ข้ามไปยังข้อมูลผลิตภัณฑ์
1 ของ 1

H11 Tool Steel

H11 Tool Steel

H11 Premium Hot Work Tool Steel

H11 is a premium chromium-molybdenum-vanadium hot work tool steel renowned for its exceptional high-temperature strength, thermal shock resistance, and superior hardenability. This versatile tool steel is specifically engineered for demanding applications requiring sustained performance under elevated temperatures and thermal cycling conditions.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs advanced vacuum melting and electroslag remelting (ESR) processes to produce H11 tool steel with exceptional cleanliness and homogeneity. Our proprietary heat treatment protocols and precise temperature control ensure optimal carbide distribution and maximum hardenability, delivering superior performance in critical tooling applications.

Key Applications

  • Hot forging dies and extrusion tooling
  • Die casting dies for aluminum and magnesium
  • Plastic injection molding tools
  • Hot shearing blades and punches
  • Precision automotive components and tooling
  • High-temperature bearing applications

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including ultrasonic testing, comprehensive hardness mapping, carbide distribution analysis, and thermal fatigue testing. Our H11 tool steel meets ASTM A681 specifications and undergoes specialized testing for residual austenite content and grain size uniformity, ensuring consistent performance in demanding tooling applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

H11 tool steel exhibits a tempered martensitic microstructure with uniformly distributed secondary carbides of chromium, molybdenum, and vanadium. The balanced alloy composition provides excellent hot hardness retention up to 600°C while maintaining superior toughness. The fine carbide distribution ensures exceptional wear resistance and thermal fatigue resistance critical for hot work applications.

Heat Treatment Process

MetalZenith employs controlled atmosphere hardening at 1010-1040°C followed by oil or air quenching, then tempering at 540-650°C depending on desired hardness. Our vacuum heat treatment capabilities eliminate decarburization and ensure uniform hardness distribution. Multiple tempering cycles optimize the carbide precipitation and stress relief for maximum tool life.

Advanced Manufacturing Process

Our H11 production utilizes vacuum induction melting (VIM) followed by electroslag remelting (ESR) to achieve exceptional cleanliness and homogeneity. Controlled forging and rolling operations ensure optimal grain flow and carbide distribution. Advanced annealing processes provide excellent machinability while maintaining uniform hardness throughout the cross-section.

Specialized Quality Testing

MetalZenith conducts comprehensive Rockwell hardness distribution mapping across tool sections, X-ray diffraction analysis for residual austenite content (typically <2%), detailed metallographic examination of carbide size and distribution, and rotating beam fatigue testing at elevated temperatures. Thermal shock testing simulates actual service conditions to validate tool performance.

Application-Specific Technical Considerations

For cutting tool applications, H11 provides excellent hot hardness and wear resistance with optimized edge retention. In die casting and forging operations, the superior thermal shock resistance and high-temperature strength ensure extended die life. For precision automotive components, the excellent hardenability and dimensional stability during heat treatment enable tight tolerance maintenance. In bearing applications, the balanced hardness and toughness provide reliable performance under high loads and temperatures.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.33 - 0.43
Chromium (Cr)4.75 - 5.50
Molybdenum (Mo)1.10 - 1.75
Vanadium (V)0.30 - 0.60
Silicon (Si)0.80 - 1.20
Manganese (Mn)0.20 - 0.50
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)38 - 45 (Hardened & Tempered)
Compressive Strength (MPa)2400 - 2800
Impact Toughness (J)15 - 25 (Charpy V-notch)
Wear Resistance IndexExcellent (8.5/10)
Hardenability (DI)6.5 - 8.0 inches
Fatigue Strength (MPa)800 - 1000

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.80
Melting Point (°C)1480 - 1520
Thermal Conductivity (W/m·K)24.5 (at 20°C)
Thermal Expansion (×10??/K)11.9 (20-100°C)
Elastic Modulus (GPa)215
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsBars, Blocks, Plates, Forgings, Custom Shapes
Diameter Range10 - 500mm
Thickness Range5 - 300mm
Length Range500 - 6000mm
Standards ComplianceASTM A681, DIN 1.2343, JIS SKD6
Heat Treatment ConditionAnnealed, Hardened & Tempered, or As-Forged
Surface FinishHot Rolled, Machined, Ground, or Polished

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing H11 Tool Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes state-of-the-art vacuum induction melting (VIM) and electroslag remelting (ESR) processes to achieve exceptional steel cleanliness and homogeneity. Our controlled atmosphere processing eliminates inclusions and ensures uniform carbide distribution, resulting in superior tool performance and extended service life.

Comprehensive Tool Steel Testing

Our specialized testing protocols include Rockwell hardness distribution mapping, residual austenite content analysis using X-ray diffraction, carbide distribution evaluation through metallographic analysis, and rotating beam fatigue strength testing. These advanced quality measures ensure consistent performance in critical tooling applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment Solutions

MetalZenith offers tailored heat treatment services including vacuum hardening, precise tempering cycles, and cryogenic treatment options. Our metallurgical experts provide comprehensive technical support for optimizing tool performance in specific applications, from die casting to precision machining operations.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo