GM190 Cast Steel: Properties and Key Applications

Table Of Content

Table Of Content

GM190 Cast Steel is a specific grade of cast steel known for its unique properties and applications in various engineering fields. Classified as a medium-carbon alloy steel, GM190 typically contains a balanced mix of carbon, manganese, and silicon, which contribute to its mechanical strength and durability. The primary alloying elements in GM190 include:

  • Carbon (C): Enhances hardness and strength.
  • Manganese (Mn): Improves hardenability and tensile strength.
  • Silicon (Si): Increases strength and resistance to oxidation.

Comprehensive Overview

GM190 Cast Steel is recognized for its excellent mechanical properties, making it suitable for a wide range of applications, particularly in the automotive and machinery sectors. Its notable characteristics include good weldability, high strength, and resistance to wear, which are essential for components subjected to mechanical stress.

The advantages of GM190 include:

  • High Strength: Suitable for load-bearing applications.
  • Good Weldability: Can be easily welded using standard techniques.
  • Wear Resistance: Ideal for components that experience friction.

However, GM190 also has limitations:

  • Corrosion Resistance: Not as resistant to corrosion as stainless steels.
  • Brittleness: Can become brittle if not properly heat-treated.

Historically, GM190 has been used in various applications, including structural components, automotive parts, and machinery, due to its favorable balance of strength and ductility.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS G19000 USA Closest equivalent to ASTM A216 WCB
ASTM A216 WCB USA Commonly used for castings
EN 1.0619 Europe Minor compositional differences
DIN 1.0619 Germany Similar properties to GM190
JIS G3106 SM490 Japan Comparable in strength

The equivalent grades listed above may have subtle differences in composition and properties that can affect performance in specific applications. For instance, while ASTM A216 WCB is similar in strength, it may not perform as well in high-temperature applications compared to GM190.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
C (Carbon) 0.20 - 0.25
Mn (Manganese) 0.60 - 0.90
Si (Silicon) 0.15 - 0.40
P (Phosphorus) ≤ 0.035
S (Sulfur) ≤ 0.035

The primary role of key alloying elements in GM190 includes:

  • Carbon: Increases hardness and strength, essential for load-bearing applications.
  • Manganese: Enhances hardenability, allowing for better performance under stress.
  • Silicon: Improves oxidation resistance, contributing to the steel's durability.

Mechanical Properties

Property Condition/Temper Test Temperature Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Annealed Room Temp 370 - 490 MPa 54 - 71 ksi ASTM E8
Yield Strength (0.2% offset) Annealed Room Temp 220 - 300 MPa 32 - 44 ksi ASTM E8
Elongation Annealed Room Temp 20 - 25% 20 - 25% ASTM E8
Hardness (Brinell) Annealed Room Temp 150 - 200 HB 150 - 200 HB ASTM E10
Impact Strength Charpy, -20°C -20°C 27 - 35 J 20 - 26 ft-lbf ASTM E23

The combination of these mechanical properties makes GM190 suitable for applications requiring high strength and toughness, such as structural components and machinery parts.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temp 7.85 g/cm³ 0.284 lb/in³
Melting Point - 1425 - 1540 °C 2600 - 2800 °F
Thermal Conductivity Room Temp 50 W/m·K 34.5 BTU·in/(hr·ft²·°F)
Specific Heat Capacity Room Temp 0.46 kJ/kg·K 0.11 BTU/lb·°F
Electrical Resistivity Room Temp 0.0000017 Ω·m 0.0000017 Ω·in

Key physical properties such as density and melting point are significant for applications where weight and thermal management are critical. The density provides insights into the material's weight, while the melting point indicates its suitability for high-temperature applications.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C) Resistance Rating Notes
Chlorides 3-5 25-60 Fair Risk of pitting corrosion
Sulfuric Acid 10-20 25-50 Poor Not recommended
Atmospheric - - Good Moderate resistance

GM190 exhibits moderate corrosion resistance, particularly in atmospheric conditions. However, it is susceptible to pitting corrosion in chloride environments and should be avoided in acidic conditions. Compared to stainless steels, GM190's corrosion resistance is limited, making it less suitable for marine or highly corrosive environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 400 °C 752 °F Suitable for moderate temperatures
Max Intermittent Service Temp 500 °C 932 °F Short-term exposure only
Scaling Temperature 600 °C 1112 °F Risk of oxidation beyond this limit

At elevated temperatures, GM190 maintains its strength but may experience oxidation. Care should be taken to avoid prolonged exposure to temperatures above 400 °C to prevent degradation of mechanical properties.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon/CO2 Good for thin sections
TIG ER70S-2 Argon Excellent for precision
Stick E7018 - Requires preheat

GM190 is generally considered to have good weldability. Preheating may be necessary to avoid cracking, especially in thicker sections. Post-weld heat treatment can enhance the mechanical properties of the weld.

Machinability

Machining Parameter GM190 AISI 1212 Notes/Tips
Relative Machinability Index 60% 100% Moderate machinability
Typical Cutting Speed (Turning) 30 m/min 50 m/min Use carbide tools for best results

GM190 has moderate machinability, which can be improved with proper tooling and cutting conditions. It is advisable to use high-speed steel or carbide tools for machining operations.

Formability

GM190 can be formed using both cold and hot processes. Cold forming is feasible but may lead to work hardening, which can affect ductility. Hot forming is preferred for complex shapes to avoid cracking and improve formability.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 600 - 700 °C / 1112 - 1292 °F 1 - 2 hours Air Reduce hardness, improve ductility
Quenching 850 - 900 °C / 1562 - 1652 °F 30 minutes Oil/Water Increase hardness
Tempering 400 - 600 °C / 752 - 1112 °F 1 hour Air Reduce brittleness, increase toughness

Heat treatment processes significantly affect the microstructure of GM190, enhancing its mechanical properties. Quenching increases hardness, while tempering reduces brittleness, making it suitable for various applications.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection
Automotive Engine Blocks High strength, good machinability Load-bearing capacity
Machinery Gearboxes Wear resistance, toughness Durability under stress
Construction Structural Components Strength, weldability Ease of fabrication

Other applications include:

  • Pipelines
  • Heavy machinery parts
  • Railway components

GM190 is chosen for these applications due to its balance of strength, ductility, and ease of fabrication, making it ideal for components that require high performance under mechanical stress.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property GM190 AISI 4140 AISI 1045 Brief Pro/Con or Trade-off Note
Key Mechanical Property Moderate High Moderate GM190 is less strong than 4140 but easier to weld.
Key Corrosion Aspect Fair Good Fair GM190 is less resistant to corrosion than 4140.
Weldability Good Fair Good GM190 is easier to weld than 4140.
Machinability Moderate Good Good GM190 is less machinable than 1045.
Formability Good Moderate Good GM190 can be formed easily compared to 4140.
Approx. Relative Cost Moderate Higher Lower GM190 is cost-effective for many applications.
Typical Availability Common Less common Common GM190 is widely available in the market.

When selecting GM190, consider factors such as cost-effectiveness, availability, and the specific mechanical properties required for the application. While it may not offer the same strength as some alloy steels, its weldability and machinability make it a preferred choice for many engineering applications. Additionally, its moderate corrosion resistance makes it suitable for environments where exposure to corrosive agents is limited.

In summary, GM190 Cast Steel is a versatile material that balances strength, ductility, and ease of fabrication, making it a valuable choice in various industrial applications.

Back to blog