9 Nickel Steel, also known as 9Ni steel, is a specialized alloy steel primarily classified as a low-alloy steel. It contains approximately 9% nickel as its primary alloying element, which significantly enhances its toughness and cryogenic properties. This steel grade is particularly notable for its ability to maintain strength and ductility at low temperatures, making it an ideal choice for applications in extreme environments, such as cryogenic storage and transport of liquefied gases.
Comprehensive Overview
The primary alloying element in 9 Nickel Steel is nickel, which contributes to its excellent low-temperature toughness and resistance to brittle fracture. The addition of nickel also improves the steel's overall corrosion resistance and weldability. Other elements, such as manganese, silicon, and carbon, are present in smaller amounts, further refining the steel's properties.
Key Characteristics:
- Low-Temperature Performance: 9Ni steel exhibits remarkable toughness at temperatures as low as -196°C (-321°F), making it suitable for cryogenic applications.
- Weldability: The steel can be welded using standard techniques, which is essential for constructing large structures or vessels.
- Corrosion Resistance: While not as corrosion-resistant as stainless steels, 9Ni steel performs adequately in many environments, particularly when properly treated.
Advantages:
- Exceptional toughness at cryogenic temperatures.
- Good weldability and formability.
- Suitable for various applications in the energy sector, particularly in LNG (liquefied natural gas) facilities.
Limitations:
- Limited availability compared to more common steel grades.
- Higher cost due to the nickel content.
- Requires careful handling and processing to avoid issues like hydrogen embrittlement during welding.
Historically, 9 Nickel Steel has played a crucial role in the development of cryogenic technology, particularly in the aerospace and energy industries, where it has been used in the construction of storage tanks and pipelines for liquefied gases.
Alternative Names, Standards, and Equivalents
| Standard Organization | Designation/Grade | Country/Region of Origin | Notes/Remarks |
|---|---|---|---|
| UNS | N08904 | USA | Closest equivalent to 9Ni steel with minor compositional differences. |
| ASTM | A353 | USA | Specification for nickel alloy steel plates for low-temperature service. |
| EN | 1.6368 | Europe | Equivalent grade with similar properties. |
| JIS | G3115 | Japan | Used for pressure vessels, similar toughness characteristics. |
The table above highlights various standards and equivalents for 9 Nickel Steel. Notably, while grades like UNS N08904 and ASTM A353 are often considered equivalents, they may have slight variations in composition that can affect performance in specific applications, particularly in cryogenic environments.
Key Properties
Chemical Composition
| Element (Symbol and Name) | Percentage Range (%) |
|---|---|
| C (Carbon) | 0.05 - 0.15 |
| Mn (Manganese) | 0.30 - 0.60 |
| Si (Silicon) | 0.15 - 0.40 |
| Ni (Nickel) | 8.0 - 10.0 |
| Cr (Chromium) | 0.25 - 0.50 |
| Mo (Molybdenum) | 0.10 - 0.30 |
| P (Phosphorus) | ≤ 0.020 |
| S (Sulfur) | ≤ 0.010 |
The primary role of nickel in 9 Nickel Steel is to enhance toughness and ductility, especially at low temperatures. Manganese contributes to hardenability and strength, while silicon improves deoxidation during steelmaking. Chromium and molybdenum provide additional strength and corrosion resistance.
Mechanical Properties
| Property | Condition/Temper | Test Temperature | Typical Value/Range (Metric) | Typical Value/Range (Imperial) | Reference Standard for Test Method |
|---|---|---|---|---|---|
| Tensile Strength | Annealed | Room Temp | 620 - 690 MPa | 90 - 100 ksi | ASTM E8 |
| Yield Strength (0.2% offset) | Annealed | Room Temp | 350 - 450 MPa | 50 - 65 ksi | ASTM E8 |
| Elongation | Annealed | Room Temp | 20 - 30% | 20 - 30% | ASTM E8 |
| Hardness (Rockwell B) | Annealed | Room Temp | 80 - 90 HRB | 80 - 90 HRB | ASTM E18 |
| Impact Strength | Charpy V-notch | -196°C | 40 - 60 J | 30 - 45 ft-lbf | ASTM E23 |
The mechanical properties of 9 Nickel Steel make it particularly suitable for applications that require high strength and toughness under mechanical loading. Its ability to withstand significant stress without failure is crucial in structural applications, especially in cryogenic environments where materials are subjected to extreme conditions.
Physical Properties
| Property | Condition/Temperature | Value (Metric) | Value (Imperial) |
|---|---|---|---|
| Density | Room Temp | 8.0 g/cm³ | 0.289 lb/in³ |
| Melting Point | - | 1450 - 1500 °C | 2642 - 2732 °F |
| Thermal Conductivity | Room Temp | 30 W/m·K | 20.9 BTU·in/h·ft²·°F |
| Specific Heat Capacity | Room Temp | 0.46 kJ/kg·K | 0.11 BTU/lb·°F |
| Electrical Resistivity | Room Temp | 0.7 µΩ·m | 0.7 µΩ·in |
The density and melting point of 9 Nickel Steel indicate its robustness, while its thermal conductivity and specific heat capacity are important for applications involving temperature fluctuations. The electrical resistivity is relatively low, which can be advantageous in certain applications where electrical conductivity is a factor.
Corrosion Resistance
| Corrosive Agent | Concentration (%) | Temperature (°C) | Resistance Rating | Notes |
|---|---|---|---|---|
| Chlorides | 3 - 10 | 20 - 60 | Fair | Risk of pitting corrosion. |
| Sulfuric Acid | 10 - 20 | 25 - 50 | Poor | Not recommended for high concentrations. |
| Sea Water | - | 25 - 50 | Good | Adequate resistance with proper treatment. |
9 Nickel Steel exhibits moderate corrosion resistance, particularly in chloride environments, where it can be susceptible to pitting. In sulfuric acid, it shows poor resistance, making it unsuitable for applications involving strong acids. Compared to stainless steels, 9Ni steel is less resistant to corrosive environments, but its toughness at low temperatures often outweighs this limitation in specific applications.
Heat Resistance
| Property/Limit | Temperature (°C) | Temperature (°F) | Remarks |
|---|---|---|---|
| Max Continuous Service Temp | 300 °C | 572 °F | Suitable for prolonged exposure. |
| Max Intermittent Service Temp | 400 °C | 752 °F | Short-term exposure limits. |
| Scaling Temperature | 600 °C | 1112 °F | Risk of oxidation beyond this point. |
At elevated temperatures, 9 Nickel Steel maintains its mechanical properties, but prolonged exposure above 300 °C can lead to scaling and oxidation. It is essential to consider these limits in applications involving high-temperature environments.
Fabrication Properties
Weldability
| Welding Process | Recommended Filler Metal (AWS Classification) | Typical Shielding Gas/Flux | Notes |
|---|---|---|---|
| SMAW | E7018 | Argon/CO2 | Preheat recommended. |
| GMAW | ER80S-Ni | Argon | Good for thin sections. |
| GTAW | ERNi-1 | Argon | Excellent for critical applications. |
9 Nickel Steel is generally considered weldable using standard processes. Preheating is often recommended to minimize the risk of cracking. Post-weld heat treatment can further enhance the properties of the weld.
Machinability
| Machining Parameter | 9 Nickel Steel | AISI 1212 | Notes/Tips |
|---|---|---|---|
| Relative Machinability Index | 60% | 100% | Requires slower cutting speeds. |
| Typical Cutting Speed | 30 m/min | 50 m/min | Use carbide tools for best results. |
Machining 9 Nickel Steel can be challenging due to its toughness. It is advisable to use slower cutting speeds and high-quality tooling to achieve optimal results.
Formability
9 Nickel Steel exhibits good formability, allowing for cold and hot forming processes. However, care must be taken to avoid excessive work hardening, which can lead to cracking. The minimum bend radius should be considered during fabrication to ensure structural integrity.
Heat Treatment
| Treatment Process | Temperature Range (°C/°F) | Typical Soaking Time | Cooling Method | Primary Purpose / Expected Result |
|---|---|---|---|---|
| Annealing | 600 - 700 °C / 1112 - 1292 °F | 1 - 2 hours | Air | Relieve stresses, improve ductility. |
| Normalizing | 800 - 900 °C / 1472 - 1652 °F | 1 - 2 hours | Air | Refine grain structure. |
| Quenching | 900 - 1000 °C / 1652 - 1832 °F | 30 min - 1 hour | Oil/Water | Increase hardness. |
Heat treatment processes such as annealing and normalizing are crucial for optimizing the microstructure of 9 Nickel Steel, enhancing its mechanical properties and ensuring uniformity throughout the material.
Typical Applications and End Uses
| Industry/Sector | Specific Application Example | Key Steel Properties Utilized in this Application | Reason for Selection (Brief) |
|---|---|---|---|
| Aerospace | Cryogenic fuel tanks | Low-temperature toughness, weldability | Essential for safety and performance. |
| Energy | LNG pipelines | High strength, corrosion resistance | Critical for transporting liquefied gases. |
| Chemical | Pressure vessels | Toughness, formability | Required for high-pressure applications. |
Other applications include:
- Storage tanks for liquefied gases.
- Components in cryogenic systems.
- Structural elements in low-temperature environments.
The selection of 9 Nickel Steel for these applications is primarily due to its exceptional toughness at low temperatures, which is critical for maintaining structural integrity and safety.
Important Considerations, Selection Criteria, and Further Insights
| Feature/Property | 9 Nickel Steel | AISI 304 Stainless Steel | AISI 4130 Alloy Steel | Brief Pro/Con or Trade-off Note |
|---|---|---|---|---|
| Key Mechanical Property | High toughness | Good corrosion resistance | High strength | 9Ni excels in low temperatures, while 304 offers better corrosion resistance. |
| Key Corrosion Aspect | Fair | Excellent | Good | 9Ni is less resistant to corrosive environments compared to 304. |
| Weldability | Good | Excellent | Fair | 9Ni requires preheating; 304 is easier to weld. |
| Machinability | Moderate | Good | Good | 9Ni is tougher, requiring slower speeds. |
| Formability | Good | Excellent | Moderate | 9Ni can be formed but requires care to avoid cracking. |
| Approx. Relative Cost | Higher | Moderate | Lower | 9Ni's nickel content increases cost. |
| Typical Availability | Limited | Widely available | Widely available | 9Ni may be harder to source. |
When selecting 9 Nickel Steel, considerations include its unique properties, availability, and cost-effectiveness. While it offers exceptional performance in cryogenic applications, its higher cost and limited availability compared to more common grades may influence decision-making. Additionally, safety and performance requirements in specific applications should guide material selection, ensuring that the chosen steel meets all operational demands.