316H stainless steel is a high-temperature variant of the 316 grade, classified as an austenitic stainless steel. It is primarily alloyed with chromium (16-18%), nickel (10-14%), and molybdenum (2-3%), which enhance its corrosion resistance and mechanical properties. The "H" designation indicates a higher carbon content (0.04% to 0.10%) compared to standard 316, which improves its strength at elevated temperatures.

Comprehensive Overview

316H stainless steel is renowned for its excellent resistance to pitting and crevice corrosion in chloride environments, making it a preferred choice for marine applications and chemical processing. Its high nickel content contributes to its toughness and ductility, while molybdenum enhances its resistance to localized corrosion.

Advantages (Pros):
- Exceptional corrosion resistance, particularly in aggressive environments.
- High strength and toughness at elevated temperatures, making it suitable for high-stress applications.
- Good weldability and formability, allowing for versatile fabrication options.

Limitations (Cons):
- Higher cost compared to lower alloyed stainless steels.
- Susceptibility to sensitization if not properly heat-treated, which can lead to intergranular corrosion.
- Not magnetic, which may be a disadvantage in applications requiring magnetic properties.

Historically, 316H has been significant in industries such as petrochemical, power generation, and marine engineering due to its ability to withstand harsh conditions. Its market position is strong, particularly in sectors that demand high-performance materials.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S31609 USA Closest equivalent to AISI 316H
AISI/SAE 316H USA Higher carbon content than 316
ASTM A240/A240M USA Standard specification for stainless steel plates
EN 1.4878 Europe Equivalent grade in European standards
JIS SUS316H Japan Similar properties with minor compositional differences

The differences between 316H and its equivalents, such as 316L (low carbon) and 316, primarily lie in their carbon content, which affects their high-temperature strength and susceptibility to sensitization.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Cr (Chromium) 16.0 - 18.0
Ni (Nickel) 10.0 - 14.0
Mo (Molybdenum) 2.0 - 3.0
C (Carbon) 0.04 - 0.10
Mn (Manganese) 2.0 max
Si (Silicon) 1.0 max
P (Phosphorus) 0.045 max
S (Sulfur) 0.030 max

The primary role of chromium is to enhance corrosion resistance, while nickel contributes to toughness and ductility. Molybdenum increases resistance to pitting and crevice corrosion, particularly in chloride environments. The higher carbon content in 316H improves its strength at elevated temperatures, making it suitable for high-stress applications.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric) Typical Value/Range (Imperial) Reference Standard for Test Method
Tensile Strength Annealed 515 - 690 MPa 75 - 100 ksi ASTM E8
Yield Strength (0.2% offset) Annealed 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed 40% min 40% min ASTM E8
Hardness (Rockwell B) Annealed 70 - 90 HRB 70 - 90 HRB ASTM E18
Impact Strength (Charpy) -20°C 40 J 30 ft-lbf ASTM E23

The combination of high tensile and yield strength, along with good elongation properties, makes 316H suitable for applications requiring structural integrity under mechanical loading. Its impact strength at low temperatures also enhances its performance in cryogenic applications.

Physical Properties

Property Condition/Temperature Value (Metric) Value (Imperial)
Density Room Temperature 8.0 g/cm³ 0.289 lb/in³
Melting Point - 1375 - 1400 °C 2500 - 2550 °F
Thermal Conductivity Room Temperature 16.2 W/m·K 112 BTU·in/ft²·h·°F
Specific Heat Capacity Room Temperature 500 J/kg·K 0.12 BTU/lb·°F
Electrical Resistivity Room Temperature 0.72 µΩ·m 0.72 µΩ·in
Coefficient of Thermal Expansion 20 - 100 °C 16.0 x 10⁻⁶/K 8.9 x 10⁻⁶/°F

The density and melting point indicate that 316H can withstand high temperatures without significant deformation. Its thermal conductivity is moderate, making it suitable for applications where heat dissipation is necessary. The specific heat capacity is also favorable for thermal applications, while the electrical resistivity suggests it is not a good conductor of electricity.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3.5% 20°C / 68°F Excellent Risk of pitting
Sulfuric Acid 10% 25°C / 77°F Good Limited resistance
Hydrochloric Acid 5% 25°C / 77°F Fair Risk of localized corrosion
Sea Water - Ambient Excellent Highly resistant
Acetic Acid 10% 25°C / 77°F Good Susceptible to stress corrosion cracking

