402 Stainless Steel: Properties and Key Applications

Table Of Content

Table Of Content

402 stainless steel is classified as an austenitic stainless steel, primarily known for its high chromium and nickel content. This grade is characterized by its excellent corrosion resistance, good formability, and high strength, making it suitable for a variety of applications in industries such as automotive, aerospace, and food processing. The primary alloying elements in 402 stainless steel include chromium (Cr), nickel (Ni), and iron (Fe), with chromium being the most significant for enhancing corrosion resistance and nickel contributing to its toughness and ductility.

Comprehensive Overview

The most significant characteristics of 402 stainless steel include its high resistance to oxidation and corrosion, particularly in mildly corrosive environments. It also exhibits good mechanical properties, including strength and ductility, which are essential for structural applications. However, it is important to note that while 402 stainless steel offers many advantages, it also has limitations. For instance, it may not perform as well in highly acidic or chloride-rich environments compared to other stainless steel grades, such as 304 or 316.

Advantages:
- Excellent corrosion resistance in mild environments
- Good mechanical properties, including strength and ductility
- High-temperature resistance

Limitations:
- Reduced performance in highly acidic or chloride-rich environments
- Lower weldability compared to some other stainless steel grades

Historically, 402 stainless steel has been used in applications where a combination of strength and corrosion resistance is required, such as in the manufacturing of automotive components and industrial equipment. Its market position is strong, particularly in sectors that prioritize durability and resistance to wear.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S40200 USA Closest equivalent to AISI 402
AISI/SAE 402 USA Minor compositional differences to be aware of
ASTM A240 USA Standard specification for stainless steel plates
EN 1.4006 Europe Equivalent grade in European standards
JIS SUS 402 Japan Similar properties with slight variations

The table above highlights the various standards and designations associated with 402 stainless steel. Notably, while grades like AISI 304 and 316 are more commonly used, 402 offers specific advantages in certain applications, particularly where moderate corrosion resistance is sufficient.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Cr (Chromium) 11.5 - 13.5
Ni (Nickel) 0.5 - 2.0
Fe (Iron) Balance
C (Carbon) 0.03 max
Mn (Manganese) 1.0 max
Si (Silicon) 1.0 max

The primary role of chromium in 402 stainless steel is to enhance its corrosion resistance, while nickel contributes to its toughness and ductility. The low carbon content helps prevent carbide precipitation, which can lead to intergranular corrosion. Manganese and silicon are included to improve the steel's overall strength and workability.

Mechanical Properties

Property Condition/Temper Test Temperature Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Annealed Room Temp 520 - 750 MPa 75 - 109 ksi ASTM E8
Yield Strength (0.2% offset) Annealed Room Temp 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed Room Temp 40 - 50% 40 - 50% ASTM E8
Hardness (Rockwell B) Annealed Room Temp 80 - 90 HRB 80 - 90 HRB ASTM E18
Impact Strength Annealed -20°C (-4°F) 40 J 29.5 ft-lbf ASTM E23

The mechanical properties of 402 stainless steel make it suitable for applications requiring good strength and ductility. Its tensile strength and yield strength indicate that it can withstand significant loads, while its elongation percentage shows that it can be deformed without breaking, which is crucial for forming processes.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temp 7.8 g/cm³ 0.282 lb/in³
Melting Point - 1400 - 1450 °C 2552 - 2642 °F
Thermal Conductivity Room Temp 25 W/m·K 14.5 BTU·in/h·ft²·°F
Specific Heat Capacity Room Temp 500 J/kg·K 0.12 BTU/lb·°F
Electrical Resistivity Room Temp 0.73 µΩ·m 0.00000073 Ω·m
Coefficient of Thermal Expansion Room Temp 16.5 x 10⁻⁶/K 9.2 x 10⁻⁶/°F

The density and melting point of 402 stainless steel indicate its robustness, while its thermal conductivity and specific heat capacity are important for applications involving heat transfer. The electrical resistivity is relatively low, making it suitable for certain electrical applications.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3 - 10 20 - 60 / 68 - 140 Fair Risk of pitting corrosion
Sulfuric Acid 10 - 30 20 - 40 / 68 - 104 Poor Not recommended
Acetic Acid 5 - 20 20 - 60 / 68 - 140 Good Moderate resistance
Atmospheric - - Excellent Good resistance

402 stainless steel exhibits good resistance to atmospheric corrosion and moderate resistance to certain acids. However, it is susceptible to pitting corrosion in chloride environments, which is a critical consideration for applications in coastal or marine environments. Compared to grades like 304 and 316, 402's performance in highly corrosive environments is notably inferior, particularly in chloride-rich conditions.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 800 °C 1472 °F Suitable for high temps
Max Intermittent Service Temp 900 °C 1652 °F Short-term exposure
Scaling Temperature 1000 °C 1832 °F Risk of oxidation

At elevated temperatures, 402 stainless steel maintains its strength and oxidation resistance, making it suitable for applications involving heat. However, prolonged exposure to temperatures above 800 °C can lead to scaling, which may compromise its structural integrity.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER 308L Argon Preheat recommended
MIG ER 308L Argon + CO2 mix Post-weld heat treatment may be necessary

402 stainless steel can be welded using standard techniques, but preheating and post-weld heat treatment are recommended to minimize the risk of cracking. The choice of filler metal is crucial to ensure compatibility and maintain corrosion resistance.

Machinability

Machining Parameter 402 Stainless Steel AISI 1212 Notes/Tips
Relative Machinability Index 40 100 Requires slower cutting speeds
Typical Cutting Speed (Turning) 30 m/min 80 m/min Use carbide tools for best results

Machining 402 stainless steel can be challenging due to its toughness. Optimal conditions include using carbide tools and slower cutting speeds to prevent tool wear.

Formability

402 stainless steel exhibits good formability, making it suitable for cold and hot forming processes. However, it is essential to consider work hardening, which can affect the material's ductility during forming operations.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 1050 - 1150 °C / 1922 - 2102 °F 1 - 2 hours Air or water Improve ductility and reduce hardness

Heat treatment processes such as annealing are crucial for enhancing the ductility and reducing the hardness of 402 stainless steel. During annealing, the microstructure transforms, leading to improved mechanical properties.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Automotive Exhaust systems Corrosion resistance, high-temperature strength Durability and performance
Aerospace Engine components High strength, heat resistance Safety and reliability
Food Processing Equipment and fixtures Corrosion resistance, ease of cleaning Hygiene and compliance

Other applications include:
- Chemical processing equipment
- Marine hardware
- Architectural applications

402 stainless steel is chosen for applications requiring a balance of strength and corrosion resistance, particularly in environments where exposure to moisture or mild corrosive agents is expected.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 402 Stainless Steel AISI 304 Stainless Steel AISI 316 Stainless Steel Brief Pro/Con or Trade-off Note
Key Mechanical Property Moderate strength High strength High strength 402 is less strong than 304 and 316
Key Corrosion Aspect Fair in chlorides Good in chlorides Excellent in chlorides 316 offers superior corrosion resistance
Weldability Moderate Good Good 402 requires more care in welding
Machinability Moderate Good Moderate 304 is easier to machine
Formability Good Excellent Good 304 has superior formability
Approx. Relative Cost Moderate Moderate Higher 402 is cost-effective for specific applications
Typical Availability Moderate High High 304 and 316 are more commonly available

When selecting 402 stainless steel, considerations include its cost-effectiveness, availability, and specific performance requirements. While it may not be as widely used as 304 or 316, it offers unique advantages in certain applications, particularly where moderate corrosion resistance and good mechanical properties are required. Safety and magnetic properties are also essential factors, especially in industries where non-magnetic materials are preferred.

In summary, 402 stainless steel is a versatile material that balances strength, corrosion resistance, and cost, making it suitable for a variety of engineering applications.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S40200, ASTM A240, EN 1.4006, JIS SUS 402). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

4 comments

“Salve a tutti! Ho letto con interesse l’articolo sulle proprietà dell’acciaio inossidabile 402 e le sue applicazioni chiave. Mi chiedevo se qualcuno ha esperienza pratica con questo materiale in contesti di alta temperatura? In particolare, sarei curioso di sapere come si comporta rispetto ad altri acciai inossidabili in ambienti industriali.

A proposito, recentemente ho trovato un’analisi comparativa molto dettagliata sulle prestazioni di diversi gradi di acciaio in varie condizioni su https://collaba.digital/performance-agency – forse potrebbe essere utile per qualcuno che sta valutando diverse opzioni materiali.

Qualcuno ha dati sulle prestazioni a lungo termine del 402 in applicazioni strutturali?"

Tiffany

Em 2025, o Stake Casino se consolidou como uma das principais opcoes para jogadores brasileiros. Para entrar no site com seguranca, basta usar o acesso oficial disponivel aqui — [url=https://stakebettingaustralia.com/br/]Receba giros gratis e participe de torneios emocionantes[/url]
. Com uma biblioteca diversificada, experiencia fluida e assistencia dedicada, o Stake atrai um publico fiel.
“Jogue mais de 3000 jogos de forma facil!”
Registro no Stake Brasil | Processo Rapido Instantaneo
A criacao de conta no Stake e simples. Voce podem comecar a apostar em pouco tempo. Basta entrar na plataforma usando a pagina indicada, selecionar “Criar Conta”, preencher seus dados e confirmar o e-mail. Depois disso, faca seu deposito e aproveite os jogos.
“Crie sua conta rapidamente e receba sua recompensa!”
Bonus no Stake para o Brasil | Vantagens Incriveis
Os bonus de boas-vindas sao um dos principais diferenciais. Jogadores iniciantes podem ganhar um extra antes de fazer a primeira aposta. Entre as vantagens estao bonus de primeiro deposito, rodadas gratis e o programa de fidelidade.
“Deposite R$ 100 e ganhe mais R$ 100 para aumentar suas chances!”

Matthewchaky

enpresa

ulisses robalo fernandes

enp+resa

ulisses robalo fernandes

Leave a comment