308 Stainless Steel is classified as an austenitic stainless steel, known for its excellent corrosion resistance and high-temperature strength. This grade is primarily alloyed with chromium (20-22%) and nickel (10-12%), with the addition of molybdenum (up to 2%) to enhance its resistance to pitting and crevice corrosion. The presence of these elements contributes to its non-magnetic properties and good weldability, making it suitable for various applications in harsh environments.

Comprehensive Overview

308 Stainless Steel is particularly valued in the welding industry due to its ability to maintain strength and corrosion resistance at elevated temperatures. It is often used as a filler metal for welding other stainless steels, especially in applications where high strength and resistance to oxidation are required. The steel's high chromium and nickel content provides a robust protective layer against corrosion, while its austenitic structure ensures excellent toughness and ductility.

Advantages (Pros):
- Corrosion Resistance: Exceptional resistance to a wide range of corrosive environments, including acidic and alkaline conditions.
- Weldability: Excellent for welding applications, particularly as a filler metal for other stainless steels.
- High-Temperature Strength: Retains strength and stability at elevated temperatures, making it suitable for high-heat applications.

Limitations (Cons):
- Cost: Generally more expensive than lower-grade steels due to alloying elements.
- Work Hardening: Can become hard and brittle if not properly handled during machining or forming processes.
- Susceptibility to Stress Corrosion Cracking: In certain environments, particularly chloride-rich conditions, it can be prone to stress corrosion cracking.

Historically, 308 Stainless Steel has played a significant role in the development of welding technologies, particularly in the fabrication of structures requiring high strength and durability. Its market position remains strong, especially in industries such as construction, automotive, and aerospace.

Alternative Names, Standards, and Equivalents

Standard Organization Designation/Grade Country/Region of Origin Notes/Remarks
UNS S30800 USA Closest equivalent to AISI 308
AISI/SAE 308 USA Commonly used filler metal
ASTM A240 USA Standard specification for stainless steel plates
EN 1.4301 Europe Equivalent to AISI 304, with higher nickel content
JIS SUS308 Japan Similar properties to AISI 308
ISO 308 International Standard designation for austenitic stainless steel

The differences between equivalent grades can significantly affect performance in specific applications. For instance, while 1.4301 (AISI 304) has a lower nickel content, it may not perform as well in high-temperature applications compared to 308.

Key Properties

Chemical Composition

Element (Symbol and Name) Percentage Range (%)
Cr (Chromium) 20.0 - 22.0
Ni (Nickel) 10.0 - 12.0
Mo (Molybdenum) 0.0 - 2.0
C (Carbon) ≤ 0.08
Mn (Manganese) ≤ 2.0
Si (Silicon) ≤ 1.0
P (Phosphorus) ≤ 0.045
S (Sulfur) ≤ 0.03

The primary role of chromium is to enhance corrosion resistance, while nickel contributes to the steel's toughness and ductility. Molybdenum improves resistance to pitting and crevice corrosion, particularly in chloride environments. Carbon, although present in low amounts, can affect the steel's hardness and strength.

Mechanical Properties

Property Condition/Temper Typical Value/Range (Metric - SI Units) Typical Value/Range (Imperial Units) Reference Standard for Test Method
Tensile Strength Annealed 515 - 690 MPa 75 - 100 ksi ASTM E8
Yield Strength (0.2% offset) Annealed 205 - 310 MPa 30 - 45 ksi ASTM E8
Elongation Annealed 40 - 50% 40 - 50% ASTM E8
Reduction of Area Annealed 60 - 70% 60 - 70% ASTM E8
Hardness (Rockwell B) Annealed 70 - 90 HRB 70 - 90 HRB ASTM E18
Impact Strength (Charpy) -40°C 40 J 30 ft-lbf ASTM E23

The combination of these mechanical properties makes 308 Stainless Steel suitable for applications requiring high strength and ductility, particularly in structural and welding applications. Its ability to withstand significant deformation without fracturing is crucial in dynamic loading conditions.

Physical Properties

Property Condition/Temperature Value (Metric - SI Units) Value (Imperial Units)
Density Room Temperature 8.0 g/cm³ 0.289 lb/in³
Melting Point/Range - 1400 - 1450 °C 2552 - 2642 °F
Thermal Conductivity Room Temperature 16 W/m·K 92 BTU·in/(hr·ft²·°F)
Specific Heat Capacity Room Temperature 500 J/kg·K 0.119 BTU/lb·°F
Electrical Resistivity Room Temperature 0.72 µΩ·m 0.0000143 Ω·in
Coefficient of Thermal Expansion Room Temperature 16.0 x 10⁻⁶ /K 8.9 x 10⁻⁶ /°F

The density of 308 Stainless Steel makes it suitable for applications where weight is a consideration, while its thermal conductivity and specific heat capacity are critical in high-temperature applications, such as in heat exchangers and furnace components.

Corrosion Resistance

Corrosive Agent Concentration (%) Temperature (°C/°F) Resistance Rating Notes
Chlorides 3-10 20-60 / 68-140 Good Risk of pitting
Sulfuric Acid 10-30 20-60 / 68-140 Fair Susceptible to stress corrosion
Acetic Acid 5-20 20-60 / 68-140 Excellent Good resistance
Sea Water - 20-60 / 68-140 Good Risk of crevice corrosion
Ammonia - 20-60 / 68-140 Excellent Resistant to stress corrosion

308 Stainless Steel exhibits excellent resistance to a variety of corrosive environments, particularly in acidic and alkaline conditions. However, it is susceptible to stress corrosion cracking in chloride-rich environments, which can be a critical consideration in marine applications. Compared to 304 Stainless Steel, 308 offers improved resistance to pitting and crevice corrosion, making it a better choice for applications in harsh environments.

Heat Resistance

Property/Limit Temperature (°C) Temperature (°F) Remarks
Max Continuous Service Temp 870 1600 Suitable for high-temperature applications
Max Intermittent Service Temp 925 1700 Can withstand short-term exposure
Scaling Temperature 900 1650 Risk of oxidation beyond this temperature
Creep Strength considerations 600 1112 Begins to lose strength at elevated temps

At elevated temperatures, 308 Stainless Steel maintains its mechanical properties and exhibits good oxidation resistance. However, prolonged exposure to temperatures above 900 °C (1650 °F) can lead to scaling and degradation of the protective oxide layer, necessitating careful consideration in high-temperature applications.

Fabrication Properties

Weldability

Welding Process Recommended Filler Metal (AWS Classification) Typical Shielding Gas/Flux Notes
TIG ER308L Argon Low carbon content for reduced carbide precipitation
MIG ER308L Argon/CO2 Good for thicker sections
SMAW E308L - Suitable for all positions

308 Stainless Steel is highly weldable, making it a preferred choice for welding applications. Preheating is generally not required, but post-weld heat treatment may be beneficial to relieve stresses and improve corrosion resistance. Common defects include porosity and cracking, which can be mitigated through proper welding techniques.

Machinability

Machining Parameter [308 Stainless Steel] AISI 1212 Notes/Tips
Relative Machinability Index 30% 100% Requires sharp tools and slower speeds
Typical Cutting Speed 30 m/min 60 m/min Use of coolant recommended

308 Stainless Steel has lower machinability compared to carbon steels, requiring careful selection of tooling and cutting parameters. High-speed steel or carbide tools are recommended, and the use of cutting fluids can enhance tool life and surface finish.

Formability

308 Stainless Steel exhibits good formability, allowing for cold and hot forming processes. However, it is important to note that excessive work hardening can occur, necessitating careful control of bending radii and forming techniques to avoid cracking.

Heat Treatment

Treatment Process Temperature Range (°C/°F) Typical Soaking Time Cooling Method Primary Purpose / Expected Result
Annealing 1010 - 1120 / 1850 - 2050 30 minutes Air Relieve stresses, improve ductility
Solution Treatment 1000 - 1100 / 1830 - 2010 30 minutes Water Enhance corrosion resistance

Heat treatment processes such as annealing and solution treatment are crucial for optimizing the microstructure and properties of 308 Stainless Steel. These treatments help to relieve internal stresses and enhance the material's corrosion resistance, making it suitable for demanding applications.

Typical Applications and End Uses

Industry/Sector Specific Application Example Key Steel Properties Utilized in this Application Reason for Selection (Brief)
Construction Structural components High strength, corrosion resistance Durability in harsh environments
Automotive Exhaust systems High-temperature strength, weldability Performance under thermal stress
Aerospace Engine components High strength, oxidation resistance Safety and reliability at high altitudes
Food Processing Equipment and piping Corrosion resistance, ease of cleaning Hygiene and durability

308 Stainless Steel is widely used in various industries due to its excellent mechanical properties and corrosion resistance. In the construction sector, it is favored for structural components exposed to harsh environments. In the automotive and aerospace industries, its high-temperature strength and weldability make it ideal for critical applications.

Important Considerations, Selection Criteria, and Further Insights

Feature/Property 308 Stainless Steel 304 Stainless Steel 316 Stainless Steel Brief Pro/Con or Trade-off Note
Key Mechanical Property High strength Moderate strength High strength 308 offers better high-temp performance than 304
Key Corrosion Aspect Good in acidic environments Good in general environments Excellent in chloride environments 316 is superior for marine applications
Weldability Excellent Excellent Good 308 is preferred for welding applications
Machinability Moderate Good Moderate 304 is easier to machine than 308
Formability Good Excellent Good 304 has better formability than 308
Approx. Relative Cost Moderate Low High 308 is more cost-effective than 316
Typical Availability Common Very Common Common 304 is the most widely available

When selecting 308 Stainless Steel, considerations include its cost-effectiveness, availability, and specific application requirements. While it offers excellent performance in high-temperature and corrosive environments, it may not be the best choice for every application, particularly where chloride exposure is a concern. The choice between 308, 304, and 316 grades will depend on the specific environmental conditions and mechanical requirements of the application.

In summary, 308 Stainless Steel is a versatile material with a strong balance of properties that make it suitable for a wide range of applications, particularly in welding and high-temperature environments. Its unique combination of corrosion resistance, strength, and weldability ensures its continued relevance in modern engineering and manufacturing.


Data Sources & Verification

Chemical composition and mechanical property values on this page are compiled from published material standards and cross-referenced against the equivalent designations listed above (UNS S30800, ASTM A240, EN 1.4301, JIS SUS308, ISO 308). Values are typical or nominal and vary with product form, thickness, and heat treatment; confirm against the governing standard and mill test certificate before design or procurement use.

Design tools: Working with this grade structurally? Use our free Load Capacity Calculator, Span Calculator, and Steel Beam Calculator. Estimate material weight with our steel weight calculators.

Technically reviewed by Dr. Zhang Zhiwei — former Senior Technical Specialist, Baosteel Group; member, Chinese Society for Metals. How we compile our data · spotted an error? Tell us and we will review it.

Back to blog

Leave a comment