8620H steel is a medium-carbon alloy steel that is primarily classified as a low-alloy steel. It is known for its excellent hardenability, strength, and toughness, making it suitable for a variety of engineering applications. The primary alloying elements in 8620H steel include chromium (Cr), molybdenum (Mo), and nickel (Ni), which enhance its mechanical properties and resistance to wear and fatigue.

Comprehensive Overview

8620H steel is characterized by its balanced composition, which typically includes around 0.18-0.23% carbon, 0.70-0.90% manganese, 0.40-0.60% chromium, 0.15-0.25% molybdenum, and 1.00-1.50% nickel. This combination of elements contributes to its high tensile strength, good ductility, and excellent toughness, making it a preferred choice for applications requiring high strength and durability.

Advantages:
- High Strength and Toughness: 8620H exhibits excellent mechanical properties, making it suitable for heavy-duty applications.
- Good Hardening Capability: The alloying elements provide good hardenability, allowing for effective heat treatment processes.
- Versatility: It can be used in various applications, including gears, shafts, and other components requiring high strength.

Limitations:
- Weldability Concerns: While it can be welded, special precautions must be taken to avoid cracking.
- Cost: The alloying elements can make it more expensive than lower-grade steels.
- Corrosion Resistance: It is not as corrosion-resistant as stainless steels, which may limit its use in certain environments.

Historically, 8620H has been utilized in the automotive and aerospace industries, where its properties are critical for performance and safety. Its market position is strong, particularly in sectors that demand high-performance materials.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS G86200 USA Closest equivalent to AISI 8620
AISI/SAE 8620 USA Commonly used designation
ASTM A29/A29M USA General specification for alloy steels
EN 1.6523 Europe Minor compositional differences
DIN 20CrMo Germany Similar properties, but different alloying elements
JIS SCM420 Japan Comparable, but with different mechanical properties

The differences between these equivalent grades can affect performance, particularly in terms of hardenability and toughness. For instance, while both AISI 8620 and UNS G86200 are similar, the latter may have stricter compositional limits that can influence its mechanical properties.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
C (Carbon) 0.18 - 0.23
Mn (Manganese) 0.70 - 0.90
Cr (Chromium) 0.40 - 0.60
Mo (Molybdenum) 0.15 - 0.25
Ni (Nickel) 1.00 - 1.50
Si (Silicon) 0.15 - 0.40
P (Phosphorus) ≤ 0.035
S (Sulfur) ≤ 0.040

The primary role of the key alloying elements in 8620H steel includes:
- Chromium: Enhances hardenability and corrosion resistance.
- Molybdenum: Improves strength at elevated temperatures and enhances toughness.
- Nickel: Increases toughness and improves the steel's ability to withstand impact.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Quenched & Tempered 850 - 1000 MPa 123 - 145 ksi ASTM E8
Yield Strength (0.2% offset) Quenched & Tempered 650 - 850 MPa 94 - 123 ksi ASTM E8
Elongation Quenched & Tempered 15 - 20% 15 - 20% ASTM E8
Reduction of Area Quenched & Tempered 50 - 60% 50 - 60% ASTM E8
Hardness (Rockwell C) Quenched & Tempered 28 - 34 HRC 28 - 34 HRC ASTM E18
Impact Strength (Charpy) Room Temperature 40 - 60 J 30 - 44 ft-lbf ASTM E23

The combination of these mechanical properties makes 8620H steel particularly suitable for applications involving dynamic loading and structural integrity, such as in the manufacturing of gears and shafts. Its high tensile and yield strength, along with good ductility, allow it to perform well under stress.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density Room Temperature 7.85 g/cm³ 0.284 lb/in³
Melting Point - 1425 - 1540 °C 2600 - 2800 °F
Thermal Conductivity Room Temperature 45 W/m·K 31 BTU·in/(hr·ft²·°F)
Specific Heat Capacity Room Temperature 0.46 kJ/kg·K 0.11 BTU/lb·°F
Electrical Resistivity Room Temperature 0.00065 Ω·m 0.00038 Ω·in
Coefficient of Thermal Expansion Room Temperature 11.5 x 10⁻⁶ /K 6.4 x 10⁻⁶ /°F

The practical significance of 8620H's physical properties includes:
- Density: Provides insight into weight considerations for structural applications.
- Thermal Conductivity: Important for applications where heat dissipation is critical.
- Melting Point: Indicates suitability for high-temperature applications.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides Varies Ambient Fair Risk of pitting
Sulfuric Acid 10% 25 °C / 77 °F Poor Not recommended
Sodium Hydroxide 5% 25 °C / 77 °F Fair Susceptible to SCC
Atmospheric - Ambient Good Moderate resistance

8620H steel exhibits moderate corrosion resistance, particularly in atmospheric conditions. However, it is susceptible to pitting in chloride environments and should not be used in acidic or highly alkaline conditions. Compared to stainless steels like 304 or 316, which offer excellent corrosion resistance, 8620H is less suitable for applications exposed to harsh environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 400 °C 752 °F Suitable for prolonged exposure
Max Intermittent Service Temp 500 °C 932 °F Short-term exposure
Scaling Temperature 600 °C 1112 °F Risk of oxidation beyond this temp
Creep Strength considerations begin 300 °C 572 °F Important for high-temperature applications

At elevated temperatures, 8620H steel maintains its strength and toughness, but oxidation can become a concern. It is suitable for applications where temperatures do not exceed its maximum service limits, making it ideal for components in engines and machinery.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
MIG ER70S-6 Argon + CO2 Preheat recommended
TIG ER80S-Ni Argon Post-weld heat treatment
Stick E7018 - Requires preheating

8620H steel can be welded using various methods, but preheating is often necessary to minimize the risk of cracking. Post-weld heat treatment is also recommended to relieve stresses and improve toughness.

Machinability

Machining Parameter [8620H Steel] AISI 1212 Notes/Tips
Relative Machinability Index 60% 100% Moderate machinability
Typical Cutting Speed (Turning) 30-50 m/min 80-100 m/min Use carbide tools for best results

Machinability of 8620H is moderate; it requires careful selection of tooling and cutting speeds. Carbide tools are recommended for optimal performance.

Formability

8620H steel exhibits good formability, allowing for both cold and hot forming processes. However, it is essential to consider work hardening effects during cold working, which can increase the material's strength but may also lead to cracking if not managed properly.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 700 - 800 °C / 1292 - 1472 °F 1 - 2 hours Air or Furnace Softening, improved ductility
Quenching 800 - 850 °C / 1472 - 1562 °F 30 minutes Oil or Water Hardening, increased strength
Tempering 400 - 600 °C / 752 - 1112 °F 1 hour Air Toughness improvement

During heat treatment, 8620H undergoes significant metallurgical transformations. Quenching increases hardness, while tempering reduces brittleness, resulting in a balanced combination of strength and toughness.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Automotive Gears High strength, toughness Critical for performance
Aerospace Shafts Good hardenability, fatigue resistance Safety and reliability
Machinery Crankshafts Excellent toughness, wear resistance Durability under stress

Other applications include:
- Oil and gas industry components
- Heavy machinery parts
- Structural components in construction

8620H steel is chosen for these applications due to its ability to withstand high stress and fatigue, making it ideal for critical components.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 8620H Steel AISI 4140 AISI 4340 Brief Pro/Con or Trade-off Note
Key Mechanical Property High strength Moderate strength High strength 8620H offers good toughness vs. 4140's higher hardness
Key Corrosion Aspect Fair Poor Fair 8620H better for moderate environments
Weldability Moderate Good Fair 8620H requires preheating
Machinability Moderate Good Fair 8620H is less machinable than 4140
Formability Good Fair Poor 8620H is easier to form
Approx. Relative Cost Moderate Moderate Higher 8620H is cost-effective for its properties
Typical Availability Good Good Moderate 8620H is widely available

When selecting 8620H steel, considerations include its cost-effectiveness, availability, and suitability for specific applications. Its moderate corrosion resistance and weldability make it a versatile choice, while its mechanical properties ensure reliability in demanding environments.

In conclusion, 8620H steel is a robust material that balances strength, toughness, and versatility, making it a preferred choice in various engineering applications. Its unique properties and performance characteristics should be carefully evaluated against project requirements to ensure optimal material selection.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS G86200, ASTM A29/A29M, EN 1.6523, DIN 20CrMo, JIS SCM420). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

1 comment

Immerse into the expansive universe of EVE Online. Become a legend today. Create alongside thousands of players worldwide. [url=https://www.eveonline.com/signup?invc=46758c20-63e3-4816-aa0e-f91cff26ade4]Download free[/url]

Robertnob

Leave a comment