JIS SUS430 is a ferritic stainless steel with a body-centered cubic (BCC) crystal structure containing 16-18% chromium. The ferritic microstructure provides excellent corrosion resistance in mildly corrosive environments while maintaining magnetic properties. MetalZenith's controlled chemistry ensures optimal grain structure and carbide distribution for enhanced formability and surface quality.
Heat Treatment Process
MetalZenith employs precise annealing at 815-900°C followed by controlled cooling to achieve optimal mechanical properties. Our continuous annealing lines feature protective atmosphere control to prevent oxidation and ensure consistent surface finish. Stress relief annealing at 400-450°C is available for formed components to restore ductility.
Manufacturing Process
Production begins with electric arc furnace melting followed by AOD refining for precise chemistry control. Hot rolling is performed at 1050-1200°C with controlled cooling rates. Cold rolling utilizes advanced mill technology for superior surface finish and dimensional accuracy. MetalZenith's integrated production line ensures consistent quality from melting to final inspection.
Quality Standards
All JIS SUS430 products undergo rigorous testing including chemical analysis by optical emission spectroscopy, mechanical testing per JIS Z2241, and corrosion resistance evaluation. MetalZenith maintains full traceability with material test certificates (MTC) complying with EN 10204 3.1. Our quality management system ensures consistent performance and reliability for critical applications.
🧪 Chemical Composition
| Element | Composition (%) |
|---|---|
| Carbon (C) | ≤ 0.12 |
| Silicon (Si) | ≤ 0.75 |
| Manganese (Mn) | ≤ 1.00 |
| Phosphorus (P) | ≤ 0.040 |
| Sulfur (S) | ≤ 0.030 |
| Chromium (Cr) | 16.00 - 18.00 |
| Nickel (Ni) | ≤ 0.60 |
| Aluminum (Al) | ≤ 0.15 |
| Nitrogen (N) | ≤ 0.030 |
| Iron (Fe) | Balance |
⚙️ Mechanical Properties
| Property | Value |
|---|---|
| Tensile Strength | 450 - 630 MPa |
| Yield Strength (0.2% offset) | ≥ 205 MPa |
| Elongation (50mm gauge) | ≥ 22% |
| Hardness (Brinell) | ≤ 183 HB |
| Hardness (Rockwell B) | ≤ 88 HRB |
| Impact Energy (Charpy V-notch, 20°C) | ≥ 40 J |
| Fatigue Limit (10&sup7; cycles) | 200 - 250 MPa |
| Young's Modulus | 200 GPa |
| Poisson's Ratio | 0.27 - 0.30 |
🔬 Physical Properties
| Property | Value |
|---|---|
| Density | 7.70 g/cm³ |
| Melting Point | 1425 - 1510°C |
| Thermal Conductivity (20°C) | 26.1 W/m·K |
| Thermal Expansion Coefficient (20-100°C) | 10.4×10-6/K |
| Thermal Expansion Coefficient (20-300°C) | 11.0×10-6/K |
| Specific Heat Capacity | 460 J/kg·K |
| Electrical Resistivity (20°C) | 0.60 µΩ·m |
| Magnetic Permeability | Ferromagnetic |
| Curie Temperature | 770°C |
📏 Product Specifications
| Specification | Available Options |
|---|---|
| Product Forms | Hot rolled sheets, Cold rolled sheets, Plates, Strips, Bars, Wire rods |
| Sheet Thickness | 0.4 - 6.0 mm |
| Plate Thickness | 6.0 - 100 mm |
| Width Range | 1000 - 2000 mm |
| Length Range | 2000 - 6000 mm (or coil) |
| Bar Diameter | 6 - 300 mm |
| Surface Finish | 2B, BA, No.4, HL (Hairline), Mirror finish |
| Standards Compliance | JIS G4305, ASTM A240, EN 10088-2 |
| Dimensional Tolerance | ±0.1mm (thickness), ±3mm (width) |
Let Us Create Success for Your Project
Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission
Our Advantages in Processing JIS SUS430
Advanced Vacuum Melting Technology
MetalZenith employs state-of-the-art vacuum induction melting (VIM) and argon oxygen decarburization (AOD) processes to produce JIS SUS430 with ultra-low inclusion content and superior chemical homogeneity, ensuring consistent mechanical properties and enhanced corrosion resistance.
Comprehensive Quality Control System
Our integrated quality management system features real-time process monitoring, automated testing equipment, and certified laboratories conducting chemical analysis, mechanical testing, and microstructural examination to guarantee compliance with JIS G4305 standards and customer specifications.
Flexible Customization Capabilities
MetalZenith offers extensive customization options including precision cutting, surface finishing, heat treatment, and packaging solutions. Our global supply chain network ensures timely delivery of JIS SUS430 products tailored to specific application requirements worldwide.
YOUR TRUSTED STEEL
MANUFACTURING PARTNER
Quick Inquiry
Industries We Serve
Professional steel solutions across major industries
Qualifications & Certifications