cryogenic treatment at -80°C is available for enhanced dimensional stability and wear resistance.

Manufacturing Process

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to achieve superior cleanliness and carbide distribution. Our controlled forging and rolling processes ensure optimal grain flow and mechanical properties. Advanced powder metallurgy routes are available for applications requiring ultra-fine carbide distribution and isotropic properties.

Specialized Quality Testing

Our comprehensive testing protocol includes Rockwell hardness mapping across cross-sections, X-ray diffraction analysis for retained austenite quantification, metallographic evaluation of carbide size and distribution, and rotating beam fatigue testing at various stress levels. Ultrasonic inspection ensures internal soundness critical for high-performance tooling applications.

Application Engineering

For cutting tool applications, M2 provides excellent balance of hardness and toughness with superior edge retention. In cold forming dies, the high compressive strength and wear resistance ensure extended tool life. For bearing manufacturing, the fine carbide structure and high hardness provide exceptional rolling contact fatigue resistance. Precision machinery components benefit from dimensional stability and consistent mechanical properties, while automotive applications leverage the material's reliability under cyclic loading conditions.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.78 - 0.88
Chromium (Cr)3.75 - 4.50
Molybdenum (Mo)4.50 - 5.50
Tungsten (W)5.50 - 6.75
Vanadium (V)1.75 - 2.20
Silicon (Si)0.20 - 0.45
Manganese (Mn)0.15 - 0.40
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)63 - 65
Compressive Strength (MPa)≥ 4000
Impact Toughness (J)15 - 25
Wear Resistance Index8.5 - 9.2
Hardenability (mm)≥ 75
Red Hardness at 600°C (HRC)≥ 58

🔬 Physical Properties

PropertyValue
Density (g/cm3)8.16
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)24.3
Thermal Expansion (×10??/K)10.8
Elastic Modulus (GPa)230
Poisson's Ratio0.27

📏 Product Specifications

SpecificationDetails
Available FormsBars, Rods, Plates, Forgings, Powder
Diameter Range6 - 500mm
Thickness Range3 - 200mm
Length Range100 - 6000mm
Standards ComplianceASTM A600, AISI M2, DIN 1.3343
Heat Treatment ConditionAnnealed, Hardened & Tempered
Surface FinishGround, Turned, Centerless Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing M2 Tool Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes vacuum induction melting and electroslag remelting processes with precise temperature control to achieve optimal carbide distribution and eliminate inclusions. Our advanced melting technology ensures consistent chemical composition and superior metallurgical cleanliness throughout the material.

Comprehensive Tool Steel Testing

MetalZenith conducts specialized testing including Rockwell hardness mapping across sections, retained austenite content analysis via X-ray diffraction, carbide distribution evaluation through metallographic analysis, and rotating beam fatigue testing to ensure optimal tool performance and longevity.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment Services

MetalZenith offers specialized heat treatment services including vacuum hardening, precise tempering cycles, and cryogenic treatment. Our metallurgical engineers provide technical support for optimal hardness profiles and dimensional stability tailored to specific tooling applications.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo