Knife Steel - Premium Stainless Steel for Cutting Applications

Knife Steel is a high-performance stainless steel specifically engineered for cutting tools and blade applications requiring exceptional sharpness retention, corrosion resistance, and durability. This martensitic stainless steel combines superior hardness with excellent edge stability, making it ideal for professional cutlery, surgical instruments, and precision cutting tools.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision vacuum melting and controlled atmosphere heat treatment to produce Knife Steel with exceptional purity and uniform microstructure. Our advanced quenching and tempering processes ensure optimal carbide distribution and grain refinement, delivering superior cutting performance and extended service life in demanding applications.

Key Applications

  • Medical and surgical instruments for healthcare applications
  • Food processing equipment and commercial kitchen tools
  • Chemical processing equipment requiring corrosion resistance
  • Marine cutting tools and offshore equipment
  • Architectural hardware and decorative cutting elements

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including pitting potential testing, intergranular corrosion assessment, stress corrosion cracking evaluation, and passivation film thickness measurement. Our Knife Steel meets FDA food contact requirements, ASTM standards, and medical device regulations, ensuring reliability in critical cutting applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Knife Steel exhibits a martensitic microstructure with fine, uniformly distributed chromium carbides that provide exceptional wear resistance and edge retention. The high carbon content combined with chromium and molybdenum creates a matrix of tempered martensite with secondary carbide precipitation, optimizing the balance between hardness and toughness essential for cutting applications.

Heat Treatment Process

MetalZenith employs controlled atmosphere hardening at 1030-1065°C followed by immediate quenching in oil or air. Tempering is performed at 150-200°C to achieve target hardness while maintaining corrosion resistance. Our proprietary sub-zero treatment at -80°C ensures complete austenite transformation and dimensional stability.

Manufacturing Process

MetalZenith utilizes vacuum induction melting followed by electroslag remelting to achieve exceptional cleanliness and homogeneity. Hot working is performed with precise temperature control to optimize carbide distribution, followed by controlled cooling and stress relief annealing before final heat treatment.

Specialized Quality Testing

Our comprehensive testing protocol includes pitting potential measurement (ASTM G61), intergranular corrosion testing (ASTM A262 Practice A), stress corrosion cracking evaluation in 3.5% NaCl solution, and passivation film thickness analysis using X-ray photoelectron spectroscopy. Edge retention testing and microstructural analysis ensure consistent cutting performance.

Application-Specific Considerations

For medical instruments, our steel meets biocompatibility requirements with superior corrosion resistance in body fluids. Food industry applications benefit from FDA compliance and resistance to organic acids. Chemical equipment applications leverage excellent resistance to mild acids and oxidizing environments. Marine applications utilize the steel's resistance to chloride-induced corrosion, while architectural applications benefit from long-term aesthetic stability and minimal maintenance requirements.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.95 - 1.20
Chromium (Cr)17.0 - 18.0
Molybdenum (Mo)0.75 - 1.20
Vanadium (V)0.07 - 0.12
Silicon (Si)≤ 1.00
Manganese (Mn)≤ 1.00
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 1900
Tensile Strength (MPa)2000 - 2200
Elongation (%)≥ 8
Hardness (HRC)58 - 62
Corrosion ResistanceExcellent in mild acids
Impact Energy (J)≥ 15

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.70
Melting Point (°C)1480 - 1530
Thermal Conductivity (W/m·K)24.2
Thermal Expansion (×10??/K)10.4
Electrical Resistivity (μΩ·cm)60
Elastic Modulus (GPa)200

📏 Product Specifications

SpecificationDetails
Available FormsBars, Sheets, Strips, Wire, Forgings
Thickness Range0.5 - 50mm
Width Range10 - 1500mm
Length Range500 - 6000mm
Standards ComplianceASTM A681, AISI 440C, DIN 1.4125
Heat Treatment ConditionHardened & Tempered
Surface FinishBright Annealed, Polished, Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Knife Steel

Manufacturing Advantage 1

Precision Vacuum Melting Technology

MetalZenith utilizes advanced vacuum induction melting with controlled atmosphere processing to achieve exceptional steel purity and uniform carbide distribution. Our precision heat treatment cycles with computer-controlled quenching and tempering ensure optimal hardness and toughness balance for superior cutting performance.

Comprehensive Corrosion Testing

MetalZenith conducts extensive corrosion testing including pitting potential measurement (>300mV vs SCE), ASTM A262 intergranular corrosion testing, stress corrosion cracking evaluation in chloride environments, and passivation film thickness analysis using XPS technology to ensure maximum corrosion resistance in service.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Technical Support

MetalZenith offers comprehensive custom processing services including precision machining, specialized heat treatment cycles, surface finishing, and edge geometry optimization. Our metallurgical engineers provide technical support for application-specific requirements and performance optimization.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo