CPM S30V

CPM S30V

Premium CPM S30V Tool Steel by MetalZenith

CPM S30V is a premium martensitic stainless steel developed using Crucible Particle Metallurgy (CPM) technology, offering exceptional wear resistance, corrosion resistance, and edge retention. This advanced tool steel is specifically engineered for high-performance applications requiring superior cutting performance and durability.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we utilize state-of-the-art powder metallurgy processes and precision heat treatment facilities to produce CPM S30V with exceptional uniformity and performance consistency. Our advanced vacuum melting technology ensures optimal carbide distribution and eliminates segregation issues common in conventional steelmaking.

Key Applications & Industries

  • Premium knife blades and cutting tools
  • Surgical instruments and medical devices
  • Precision tooling and dies
  • Aerospace components requiring corrosion resistance
  • High-performance industrial cutting applications

Quality Assurance & Certification

MetalZenith maintains ISO 9001:2015 certification and implements comprehensive quality control throughout the production process. Every batch undergoes rigorous chemical analysis, mechanical testing, and microstructural examination to ensure consistent performance and compliance with international standards.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

CPM S30V is a martensitic stainless steel produced through Crucible Particle Metallurgy (CPM) technology, which involves rapid solidification of molten steel into fine powder particles followed by consolidation. This process results in a uniform distribution of fine vanadium carbides throughout the steel matrix, providing exceptional wear resistance and edge retention properties.

Manufacturing Process

MetalZenith employs advanced powder metallurgy techniques including gas atomization, hot isostatic pressing (HIP), and controlled atmosphere processing. The steel undergoes vacuum melting to ensure cleanliness, followed by rapid solidification to achieve fine carbide distribution. Subsequent consolidation processes eliminate porosity and achieve full density.

Heat Treatment Procedures

Annealing: Heat to 870-900°C, hold for 2-4 hours, cool slowly to achieve 255-285 HB hardness. Hardening: Austenitize at 1065-1095°C, quench in oil or air to achieve maximum hardness. Tempering: Temper at 150-540°C depending on desired hardness and toughness balance. Multiple tempering cycles may be employed for stress relief.

Quality Standards & Testing

All CPM S30V products undergo comprehensive quality control including chemical analysis by optical emission spectroscopy, hardness testing per ASTM E18, microstructural examination, and dimensional verification. MetalZenith maintains traceability records for each heat and implements statistical process control to ensure consistent quality. Products comply with international standards and customer-specific requirements.

Corrosion Resistance & Performance

The 14% chromium content provides excellent corrosion resistance in mild environments, while the high vanadium content (4%) forms hard vanadium carbides that contribute to superior wear resistance. The steel exhibits excellent edge retention and can maintain sharpness significantly longer than conventional tool steels, making it ideal for premium cutting applications.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)1.45
Chromium (Cr)14.00
Vanadium (V)4.00
Molybdenum (Mo)2.00
Manganese (Mn)0.50
Silicon (Si)0.50
Phosphorus (P)≤ 0.030
Sulfur (S)≤ 0.030
Nickel (Ni)≤ 0.50
Copper (Cu)≤ 0.25

⚙️ Mechanical Properties

PropertyValue
Hardness (HRC) - As Hardened58-61
Hardness (HRC) - Tempered 200°C59-61
Hardness (HRC) - Tempered 400°C56-58
Tensile Strength2070-2275 MPa
Yield Strength (0.2% offset)1725-1930 MPa
Elongation1.5-2.5%
Reduction of Area3-5%
Impact Strength (Charpy V-notch)15-25 J
Fatigue Limit (107 cycles)900-1100 MPa
Modulus of Elasticity210 GPa

🔬 Physical Properties

PropertyValue
Density7.65 g/cm³
Melting Point1480-1520°C
Thermal Conductivity (20°C)24.3 W/m·K
Thermal Expansion Coefficient (20-100°C)10.4×10-6/K
Thermal Expansion Coefficient (20-200°C)11.2×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.60 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature~450°C
Poisson's Ratio0.27-0.30

📏 Product Specifications

SpecificationAvailable Options
Product FormsRound bars, flat bars, plates, sheets, custom shapes
Round Bar Diameter6mm - 300mm
Flat Bar Dimensions10×20mm - 100×500mm
Plate Thickness5mm - 150mm
Sheet Thickness0.5mm - 5mm
LengthUp to 6000mm (custom lengths available)
Surface FinishAnnealed, hardened & tempered, ground, polished
Dimensional Tolerance±0.1mm to ±0.5mm (depending on size)
Standards ComplianceASTM A681, Custom specifications
Heat Treatment ConditionAnnealed, spheroidized, hardened & tempered

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing CPM S30V

Manufacturing Advantage 1

Advanced Powder Metallurgy Technology

MetalZenith employs cutting-edge Crucible Particle Metallurgy (CPM) processes with precise powder atomization and consolidation techniques, ensuring uniform carbide distribution and eliminating the segregation issues found in conventional cast steels, resulting in superior performance consistency.

Precision Heat Treatment & Quality Control

Our state-of-the-art vacuum heat treatment facilities with computer-controlled atmosphere management deliver precise hardness control and optimal microstructure. Comprehensive testing including chemical analysis, hardness mapping, and microstructural examination ensures every batch meets stringent quality standards.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Processing & Global Supply Chain

MetalZenith offers extensive customization capabilities including precision machining, surface treatments, and specialized heat treatment cycles. Our global distribution network and flexible production scheduling ensure reliable supply chain management with competitive lead times for customers worldwide.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo