D3 Tool Steel

D3 Tool Steel

D3 High Carbon High Chromium Tool Steel

D3 is a high carbon, high chromium cold work tool steel renowned for its exceptional wear resistance, dimensional stability, and moderate toughness. This air-hardening steel grade is specifically engineered for demanding applications requiring superior abrasion resistance and edge retention in cutting tools, forming dies, and precision manufacturing components.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs advanced vacuum melting and controlled forging processes to produce D3 tool steel with exceptional carbide distribution and microstructural uniformity. Our proprietary heat treatment protocols ensure optimal hardness gradients and minimize residual stress, delivering superior performance in critical tooling applications.

Key Applications

  • Cutting tools for metal forming and machining operations
  • Cold forming dies and punches for automotive components
  • Precision bearing races and rolling elements
  • High-wear machine components and guides
  • Stamping dies for electronics and appliance manufacturing

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including ultrasonic testing, comprehensive hardness mapping, carbide distribution analysis, and residual austenite measurement. Our D3 tool steel meets ASTM A681 specifications and undergoes specialized testing for fatigue strength and dimensional stability, ensuring reliability in precision tooling applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

D3 tool steel exhibits a complex microstructure consisting of a martensitic matrix with uniformly distributed chromium carbides (M7C3 and M23C6). The high carbon content (2.0-2.35%) combined with significant chromium addition (11-13%) provides exceptional wear resistance through hard carbide formation. The air-hardening characteristics eliminate the need for oil quenching, reducing distortion and cracking risks in complex tool geometries.

Heat Treatment Process

MetalZenith employs controlled atmosphere hardening at 980-1020°C followed by air cooling to achieve optimal hardness. Sub-zero treatment at -80°C is applied to minimize retained austenite content below 5%. Double tempering at 150-200°C ensures dimensional stability and stress relief while maintaining hardness levels of 58-62 HRC for maximum tool performance.

Advanced Manufacturing Process

Our production process begins with vacuum induction melting to ensure chemical homogeneity and minimize inclusions. Electroslag remelting further refines the microstructure and eliminates segregation. Controlled forging with precise temperature monitoring optimizes grain flow and carbide distribution. Final machining and grinding operations maintain tight dimensional tolerances critical for precision tooling applications.

Specialized Quality Testing

MetalZenith implements comprehensive testing protocols including Rockwell hardness distribution mapping across the entire cross-section, X-ray diffraction analysis for retained austenite quantification (target <5%), metallographic examination of carbide size and distribution uniformity, and rotating beam fatigue testing at 10^7 cycles. Dimensional stability testing under thermal cycling conditions ensures predictable performance in precision applications.

Application-Specific Technical Considerations

For cutting tool applications, D3's high wear resistance and edge retention make it ideal for blanking and forming operations on hard materials. In die manufacturing, the air-hardening characteristics minimize distortion in complex geometries. For bearing applications, the uniform carbide distribution provides consistent wear patterns and extended service life. In precision machinery, the dimensional stability after heat treatment ensures tight tolerances. For automotive components, the combination of hardness and toughness provides reliable performance under cyclic loading conditions.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)2.00 - 2.35
Chromium (Cr)11.00 - 13.00
Manganese (Mn)0.15 - 0.45
Silicon (Si)0.10 - 0.60
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Vanadium (V)≤ 1.00
Molybdenum (Mo)≤ 1.00

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC)58 - 62
Compressive Strength (MPa)≥ 2800
Impact Toughness (J)15 - 25
Wear Resistance Index8.5 - 9.2
Hardenability (mm)75 - 100
Fatigue Strength (MPa)≥ 850

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.70
Melting Point (°C)1420 - 1460
Thermal Conductivity (W/m·K)20.5
Thermal Expansion (×10??/K)10.8
Elastic Modulus (GPa)210
Poisson's Ratio0.27 - 0.30

📏 Product Specifications

SpecificationDetails
Available FormsRounds, Flats, Squares, Plates, Custom Forgings
Diameter Range10 - 500mm
Thickness Range5 - 200mm
Length Range100 - 6000mm
Standards ComplianceASTM A681, DIN 1.2080, JIS SKD1
Heat Treatment ConditionAnnealed, Hardened & Tempered
Surface FinishHot Rolled, Cold Drawn, Precision Ground

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing D3 Tool Steel

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith utilizes state-of-the-art vacuum induction melting followed by electroslag remelting to achieve superior cleanliness and homogeneous carbide distribution. Our controlled forging process with precise temperature monitoring ensures optimal grain flow and eliminates segregation, resulting in consistent mechanical properties throughout the material cross-section.

Comprehensive Tool Steel Testing

Our specialized testing protocols include Rockwell hardness mapping across the entire cross-section, X-ray diffraction analysis for residual austenite content measurement, metallographic examination of carbide distribution uniformity, and rotating beam fatigue testing. These advanced quality control measures ensure optimal performance in demanding tooling applications.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Heat Treatment Services

MetalZenith offers tailored heat treatment solutions including vacuum hardening, sub-zero treatment, and precision tempering with computer-controlled atmosphere furnaces. Our metallurgical engineers provide technical support for application-specific hardness requirements and dimensional stability optimization, ensuring maximum tool life and performance.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo