SPHC Steel: Properties and Key Applications Overview

Table Of Content

Table Of Content

SPHC steel, classified as hot-rolled commercial quality steel, is primarily a low-carbon mild steel. It is characterized by its excellent formability and weldability, making it a popular choice in various engineering applications. The primary alloying element in SPHC steel is carbon, typically present in low concentrations, which contributes to its ductility and malleability. Other elements may include manganese and phosphorus, which can influence its mechanical properties and overall performance.

Comprehensive Overview

SPHC steel is widely used in the manufacturing of products that require good weldability and formability. Its low carbon content typically ranges from 0.05% to 0.15%, which allows for easy shaping and forming processes. The steel is produced through hot rolling, a process that involves heating the steel above its recrystallization temperature and then deforming it into the desired shape. This method not only enhances the steel's mechanical properties but also improves its surface finish.

Key Characteristics:
- Ductility: SPHC steel exhibits high ductility, allowing it to be easily formed into complex shapes without cracking.
- Weldability: The low carbon content ensures that SPHC steel can be welded using various techniques without significant risk of cracking.
- Surface Finish: The hot-rolled process provides a rough surface finish, which may require additional treatment for aesthetic applications.

Advantages:
- Excellent formability and weldability make it suitable for a wide range of applications.
- Cost-effective due to its low carbon content and the simplicity of the manufacturing process.
- Good mechanical properties for general structural applications.

Limitations:
- Lower strength compared to higher carbon steels or alloy steels, which may limit its use in high-stress applications.
- Susceptibility to corrosion if not properly treated or coated.

SPHC steel holds a significant position in the market due to its versatility and cost-effectiveness, making it a staple in industries such as automotive, construction, and manufacturing.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS G10100 USA Closest equivalent to SPHC
AISI/SAE 1010 USA Minor compositional differences
ASTM A569 USA Hot-rolled steel specification
EN S235JR Europe Similar mechanical properties
JIS SPHC Japan Direct designation for hot-rolled steel
ISO 6301 International General standard for hot-rolled steel

The table above outlines various standards and equivalents for SPHC steel. While these grades may be considered equivalent, subtle differences in composition and processing can affect performance. For instance, while AISI 1010 and SPHC share similar carbon content, their mechanical properties may vary due to differences in manufacturing processes and heat treatment.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
C (Carbon) 0.05 - 0.15
Mn (Manganese) 0.30 - 0.60
P (Phosphorus) ≤ 0.04
S (Sulfur) ≤ 0.05

The primary alloying element in SPHC steel is carbon, which plays a crucial role in determining the steel's hardness and strength. Manganese enhances the steel's toughness and improves its hardenability, while phosphorus and sulfur are controlled to minimize their detrimental effects on ductility and weldability.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Hot-Rolled 270 - 410 MPa 39 - 60 ksi ASTM E8
Yield Strength (0.2% offset) Hot-Rolled 235 - 300 MPa 34 - 44 ksi ASTM E8
Elongation Hot-Rolled 20 - 30% 20 - 30% ASTM E8
Hardness (Brinell) Hot-Rolled 120 - 160 HB 120 - 160 HB ASTM E10
Impact Strength Hot-Rolled 27 J at -20°C 20 ft-lbf at -4°F ASTM E23

The mechanical properties of SPHC steel make it suitable for applications requiring moderate strength and good ductility. Its tensile and yield strengths are adequate for structural applications, while its elongation indicates good formability. The hardness values suggest that while it can withstand some wear, it is not intended for high-abrasion environments.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temperature 7.85 g/cm³ 0.284 lb/in³
Melting Point - 1425 - 1540 °C 2600 - 2800 °F
Thermal Conductivity Room Temperature 50 W/m·K 29 BTU·in/h·ft²·°F
Specific Heat Capacity Room Temperature 0.48 kJ/kg·K 0.11 BTU/lb·°F

The density of SPHC steel is typical for mild steels, providing a good balance between weight and strength. Its melting point indicates that it can withstand high temperatures during processing. The thermal conductivity is essential for applications where heat dissipation is critical, while the specific heat capacity affects how the material responds to temperature changes.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C) Resistance Rating Notes
Atmospheric Varies Ambient Fair Susceptible to rust
Chlorides Varies Ambient Poor Risk of pitting
Acids Varies Ambient Poor Not recommended
Alkalis Varies Ambient Fair Moderate resistance

SPHC steel exhibits moderate resistance to corrosion, particularly in atmospheric conditions. However, it is susceptible to rusting if not properly protected, especially in environments with high humidity or exposure to chlorides. In acidic or alkaline environments, SPHC steel is not recommended due to the risk of significant corrosion.

When compared to other grades, such as S235JR or A36, SPHC steel may show similar corrosion resistance; however, the choice of protective coatings and surface treatments can significantly enhance its performance in corrosive environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 400 °C 752 °F Suitable for moderate temperatures
Max Intermittent Service Temp 500 °C 932 °F Short-term exposure only
Scaling Temperature 600 °C 1112 °F Risk of oxidation beyond this temp

SPHC steel can withstand moderate temperatures, making it suitable for applications that do not involve extreme heat. However, at temperatures above 400 °C, the risk of oxidation increases, which can affect its mechanical properties. Users should consider the thermal environment of their applications when selecting SPHC steel.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon + CO2 Good for thin sections
TIG ER70S-2 Argon Clean welds, low heat input
Stick E7018 None Suitable for outdoor work

SPHC steel is highly weldable, making it suitable for various welding processes. The recommended filler metals ensure compatibility and strength in the weld joint. Pre-heating may be necessary for thicker sections to avoid cracking.

Machinability

Machining Parameter SPHC Steel AISI 1212 Notes/Tips
Relative Machinability Index 60% 100% SPHC is less machinable than 1212
Typical Cutting Speed (Turning) 30 m/min 50 m/min Adjust for tool wear

SPHC steel has moderate machinability, which can be improved with proper tooling and cutting conditions. It is less machinable than higher alloy steels, requiring slower cutting speeds and careful tool selection.

Formability

SPHC steel exhibits excellent formability, allowing for cold and hot forming processes. It can be easily bent, stamped, or drawn into complex shapes without cracking. The work hardening effect is minimal due to its low carbon content, making it suitable for applications requiring intricate designs.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 600 - 700 °C / 1112 - 1292 °F 1 - 2 hours Air Improve ductility and reduce hardness
Normalizing 850 - 900 °C / 1562 - 1652 °F 1 - 2 hours Air Refine grain structure
Quenching 800 - 900 °C / 1472 - 1652 °F 1 hour Water/Oil Increase hardness

Heat treatment processes such as annealing and normalizing can significantly alter the microstructure of SPHC steel, enhancing its mechanical properties. Annealing reduces hardness and increases ductility, while normalizing refines the grain structure, improving strength and toughness.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Automotive Body panels Good formability, weldability Lightweight and cost-effective
Construction Structural beams Adequate strength, ease of fabrication Versatile and readily available
Manufacturing Machinery parts Ductility, machinability Suitable for complex shapes

SPHC steel is commonly used in the automotive industry for body panels due to its excellent formability and weldability. In construction, it serves as structural beams where moderate strength is required. Its versatility makes it a preferred choice in manufacturing for various machinery parts.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property SPHC Steel A36 Steel S235JR Steel Brief Pro/Con or Trade-off Note
Key Mechanical Property Moderate Moderate Moderate Similar strength profiles
Key Corrosion Aspect Fair Fair Fair All are susceptible to rust
Weldability Excellent Good Good SPHC offers better weldability
Machinability Moderate Good Good A36 and S235JR are easier to machine
Formability Excellent Good Good SPHC excels in forming processes
Approx. Relative Cost Low Low Low Cost-effective options
Typical Availability High High High Widely available in the market

When selecting SPHC steel, considerations include its cost-effectiveness, availability, and suitability for specific applications. While it offers excellent formability and weldability, its lower strength compared to higher carbon or alloy steels may limit its use in high-stress applications. Additionally, users should consider the potential for corrosion and the need for protective coatings in certain environments.

In summary, SPHC steel is a versatile material that balances cost, formability, and weldability, making it suitable for a wide range of applications across various industries. Its properties and performance characteristics should be carefully evaluated against specific project requirements to ensure optimal selection.

Back to blog