316H exhibits excellent resistance to a variety of corrosive agents, particularly in marine environments. Its performance in chloride-rich conditions is superior to that of 304 and 316L grades, which are more susceptible to pitting corrosion. However, it is important to note that while 316H performs well in many acidic environments, it can still be vulnerable to localized corrosion in specific conditions, particularly with strong acids like hydrochloric acid.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 800°C 1472°F Suitable for high-temperature applications
Max Intermittent Service Temp 870°C 1598°F Short-term exposure only
Scaling Temperature 925°C 1697°F Above this temperature, oxidation occurs
Creep Strength considerations begin 600°C 1112°F Creep resistance decreases above this temperature

316H maintains its mechanical properties at elevated temperatures, making it suitable for applications such as furnace components and heat exchangers. However, prolonged exposure to temperatures above 800°C can lead to oxidation and scaling, which may compromise its integrity.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER316L Argon Good for thin sections
MIG ER316L Argon + CO2 mix Suitable for thicker sections
SMAW E316L - Requires preheat for thick sections

316H is highly weldable, but care must be taken to avoid sensitization during welding. Preheating and post-weld heat treatment are recommended to minimize the risk of intergranular corrosion. The use of filler metals like ER316L ensures compatibility and maintains corrosion resistance.

Machinability

Machining Parameter 316H AISI 1212 Notes/Tips
Relative Machinability Index 30% 100% 316H is more challenging to machine
Typical Cutting Speed (Turning) 20 m/min 40 m/min Use carbide tools for best results

316H has lower machinability compared to carbon steels, requiring slower cutting speeds and specialized tooling. Optimal conditions include using sharp tools and adequate lubrication to reduce work hardening.

Formability

316H exhibits good formability, allowing for cold and hot forming processes. However, due to its work hardening characteristics, careful control of bending radii is necessary to avoid cracking. It is suitable for applications requiring complex shapes and configurations.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Solution Annealing 1010 - 1120 °C / 1850 - 2050 °F 30 minutes Air or water Dissolve carbides, relieve stress
Stress Relieving 400 - 600 °C / 750 - 1112 °F 1 hour Air Reduce residual stresses

Heat treatment processes like solution annealing enhance the corrosion resistance of 316H by dissolving carbides and preventing sensitization. The metallurgical transformations during these treatments significantly impact the microstructure, leading to improved toughness and ductility.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection
Marine Engineering Shipbuilding Corrosion resistance, strength Exposure to seawater
Chemical Processing Reactor vessels High-temperature strength, corrosion resistance Harsh chemical environments
Oil & Gas Pipeline systems Toughness, weldability High-stress applications
Power Generation Heat exchangers High-temperature performance Thermal efficiency

Other applications include:
* Pharmaceutical equipment
* Food processing machinery
* Architectural structures exposed to harsh environments

316H is chosen for these applications due to its superior corrosion resistance and ability to maintain strength at elevated temperatures, ensuring reliability and longevity in demanding environments.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 316H 304 321 Brief Pro/Con or Trade-off Note
Key Mechanical Property High strength Moderate strength High strength 316H offers better high-temp performance
Key Corrosion Aspect Excellent Good Excellent 321 is better for high-temperature applications
Weldability Good Excellent Good 316H requires careful handling to avoid sensitization
Machinability Moderate Good Moderate 316H is more challenging to machine
Approx. Relative Cost Higher Lower Higher Cost considerations may affect selection
Typical Availability Moderate High Moderate 304 is more commonly available

When selecting 316H, considerations include cost-effectiveness, availability, and specific application requirements. Its high performance in corrosive environments and at elevated temperatures makes it a preferred choice in critical applications. However, its higher cost and lower machinability compared to alternatives like 304 may influence decisions, especially in less demanding environments.

In conclusion, 316H stainless steel is a versatile and high-performance material that excels in challenging conditions, making it indispensable in various industries. Its unique properties and capabilities warrant careful consideration during material selection to ensure optimal performance and longevity in applications.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S31609, ASTM A240/A240M, EN 1.4878, JIS SUS316H). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

Leave a comment