Carbon Tool Steel: Properties and Key Applications

Table Of Content

Table Of Content

Carbon tool steel is a category of steel that is primarily composed of carbon and is used for manufacturing tools and dies. It is classified as a high-carbon steel, typically containing between 0.5% to 1.5% carbon, which significantly enhances its hardness and wear resistance. The primary alloying element in carbon tool steel is carbon itself, which plays a crucial role in determining the steel's hardness, strength, and overall performance.

Comprehensive Overview

Carbon tool steels are known for their excellent hardness and ability to maintain a sharp edge, making them ideal for cutting tools, dies, and other applications where wear resistance is critical. The high carbon content contributes to the formation of hard microstructures, such as martensite, when subjected to heat treatment processes like quenching and tempering.

Advantages:
- High Hardness: Carbon tool steels can achieve high hardness levels, making them suitable for cutting and shaping tools.
- Wear Resistance: The wear resistance of these steels is superior, allowing them to withstand abrasive conditions.
- Cost-Effectiveness: Generally, carbon tool steels are more economical compared to alloy tool steels, making them a popular choice for many applications.

Limitations:
- Brittleness: High carbon content can lead to brittleness, making the steel susceptible to cracking under impact.
- Limited Toughness: Compared to other tool steels, carbon tool steels may exhibit lower toughness, which can be a disadvantage in certain applications.
- Corrosion Susceptibility: Carbon tool steels are prone to rusting if not properly maintained, as they lack alloying elements that enhance corrosion resistance.

Historically, carbon tool steels have been significant in the development of industrial tools and machinery, with applications ranging from hand tools to complex machinery components. Their market position remains strong due to their balance of performance and cost.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS T1 USA High-speed tool steel, similar properties
AISI/SAE AISI D2 USA High carbon, high chromium tool steel
ASTM A681 USA Specification for tool steels
EN 1.2379 Europe Equivalent to AISI D2, high wear resistance
JIS SKD11 Japan Similar to D2, with minor compositional differences
DIN X153CrMoV12 Germany High carbon tool steel with chromium and molybdenum

The differences between equivalent grades can be subtle but impactful. For example, while AISI D2 and JIS SKD11 are often considered equivalent, SKD11 may have slightly different toughness and wear resistance characteristics due to its specific alloying elements.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
C (Carbon) 0.5 - 1.5
Mn (Manganese) 0.3 - 0.9
Si (Silicon) 0.1 - 0.4
Cr (Chromium) 0.5 - 1.5
Mo (Molybdenum) 0.1 - 0.5
P (Phosphorus) ≤ 0.03
S (Sulfur) ≤ 0.03

The primary role of carbon in carbon tool steel is to enhance hardness and strength through the formation of hard microstructures during heat treatment. Manganese improves hardenability and toughness, while chromium and molybdenum contribute to wear resistance and stability at elevated temperatures.

Mechanical Properties

Property Condition/Temper Test Temperature Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Quenched & Tempered Room Temp 700 - 900 MPa 101.5 - 130 ksi ASTM E8
Yield Strength (0.2% offset) Quenched & Tempered Room Temp 600 - 800 MPa 87 - 116 ksi ASTM E8
Elongation Quenched & Tempered Room Temp 5 - 10% 5 - 10% ASTM E8
Hardness (HRC) Quenched & Tempered Room Temp 58 - 65 HRC 58 - 65 HRC ASTM E18
Impact Strength (Charpy) Quenched & Tempered -20°C 20 - 30 J 14.8 - 22.1 ft-lbf ASTM E23

The combination of high tensile and yield strength, along with significant hardness, makes carbon tool steel suitable for applications involving high mechanical loads and wear, such as cutting tools and dies. However, the lower elongation values indicate a tendency toward brittleness, which must be considered in design.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temp 7.85 g/cm³ 0.284 lb/in³
Melting Point/Range - 1425 - 1540 °C 2600 - 2800 °F
Thermal Conductivity Room Temp 45 W/m·K 31.2 BTU·in/h·ft²·°F
Specific Heat Capacity Room Temp 0.46 kJ/kg·K 0.11 BTU/lb·°F
Electrical Resistivity Room Temp 0.0006 Ω·m 0.0004 Ω·in

The density of carbon tool steel indicates a robust material, while its melting point suggests good thermal stability. The thermal conductivity is moderate, which is beneficial for heat dissipation in cutting applications. The specific heat capacity is relatively low, indicating that it heats up quickly, which can be advantageous in machining processes.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C) Resistance Rating Notes
Water 0 - 100 20 Poor Prone to rusting without protection
Acids (HCl) 0 - 10 20 Poor Susceptible to pitting corrosion
Alkalis 0 - 10 20 Fair Limited resistance, requires coatings
Chlorides 0 - 5 20 Poor Risk of stress corrosion cracking

Carbon tool steel exhibits poor corrosion resistance, particularly in humid environments or when exposed to acidic or chlorinated conditions. This susceptibility necessitates protective coatings or regular maintenance to prevent rusting. Compared to stainless steels, such as AISI 304, which offer excellent corrosion resistance, carbon tool steels are less suitable for applications where exposure to corrosive environments is expected.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 200 392 Beyond this, properties degrade
Max Intermittent Service Temp 300 572 Short-term exposure only
Scaling Temperature 500 932 Risk of oxidation beyond this

At elevated temperatures, carbon tool steel can lose hardness and strength, making it unsuitable for high-temperature applications without proper heat treatment. Oxidation can occur at temperatures above 500 °C, leading to surface degradation.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon + CO2 Preheat recommended
TIG ER70S-2 Argon Requires post-weld heat treatment
Stick E7018 N/A Not ideal for thick sections

Carbon tool steels can be welded, but care must be taken to avoid cracking. Preheating before welding and post-weld heat treatment are often necessary to relieve stresses and improve toughness.

Machinability

Machining Parameter Carbon Tool Steel AISI 1212 Notes/Tips
Relative Machinability Index 70 100 Carbon tool steel is less machinable than 1212
Typical Cutting Speed (Turning) 30 m/min 50 m/min Adjust based on tool wear

Machinability is moderate; while carbon tool steels can be machined, they require careful selection of cutting tools and parameters to avoid excessive wear.

Formability

Carbon tool steels are generally not as formable as lower carbon steels. Cold forming can lead to work hardening, while hot forming is more feasible but requires careful temperature control to avoid brittleness.

Heat Treatment

Treatment Process Temperature Range (°C) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 700 - 800 1 - 2 hours Air Softening, improving machinability
Quenching 800 - 900 30 minutes Oil or Water Hardening, forming martensite
Tempering 150 - 300 1 hour Air Reducing brittleness, increasing toughness

Heat treatment processes significantly affect the microstructure and properties of carbon tool steel. Quenching transforms the steel into a hard martensitic structure, while tempering reduces brittleness and enhances toughness.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection
Manufacturing Cutting tools High hardness, wear resistance Essential for cutting performance
Automotive Dies for stamping Toughness, strength Required for high-stress applications
Aerospace Tooling for machining Hardness, dimensional stability Precision and durability are critical

Other applications include:
* Hand tools (chisels, hammers)
* Molds for plastic injection
* Jigs and fixtures in manufacturing

Carbon tool steel is chosen for these applications due to its ability to maintain sharp edges and withstand wear, making it ideal for tools and dies.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property Carbon Tool Steel AISI D2 AISI 4140 Brief Pro/Con or Trade-off Note
Key Mechanical Property High hardness Higher wear resistance Better toughness D2 offers better wear resistance but is more expensive
Key Corrosion Aspect Poor Fair Good 4140 is more suitable for corrosive environments
Weldability Moderate Poor Good 4140 can be welded more easily
Machinability Moderate Good Fair D2 is harder to machine than carbon tool steel
Approx. Relative Cost Low Moderate Moderate Carbon tool steel is cost-effective for many applications
Typical Availability High Moderate High Carbon tool steel is widely available

When selecting carbon tool steel, considerations include cost-effectiveness, availability, and the specific mechanical properties required for the application. While it offers excellent hardness and wear resistance, its limitations in toughness and corrosion resistance must be evaluated against the demands of the intended use.

Back to blog

Leave a comment