SCM435

SCM435

SCM435 Chromium-Molybdenum Alloy Structural Steel

SCM435 is a high-strength chromium-molybdenum alloy structural steel designed for demanding applications requiring exceptional strength, toughness, and hardenability. This versatile steel grade offers superior mechanical properties through controlled alloying and heat treatment, making it ideal for critical structural components in automotive, machinery, and construction industries.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision electric arc furnace melting and controlled rolling processes to produce SCM435 steel with exceptional uniformity and mechanical properties. Our advanced quenching and tempering facilities ensure optimal microstructural development, delivering consistent hardenability and superior fatigue resistance critical for structural applications.

Key Applications

  • Automotive drive shafts, axles, and transmission components
  • Heavy machinery structural frames and supports
  • Bridge construction and structural steelwork
  • Industrial equipment housings and brackets
  • High-stress bolts and fasteners for construction

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control throughout production, including comprehensive mechanical testing, ultrasonic inspection, and complete chemical analysis. Our SCM435 steel meets JIS G4053, ASTM A29, and ISO 683 standards, ensuring reliability in critical structural applications with full traceability and certification documentation.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

SCM435 exhibits a tempered martensitic microstructure after proper quenching and tempering treatment. The chromium content enhances hardenability and provides moderate corrosion resistance, while molybdenum additions improve high-temperature strength and reduce temper brittleness. The fine-grained structure achieved through controlled processing ensures excellent combination of strength and toughness essential for structural applications.

Heat Treatment Process

MetalZenith employs controlled austenitizing at 850-880°C followed by oil quenching to achieve uniform martensitic transformation. Subsequent tempering at 550-650°C optimizes the strength-toughness balance. Our computer-controlled heat treatment ensures consistent mechanical properties and eliminates internal stresses critical for structural integrity.

Manufacturing Excellence

Our production process includes vacuum degassing for enhanced cleanliness, controlled rolling for grain refinement, and precision heat treatment with real-time monitoring. Advanced quality control systems ensure dimensional accuracy and surface quality meeting the most demanding structural applications.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including welding performance evaluation per AWS standards, forming capability assessment through bend testing, rotating beam fatigue testing, and salt spray atmospheric corrosion testing. These specialized tests ensure optimal performance in structural applications where reliability is paramount.

Application Engineering

For building construction, SCM435 provides excellent weldability and forming characteristics essential for complex structural assemblies. In bridge engineering, its superior fatigue resistance ensures long-term durability under cyclic loading. For machinery manufacturing, the high strength-to-weight ratio enables compact designs, while in vehicle construction, the material's crashworthiness and formability meet safety requirements. General engineering applications benefit from the steel's versatility and consistent mechanical properties across various processing conditions.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.33 - 0.38
Manganese (Mn)0.60 - 0.85
Silicon (Si)0.15 - 0.35
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Chromium (Cr)0.90 - 1.20
Molybdenum (Mo)0.15 - 0.30
Nickel (Ni)≤ 0.25

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 835
Tensile Strength (MPa)980 - 1180
Elongation (%)≥ 12
Impact Energy at 20°C (J)≥ 49
Hardness (HRC)30 - 37
Fatigue Strength (MPa)≥ 450

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.85
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)42.7
Thermal Expansion (×10??/K)12.3
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsRound Bars, Square Bars, Flat Bars, Plates, Forgings
Diameter Range10 - 300mm
Length Range3000 - 12000mm
Plate Thickness8 - 80mm
Standards ComplianceJIS G4053, ASTM A29, ISO 683-2
Heat Treatment ConditionQuenched and Tempered (Q&T)
Surface FinishHot Rolled, Cold Drawn, Machined

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing SCM435

Manufacturing Advantage 1

Advanced Heat Treatment Technology

MetalZenith utilizes state-of-the-art quenching and tempering processes with precise temperature control and automated cooling systems to achieve optimal microstructural refinement in SCM435 steel. Our controlled heat treatment ensures consistent hardenability and superior mechanical properties throughout the material cross-section.

Comprehensive Structural Testing

Our quality assurance program includes specialized testing for structural applications: advanced welding performance evaluation, forming capability assessment, fatigue strength testing up to 10^7 cycles, and accelerated atmospheric corrosion resistance testing to ensure long-term structural integrity in demanding environments.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Engineering Support

MetalZenith provides tailored heat treatment schedules, precision machining services, and comprehensive technical support for SCM435 applications. Our metallurgical engineers work closely with customers to optimize material properties for specific structural requirements and provide complete material certification documentation.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo