Premium 738 Mold Steel from MetalZenith

738 is a premium pre-hardened plastic mold steel that combines excellent machinability with superior surface finish capabilities. This versatile steel grade is specifically engineered for injection molding applications where dimensional stability and consistent performance are critical requirements.

MetalZenith's Advanced Manufacturing Excellence

At MetalZenith, we leverage state-of-the-art vacuum melting technology and precision heat treatment processes to produce 738 steel with exceptional uniformity and cleanliness. Our advanced manufacturing facilities ensure consistent mechanical properties throughout the material, eliminating the risk of dimensional distortion during machining operations.

Key Applications and Industries

  • Plastic injection molds for automotive components
  • Consumer electronics housings and precision parts
  • Medical device manufacturing tooling
  • Optical component molding applications
  • High-precision mechanical components

Quality Assurance and Certification

MetalZenith maintains comprehensive quality control systems including ultrasonic testing, chemical analysis, and mechanical property verification. Our 738 steel meets international standards including ASTM, EN, and JIS specifications, backed by full material traceability and certification documentation for critical applications.

ดูรายละเอียดทั้งหมด

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

738 steel features a tempered martensitic microstructure that provides an optimal balance of strength, toughness, and machinability. The controlled addition of aluminum creates fine precipitates that enhance strength while maintaining excellent dimensional stability during machining operations. The low sulfur content ensures superior surface finish quality and reduces the risk of inclusion-related defects.

Heat Treatment Process

MetalZenith's proprietary heat treatment process involves austenitizing at 850-870°C followed by controlled cooling and tempering at 550-600°C. This process ensures uniform hardness distribution and optimal microstructure development. The pre-hardened condition eliminates the need for post-machining heat treatment, reducing manufacturing time and preventing dimensional distortion.

Manufacturing Process Excellence

Our manufacturing process begins with vacuum induction melting to ensure chemical homogeneity and cleanliness. The steel undergoes electroslag remelting for further purification, followed by controlled forging and rolling operations. Each production lot is subjected to comprehensive testing including ultrasonic inspection, chemical analysis, and mechanical property verification to ensure consistent quality.

Quality Standards and Certifications

MetalZenith's 738 steel production facilities are certified to ISO 9001:2015, ISO 14001:2015, and OHSAS 18001 standards. Our quality management system ensures full traceability from raw materials to finished products, with comprehensive documentation including material certificates, test reports, and dimensional inspection records for every shipment.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)0.35-0.42
Silicon (Si)0.20-0.40
Manganese (Mn)1.35-1.65
Phosphorus (P)≤ 0.025
Sulfur (S)≤ 0.010
Chromium (Cr)0.90-1.20
Nickel (Ni)1.65-2.00
Molybdenum (Mo)0.15-0.25
Aluminum (Al)0.95-1.35

⚙️ Mechanical Properties

PropertyValue
Tensile Strength1030-1180 MPa
Yield Strength (0.2% offset)≥ 930 MPa
Elongation≥ 12%
Reduction of Area≥ 45%
Hardness (Pre-hardened)30-37 HRC
Impact Energy (Charpy V-notch)≥ 25 J
Fatigue Limit (10&sup7; cycles)450 MPa
Young's Modulus210 GPa
Poisson's Ratio0.30

🔬 Physical Properties

PropertyValue
Density7.85 g/cm³
Melting Point1420-1460°C
Thermal Conductivity (20°C)42 W/m·K
Thermal Expansion Coefficient (20-100°C)11.5×10-6/K
Specific Heat Capacity460 J/kg·K
Electrical Resistivity (20°C)0.25 µΩ·m
Magnetic PermeabilityFerromagnetic
Curie Temperature750°C

📏 Product Specifications

SpecificationAvailable Options
Product FormsRound bars, flat bars, plates, blocks, forged pieces
Round Bar Diameter10-500 mm
Flat Bar Thickness10-200 mm
Plate Thickness20-300 mm
LengthUp to 6000 mm
Surface FinishBlack, machined, ground, polished
Dimensional Toleranceh9 to h11 (standard), h6 to h8 (precision)
Standards ComplianceASTM A681, EN ISO 4957, JIS SKD61
ConditionPre-hardened, annealed, normalized

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing 738

Manufacturing Advantage 1

Advanced Vacuum Melting Technology

MetalZenith employs cutting-edge vacuum induction melting and electroslag remelting processes to produce 738 steel with exceptional cleanliness and homogeneity. Our controlled atmosphere melting eliminates inclusions and ensures consistent chemical composition throughout the material, resulting in superior machinability and surface finish quality.

Precision Heat Treatment Control

Our state-of-the-art heat treatment facilities feature computer-controlled furnaces with precise temperature monitoring and atmosphere control. This ensures optimal microstructure development and consistent hardness levels across all 738 steel products, eliminating dimensional distortion and guaranteeing predictable machining characteristics.

Manufacturing Advantage 2
Manufacturing Advantage 3

Comprehensive Customization Capabilities

MetalZenith offers extensive customization options for 738 steel including specific dimensional tolerances, surface finishes, and packaging requirements. Our global supply chain network ensures rapid delivery worldwide, while our technical support team provides expert guidance for optimal material selection and application engineering.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
ติดต่อเรา

สอบถามด่วน

ขั้นต่ำในการสั่งซื้อ: 3 ตัน

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo