Nitronic 40 Stainless Steel

Nitronic 40 Stainless Steel

Nitronic 40 High-Performance Stainless Steel

Nitronic 40 is a nitrogen-strengthened austenitic stainless steel offering exceptional strength, superior corrosion resistance, and outstanding galling resistance. This advanced alloy combines the corrosion resistance of 316 stainless steel with nearly twice the yield strength, making it ideal for demanding applications in chemical processing, marine environments, and high-stress mechanical components.

MetalZenith's Advanced Manufacturing Excellence

MetalZenith employs precision controlled atmosphere melting and advanced nitrogen injection techniques to produce Nitronic 40 with optimal nitrogen content and microstructural uniformity. Our state-of-the-art solution annealing processes ensure complete austenitic structure formation and maximum corrosion resistance, while maintaining the superior mechanical properties critical for high-performance applications.

Key Applications

  • Chemical processing equipment and reactor vessels
  • Food processing machinery and pharmaceutical equipment
  • Medical implants and surgical instruments
  • Marine hardware and offshore platform components
  • Architectural facades and decorative structural elements

Quality Assurance & Certifications

MetalZenith maintains rigorous quality control including pitting potential testing, intergranular corrosion evaluation, stress corrosion cracking assessment, and passivation film thickness measurement. Our Nitronic 40 meets ASTM A240, ASME specifications, and FDA requirements for food contact applications, ensuring reliability in critical industrial and medical applications.

View full details

20 Years Experience | 1000+ Brand Partners | Full Customization

We have 20 years of industry experience, have partnered with over 1,000 brands, and support any customization needs.

Technical Specifications

Product Overview

Metallurgical Characteristics

Nitronic 40 features a fully austenitic microstructure strengthened by interstitial nitrogen atoms. The nitrogen content of 0.15-0.40% provides solid solution strengthening while maintaining excellent ductility and toughness. The balanced chromium-nickel-manganese composition ensures stable austenite formation and superior corrosion resistance in chloride environments.

Heat Treatment Process

MetalZenith employs solution annealing at 1900-2100°F (1040-1150°C) followed by rapid water quenching to retain maximum nitrogen in solution and prevent carbide precipitation. This process ensures optimal mechanical properties and corrosion resistance while maintaining the fine-grained austenitic structure essential for superior performance.

Advanced Manufacturing Process

Our controlled atmosphere electric arc furnace melting with nitrogen injection ensures precise nitrogen control and minimal inclusion content. Advanced hot rolling with controlled cooling rates optimizes grain structure, while our proprietary surface conditioning processes enhance passivation film formation for maximum corrosion protection.

Specialized Quality Testing

MetalZenith conducts comprehensive testing including pitting potential measurement at +350mV vs SCE minimum, intergranular corrosion testing per ASTM A262 Practice E, stress corrosion cracking evaluation in boiling MgCl2, and passivation film thickness analysis ensuring 2-5nm optimal thickness for maximum protection in aggressive environments.

Application-Specific Considerations

For chemical processing equipment, our material meets NACE MR0175 requirements for sour service. Food industry applications benefit from FDA compliance and enhanced cleanability. Medical device applications utilize our ultra-low inclusion grades with validated biocompatibility. Marine applications leverage superior pitting resistance in seawater, while architectural applications benefit from excellent atmospheric corrosion resistance and aesthetic durability.

🧪 Chemical Composition

ElementComposition (%)
Carbon (C)≤ 0.04
Chromium (Cr)19.0 - 21.5
Nickel (Ni)11.5 - 13.5
Manganese (Mn)8.0 - 10.0
Silicon (Si)≤ 1.0
Nitrogen (N)0.15 - 0.40
Phosphorus (P)≤ 0.04
Sulfur (S)≤ 0.03

⚙️ Mechanical Properties

PropertyValue
Yield Strength (MPa)≥ 380
Tensile Strength (MPa)690 - 930
Elongation (%)≥ 35
Hardness (HRB)95 - 105
Pitting Resistance (PREN)≥ 25
Galling ResistanceExcellent

🔬 Physical Properties

PropertyValue
Density (g/cm3)7.90
Melting Point (°C)1400 - 1450
Thermal Conductivity (W/m·K)14.2
Thermal Expansion (×10??/K)16.0
Electrical Resistivity (μΩ·cm)85
Elastic Modulus (GPa)200

📏 Product Specifications

SpecificationDetails
Available FormsPlates, Sheets, Bars, Rods, Tubes, Forgings
Thickness Range0.5 - 150mm
Width Range1000 - 3000mm
Length Range2000 - 12000mm
Standards ComplianceASTM A240, ASME SA-240, UNS S21900
Surface Finish2B, BA, No.4, No.8, Custom
Heat Treatment ConditionSolution Annealed

Let Us Create Success for Your Project

Professional Team, Premium Products, Complete Service - Your Project Success is Our Mission

Our Advantages in Processing Nitronic 40 Stainless Steel

Manufacturing Advantage 1

Advanced Nitrogen-Enhanced Processing

MetalZenith utilizes precision controlled atmosphere melting with optimized nitrogen injection to achieve uniform nitrogen distribution throughout the austenitic matrix. Our advanced solution annealing process at 1900-2100°F ensures complete carbide dissolution and optimal nitrogen retention for maximum strength and corrosion resistance.

Comprehensive Corrosion Testing Protocol

Our specialized testing laboratory conducts extensive pitting potential measurements (ASTM G150), intergranular corrosion testing (ASTM A262), stress corrosion cracking evaluation (ASTM G123), and passivation film thickness analysis using XPS technology. This ensures superior performance in chloride environments and aggressive chemical media.

Manufacturing Advantage 2
Manufacturing Advantage 3

Custom Fabrication & Technical Support

MetalZenith provides comprehensive custom processing including precision machining, forming, and welding services specifically optimized for Nitronic 40's unique properties. Our metallurgical engineers offer technical consultation for application-specific heat treatment and surface finishing to maximize performance in demanding environments.

YOUR TRUSTED STEEL

MANUFACTURING PARTNER

20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
20
Years Experience
Leading Steel Manufacturing & Distribution
1000+
Brand Partners
Trusted by Global Industry Leaders
Full
Customization
Tailored Solutions for Every Project
50M+
Tons Delivered
High-Quality Steel Products Worldwide
95%
Client Retention
Long-term Partnership Success
ISO 9001
Certified Quality
International Standards Compliance
GET IN TOUCH

Quick Inquiry

Minimum Order Quantity: 3 Tons

Industries We Serve

Professional steel solutions across major industries

Construction

High-rise Buildings • Infrastructure • Commercial Real Estate

Oil & Gas

Pipeline Systems • Storage Equipment • Refinery Facilities

Manufacturing

Precision Machinery • Industrial Equipment • Automation Systems

Automotive

Body Structure • Chassis Components • Engine Parts

Shipbuilding

Hull Structure • Marine Engineering • Port Equipment

Energy & Power

Power Generation • Transmission Towers • Renewable Energy

Aerospace

Aircraft Materials • Precision Components • Special Alloys

Railway

Track Systems • Vehicle Manufacturing • Infrastructure

Qualifications & Certifications

Client logo
Client logo
Client logo
Client logo
Client logo