Steel Rebar Weight Calculator

Calculate reinforcing bar weight by metric diameter or US bar number. Enter the bar size, the length and how many bars, and get the total tonnage for your order or bar schedule.

Rebar weight W = πd²/4 × L × ρ
Weight
—

Nominal weight from dimensions and density. Actual weight varies with mill tolerance and coating — check the mill certificate for critical use.

Rebar unit weights

Metric kg/m US bar Nominal dia lb/ft
6 mm 0.222 #3 9.5 mm 0.374
8 mm 0.395 #4 12.7 mm 0.668
10 mm 0.617 #5 15.9 mm 1.047
12 mm 0.888 #6 19.1 mm 1.511
14 mm 1.208 #7 22.2 mm 2.042
16 mm 1.578 #8 25.4 mm 2.673
18 mm 1.998 #9 28.7 mm 3.412
20 mm 2.466 #10 32.3 mm 4.322
22 mm 2.984 #11 35.8 mm 5.309
25 mm 3.853 #14 43.0 mm 7.660
28 mm 4.834 #18 57.3 mm 13.602

US bar numbers give the diameter in eighths of an inch — a #5 bar is 5/8 inch (about 15.9 mm). The unit weight formula is the same as round bar: kg/m = d² × 0.006165.

Frequently asked questions

How do you calculate rebar weight?

Multiply the bar's unit weight by its length and the number of bars. Unit weight in kg/m equals diameter in mm squared times 0.006165.

What does rebar size #4 mean?

US bar numbers give the nominal diameter in eighths of an inch, so #4 is 4/8 = 1/2 inch, about 12.7 mm.

How much does 12 mm rebar weigh?

About 0.888 kg per metre. A 12 m length weighs roughly 10.7 kg.

Related tools: Universal Metal Weight · Gauge Chart · Plate · Bar · Tube · Angle · All calculators

Steel Rebar Weight Calculator

Calculate the weight of steel rebars based on diameter, length and material type.

Weight per rebar: 0 kg
Total weight: 0 kg
Cross-sectional area: 0 mm²
Volume per rebar: 0 cm³
Total length: 0 m

How to use this calculator:

  1. Select the rebar diameter from standard sizes (in mm)
  2. Enter the length of the rebar in meters or feet
  3. Select the material type from the dropdown menu
  4. Enter the quantity of rebars (default is 1)
  5. Click "Calculate Weight" to get the results

This calculator provides the weight of steel rebars based on their dimensions and material density. Results are shown in kilograms (kg).

Standard Rebar Sizes Reference

Metric Size (mm) US Size Cross Section (mm²) Weight (kg/m)
6 mm #2 28.3 0.222
10 mm #3 78.5 0.616
12 mm #4 113.1 0.888
16 mm #5 201.1 1.579
20 mm #6 314.2 2.466
25 mm #8 490.9 3.853
32 mm #10 804.2 6.313
40 mm - 1256.6 9.864